CN101560379A - 矿用速凝固化材料 - Google Patents

矿用速凝固化材料 Download PDF

Info

Publication number
CN101560379A
CN101560379A CNA2009100746228A CN200910074622A CN101560379A CN 101560379 A CN101560379 A CN 101560379A CN A2009100746228 A CNA2009100746228 A CN A2009100746228A CN 200910074622 A CN200910074622 A CN 200910074622A CN 101560379 A CN101560379 A CN 101560379A
Authority
CN
China
Prior art keywords
portions
parts
rapid solidification
mining
solidification material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA2009100746228A
Other languages
English (en)
Other versions
CN101560379B (zh
Inventor
张立中
黄玉诚
曲桂荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DATONG KANGNENG MINING NEW TECHNOLOGY Co Ltd
Original Assignee
DATONG KANGNENG MINING NEW TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DATONG KANGNENG MINING NEW TECHNOLOGY Co Ltd filed Critical DATONG KANGNENG MINING NEW TECHNOLOGY Co Ltd
Priority to CN 200910074622 priority Critical patent/CN101560379B/zh
Publication of CN101560379A publication Critical patent/CN101560379A/zh
Application granted granted Critical
Publication of CN101560379B publication Critical patent/CN101560379B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种矿用速凝固化材料,由下列重量配比的原料组成:铝矾土80份、硅酸盐10~15份、碱1~4份、氧化硅2~3份、氧化铝2~3份、石膏60份、石灰35~40份、聚氨酯0.5~1份、多元醇0.3~2份、多元胺0.2~2份,粉煤灰100份。本发明解决了现有技术中存在的传统井下材料容易开裂、密闭不严、气密性能差、缺乏韧性和膨胀性,造成漏风问题;不能有效治理各类有害气体以及水、火等自然灾害;不能降低劳动强度、减少作业工序和提高功效等问题。

Description

矿用速凝固化材料
技术领域
本发明属于一种固化材料,具体涉及一种矿用速凝固化材料。
背景技术
传统的矿业生产,通风质量差和水患频繁,是普遍存在的安全隐患问题。特别是煤矿,井下安全通风设施质量差,自燃发火频繁,有害气体泄漏,瓦斯爆炸事故不断发生,给国家财产和矿工人身安全造成了很大的损害。
目前,现有技术中使用的传统水泥、沙石构筑的各类密闭设施整体性差,漏风严重,施工工序多,劳动强度大。特别是井下施工环境大部分处于危险区,运料距离远,施工区巷道狭窄,作业难度增加,密闭质量无法提高,不能把采空区彻底密闭隔绝,影响了有效风量,并且不能有效的解决瓦斯、一氧化碳等有害气体灾害预防及治理问题。
发明内容
本发明就是针对上述现有技术中存在的缺陷,提供一种矿用速凝固化材料,解决上述现有技术中存在的传统井下材料容易开裂、密闭不严、气密性能差、缺乏韧性和膨胀性,造成漏风问题;不能有效治理各类有害气体以及水、火等自然灾害;不能降低劳动强度、减少作业工序和提高功效等问题。
本发明采用以下技术方案:一种矿用速凝固化材料,由下列重量配比的原料组成:铝矾土80份、硅酸盐10~15份、碱1~4份、氧化硅2~3份、氧化铝2~3份、石膏60份、石灰35~40份、聚安酯0.5~1份、多元醇0.3~2份、多元胺0.2~2份,粉煤灰100份。
本发明与现有技术相比具有以下有益效果:本发明的材料特性是无机材料,不污染环境,自身不燃烧,无毒、无害、无腐蚀性,材料性能具有在初凝时间上,在膨胀系数上,在抗压强度上都能够根据工作对象的要求进行调节,适应不同的环境条件,有效解决传统井下材料容易开裂、密闭不严、气密性能差、缺乏韧性和膨胀性,造成漏风问题;不能有效治理各类有害气体以及水、火等自然灾害;不能降低劳动强度、减少作业工序和提高功效等问题。
具体实施方式
实施例1
一种矿用速凝固化材料,将下列重量配比的原料:铝矾土80份、硅酸盐10份、碱4份、氧化硅3份、氧化铝3份,放入球磨机进行粉碎研磨均化后取100份,将下列重量配比的原料石膏60份、石灰35份、聚安酯1份、多元醇2份、多元胺2份放入球磨机进行粉碎研磨均化后取100份,粉煤灰100份,将上述材料加入到水为100份的搅拌容器中,充分搅拌、溶解,搅拌均匀后,通过泵送至充填体。
实施例2
一种矿用速凝固化材料,将下列重量配比的原料铝矾土80份、硅酸盐12.5份、碱2.5份、氧化硅2.5份、氧化铝2.5份,放入球磨机进行粉碎研磨均化后取100份,将下列重量配比的原料石膏60份、石灰37.5份、聚安酯0.5份、多元醇1份、多元胺1份,放入球磨机进行粉碎研磨均化后取100份,粉煤灰100份,将上述材料加入到水为100份的搅拌容器中,充分搅拌、溶解,搅拌均匀后,通过泵送至充填体。
实施例3
一种矿用速凝固化材料,将下列重量配比的原料铝矾土80份、硅酸盐15份、聚安酯1份、多元醇2份、多元胺2份,放入球磨机进行粉碎研磨均化后取100份,将下列重量配比的原料石膏60份、石灰40份、聚安酯0.5份、多元醇0.3份、多元胺0.2份放入球磨机进行粉碎研磨均化后取100份,粉煤灰100份,将上述材料加入到水为100份的搅拌容器中,充分搅拌、溶解,搅拌均匀后,通过泵送至充填体。

Claims (1)

1、一种矿用速凝固化材料,其特征在于:由下列重量配比的原料组成:铝矾土80份、硅酸盐10~15份、碱1~4份、氧化硅2~3份、氧化铝2~3份、石膏60份、石灰35~40份、聚安酯0.5~1份、多元醇0.3~2份、多元胺0.2~2份,粉煤灰100份。
CN 200910074622 2009-05-27 2009-05-27 矿用速凝固化材料 Expired - Fee Related CN101560379B (zh)