CN101531495B - 凹凸棒外墙乳胶漆 - Google Patents

凹凸棒外墙乳胶漆 Download PDF

Info

Publication number
CN101531495B
CN101531495B CN2009100262963A CN200910026296A CN101531495B CN 101531495 B CN101531495 B CN 101531495B CN 2009100262963 A CN2009100262963 A CN 2009100262963A CN 200910026296 A CN200910026296 A CN 200910026296A CN 101531495 B CN101531495 B CN 101531495B
Authority
CN
China
Prior art keywords
attapulgite
wall emulsion
emulsion varnish
varnish
sludge slurry
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009100262963A
Other languages
English (en)
Other versions
CN101531495A (zh
Inventor
喻爱芳
许庆华
许盛英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Liwang Chemical (Nantong) Co., Ltd.
Original Assignee
许盛英
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 许盛英 filed Critical 许盛英
Priority to CN2009100262963A priority Critical patent/CN101531495B/zh
Publication of CN101531495A publication Critical patent/CN101531495A/zh
Application granted granted Critical
Publication of CN101531495B publication Critical patent/CN101531495B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种凹凸棒外墙乳胶漆,其技术方案的要点是,凹凸棒外墙乳胶漆是由膏状凹凸棒石粘土、苯丙乳液、超细重质碳酸钙、金红石型钛白粉、羟乙基纤维素、乙二醇、磷酸三丁酯和去离子水组成。凹凸棒外墙乳胶漆的生产方法是:配料、粉碎、搅拌、分散、溶解、均质、乳化、消泡、研磨、罐装为凹凸棒外墙乳胶漆的成品。凹凸棒外墙乳胶漆附着力好,具有较好的耐候性、耐水性和耐冻融性,凹凸棒外墙乳胶漆安全无毒,无污染,属于环保型外墙乳胶漆。凹凸棒外墙乳胶漆是白色基准涂料,可以直接进行调色生产各种不同颜色的彩色涂料,凹凸棒外墙乳胶漆适用于建筑物装饰装修。

Description

凹凸棒外墙乳胶漆
技术领域
本发明涉及涂料,具体涉及一种凹凸棒外墙乳胶漆。
背景技术
乳胶漆作为环保型涂料,已越来越多地被建筑及装修行业所认可,乳胶漆以水为稀释剂,是一种施工方便、安全、耐水洗、透气性好的漆种,它可根据不同的配色方案调配出不同的色泽。
外墙乳胶漆的基本性能与内墙乳胶漆差不多,但外墙乳胶漆的漆膜较硬,抗水能力更强,保光保色性好,对抗紫外线要求比外墙乳胶漆要高得多。
中国专利授权公告号CN1304494,授权公告日为2007年3月14日,名称为“环保调湿乳胶漆”,公开了“一种环保调湿乳胶漆,其工艺配方是:除包括现有乳胶漆成分水、乳液、颜料、填料、各种助剂外,还包括有占总量(重量百分比)1%-3%的凹凸棒粉、7%-13%的硅藻土、0.1%-0.4%的高吸水树脂和0.1%-0.3%的干膜防霉剂。生产工艺是在搅拌器中加入水,在搅拌过程中依次加入分散剂、润湿剂、硅藻土、颜填料、凹凸棒土和部分消泡剂,搅拌均匀后注入砂磨机砂磨至一定细度,然后倒入调漆罐中,加入乳液和剩余消泡剂搅拌均匀,再缓慢加入成膜助剂、干膜防霉剂、防腐剂和高吸水树脂充分搅拌,最后加入增稠剂和胺中和剂,将乳胶漆调整至合适的粘度,搅拌均匀后过滤、包装即可。这种乳胶漆成本较低,调湿功能更持久、装饰性好。”
上述专利的不足之处是该项技术中选用没有经过提纯和改性处理的凹凸棒粉作为填料,而且凹凸棒粉只是占总量(重量百分比)1%-3%,是起不到容留水蒸气的作用,增稠效果也较差。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种凹凸棒外墙乳胶漆。
凹凸棒外墙乳胶漆是由膏状凹凸棒石粘土、苯丙乳液、超细重质碳酸钙、金红石型钛白粉、羟乙基纤维素、乙二醇、磷酸三丁酯和去离子水组成。
凹凸棒外墙乳胶漆的生产方法是:配料、粉碎、搅拌、分散、溶解、均质、乳化、消泡、研磨、罐装为凹凸棒外墙乳胶漆的成品。
凹凸棒石粘土是一种含水富镁纳米级多孔纤维状硅酸盐粘土矿物,当凹凸棒石粘土中的凹凸棒含量≥80%以上时,其比表面积较大,可达500m2/g以上。使用“凹凸棒的湿法选矿工艺”和“凹凸棒矿造浆生产工艺”,将凹凸棒石粘土中的水云母、石英、蛋白石和碳酸盐等矿物筛选去除掉,得到一种凹凸棒矿泥浆;经过钠化处理和酸化处理后的膏状凹凸棒石粘土,是一种触变性和胶黏性特好的天然硅酸镁铝凝胶,pH值呈中性,凹凸棒石粘土的粘度、膨胀容、胶质价、白度、比表面积、吸附性能和悬浮率都得到了较大的提高。
凹凸棒石粘土土质细腻,表面光滑,质地较轻,潮湿时呈粘性和可塑性,其粘度可达到3000mPa·s以上,有利于原料之间的粘结;凹凸棒石粘土干燥收缩率小,且不产生龟裂,能提高外墙涂料对建筑物墙面的附着力,膏状凹凸棒石粘土加入涂料溶液中,在外力搅拌下快速形成稳定的不分层的凝胶体,有较好的粘滞性和触变性,凹凸棒石粘土涂料涂膜的显微照片显示,其晶体呈网状排列,均匀地分布在涂料中,所以涂膜表面耐磨性能好。
凹凸棒石粘土具有选择吸附能力,如对极性分子水、氨、甲醇、乙醇、醛、酮、烯、烃等能被通道孔吸收,而对非极性分子如氧等则不能进入孔道,利用这种吸附特性,能吸附空气中的甲醛和挥发性有机物,净化空气。
苯丙乳液是苯乙烯、丙烯酸酯类共聚乳液的简称,具有较好的化学稳定性、冻融稳定性和亲和性,苯丙乳液有良好的附着力、耐水性和流平性。
超细重质碳酸钙具有粒径小、粒度分布窄、杂质极少、吸油值低、高白度等优点,有助于提高凹凸棒外墙乳胶漆的光泽度、干燥性和遮盖力。
金红石型钛白粉耐光性非常强,是建筑涂料的基础白色颜料,对涂料的装饰性、耐候性、耐化学稳定性等方面起着关键作用,特别适用于外墙涂料。
羟乙基纤维素在凹凸棒外墙乳胶漆中能起增稠、粘结、乳化、分散、稳定作用,并能保持水份,形成薄膜和保持稳定的胶体性能。
乙二醇是助成膜剂和防冻剂。
磷酸三丁酯是一种消泡剂。
本发明通过下述技术方案予以实现:
1、凹凸棒外墙乳胶漆的配料按重量百分比由下列组分组成:膏状凹凸棒石粘土20~55%、苯丙乳液15~45%、超细重质碳酸钙5~35%、金红石型钛白粉1~10%、羟乙基纤维素0.5~5%、乙二醇0.5~5%、磷酸三丁酯0.01~2%和去离子水5~35%。
2、凹凸棒外墙乳胶漆的生产方法:①将凹凸棒外墙乳胶漆的配料加入粉碎打浆机内进行粉碎,粉碎打浆混合均匀后为凹凸棒外墙乳胶漆的混合物;②将步骤①获得的混合物输入高粘度真空搅拌机中,凹凸棒外墙乳胶漆的配料在真空下经过搅拌、分散、溶解、均质、乳化和消泡后为凹凸棒外墙乳胶漆的半成品;③将步骤②获得的凹凸棒外墙乳胶漆的半成品输入多功能胶体磨中进行研磨,研磨后的颗粒细度小于0.015毫米,罐装为凹凸棒外墙乳胶漆的成品。
所述膏状凹凸棒石粘土的生产工艺是:(1)选用凹凸棒矿泥浆为主体原料,凹凸棒矿泥浆按重量百分比由下列组分组成:凹凸棒石粘土15~35%和水65~85%;(2)钠化处理:将凹凸棒矿泥浆输送到搅拌机内,添加氢氧化钠后进行搅拌,经过搅拌后的凹凸棒矿泥浆输送到钠化池中陈化1~7天;钠化配料按重量百分比由下列组分组成:凹凸棒矿泥浆95~99.5%和氢氧化钠0.5~5%;(3)酸化处理:将钠化后凹凸棒矿泥浆输送到搅拌机内,添加浓度为98%的硫酸后进行搅拌,经过搅拌后的凹凸棒矿泥浆输送到酸化池中陈化1~3天;酸化配料按重量百分比由下列组分组成:钠化后的凹凸棒矿泥浆92~99.5%和浓度为98%的硫酸0.5~8%;(4)水洗和筛去杂质:将酸化后的凹凸棒矿泥浆输送到沉淀池中,重新加水浸泡,用气泵冲翻,筛去杂质,沉淀后放出浸泡水,并将沉淀后的泥浆输送到成品池内,沉淀后的泥浆为膏状凹凸棒石粘土;水洗配料按重量百分比由下列组分组成:酸化后的凹凸棒矿泥浆25~65%和水35~75%;膏状凹凸棒石粘土按重量百分比由下列组分组成:凹凸棒石粘土5~40%和水60~95%。
上述生产工艺是采用由本发明人于2008年8月25日申请的“膏状凹凸棒石粘土的生产工艺”,中国专利公开号为:CN101348257,公开日:2009年1月21日。
所述凹凸棒矿造浆生产工艺是:将凹凸棒矿输入搅拌机内搅拌,经挤出机挤压成片状后,再次输入搅拌机内搅拌,经挤出机挤压成片状后自然晾晒,晾干的凹凸棒矿输送到原料池中浸泡,用气泵冲翻,沉淀后放出浸泡水,筛去杂质,输入半成品池中,重新加水浸泡,用气泵冲翻,沉淀后放出浸泡水,并将沉淀后的泥浆输送到成品池内,即为凹凸棒矿泥浆成品。
上述生产工艺是采用由本发明人于2004年1月6日申请的“凹凸棒矿造浆生产工艺”,中国专利授权公告号为:CN1287965C,授权公告日:2006年12月6日。
凹凸棒外墙乳胶漆附着力好,具有较好的耐候性、耐水性和耐冻融性,凹凸棒外墙乳胶漆安全无毒,无污染,属于环保型外墙乳胶漆。
凹凸棒外墙乳胶漆是白色基准涂料,可以直接进行调色生产各种不同颜色的彩色涂料。
凹凸棒外墙乳胶漆适用于建筑物装饰装修。
具体实施方式
下面结合实施例对本发明作进一步的描述:
1、凹凸棒外墙乳胶漆的配料按重量百分比由下列组分组成:膏状凹凸棒石粘土35%、苯丙乳液28%、超细重质碳酸钙20%、金红石型钛白粉4%、羟乙基纤维素2%、乙二醇0.6%、磷酸三丁酯0.4%和去离子水10%。
2、凹凸棒外墙乳胶漆的生产方法:①将凹凸棒外墙乳胶漆的配料加入粉碎打浆机内进行粉碎,粉碎打浆混合均匀后为凹凸棒外墙乳胶漆的混合物;②将步骤①获得的混合物输入高粘度真空搅拌机中,凹凸棒外墙乳胶漆的配料在真空下经过搅拌、分散、溶解、均质、乳化和消泡后为凹凸棒外墙乳胶漆的半成品;③将步骤②获得的凹凸棒外墙乳胶漆的半成品输入多功能胶体磨中进行研磨,研磨后的颗粒细度小于0.015毫米,罐装为凹凸棒外墙乳胶漆的成品。

Claims (2)

1.一种凹凸棒外墙乳胶漆,其特征在于,凹凸棒外墙乳胶漆的配料按重量百分比由下列组分组成:膏状凹凸棒石粘土20~55%、苯丙乳液15~45%、超细重质碳酸钙5~35%、金红石型钛白粉1~10%、羟乙基纤维素0.5~5%、乙二醇0.5~5%、磷酸三丁酯0.01~2%和去离子水5~35%;
所述膏状凹凸棒石粘土的生产工艺是:(1)选用凹凸棒矿泥浆为主体原料,凹凸棒矿泥浆按重量百分比由下列组分组成:凹凸棒石粘土15~35%和水65~85%;(2)钠化处理:将凹凸棒矿泥浆输送到搅拌机内,添加氢氧化钠后进行搅拌,经过搅拌后的凹凸棒矿泥浆输送到钠化池中陈化1~7天;钠化配料按重量百分比由下列组分组成:凹凸棒矿泥浆95~99.5%和氢氧化钠0.5~5%;(3)酸化处理:将钠化后凹凸棒矿泥浆输送到搅拌机内,添加浓度为98%的硫酸后进行搅拌,经过搅拌后的凹凸棒矿泥浆输送到酸化池中陈化1~3天;酸化配料按重量百分比由下列组分组成:钠化后的凹凸棒矿泥浆92~99.5%和浓度为98%的硫酸0.5~8%;(4)水洗和筛去杂质:将酸化后的凹凸棒矿泥浆输送到沉淀池中,重新加水浸泡,用气泵冲翻,筛去杂质,沉淀后放出浸泡水,并将沉淀后的泥浆输送到成品池内,沉淀后的泥浆为膏状凹凸棒石粘土;水洗配料按重量百分比由下列组分组成:酸化后的凹凸棒矿泥浆25~65%和水35~75%;膏状凹凸棒石粘土按重量百分比由下列组分组成:凹凸棒石粘土5~40%和水60~95%;
所述凹凸棒矿造浆生产工艺是:将凹凸棒矿输入搅拌机内搅拌,经挤出机挤压成片状后,再次输入搅拌机内搅拌,经挤出机挤压成片状后自然晾晒,晾干的凹凸棒矿输送到原料池中浸泡,用气泵冲翻,沉淀后放出浸泡水,筛去杂质,输入半成品池中,重新加水浸泡,用气泵冲翻,沉淀后放出浸泡水,并将沉淀后的泥浆输送到成品池内,即为凹凸棒矿泥浆成品。
2.根据权利要求1所述的凹凸棒外墙乳胶漆的生产方法,其特征在于,①将凹凸棒外墙乳胶漆的配料加入粉碎打浆机内进行粉碎,粉碎打浆混合均匀后为凹凸棒外墙乳胶漆的混合物;②将步骤①获得的混合物输入高粘度真空搅拌机中,凹凸棒外墙乳胶漆的配料在真空下经过搅拌、分散、溶解、均质、乳化和消泡后为凹凸棒外墙乳胶漆的半成品;③将步骤②获得的凹凸棒外墙乳胶漆的半成品输入多功能胶体磨中进行研磨,研磨后的颗粒细度小于0.015毫米,罐装为凹凸棒外墙乳胶漆的成品。
CN2009100262963A 2009-03-27 2009-03-27 凹凸棒外墙乳胶漆 Expired - Fee Related CN101531495B (zh)