CN101508530B - Luminescence glass and method of producing the same - Google Patents

Luminescence glass and method of producing the same Download PDF

Info

Publication number
CN101508530B
CN101508530B CN2009101150912A CN200910115091A CN101508530B CN 101508530 B CN101508530 B CN 101508530B CN 2009101150912 A CN2009101150912 A CN 2009101150912A CN 200910115091 A CN200910115091 A CN 200910115091A CN 101508530 B CN101508530 B CN 101508530B
Authority
CN
China
Prior art keywords
strontium
luminescence
glass
light
coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009101150912A
Other languages
Chinese (zh)
Other versions
CN101508530A (en
Inventor
严海
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TAICANG GUANGMING GLASS PRODUCT CO Ltd
Original Assignee
TAICANG GUANGMING GLASS PRODUCT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TAICANG GUANGMING GLASS PRODUCT CO Ltd filed Critical TAICANG GUANGMING GLASS PRODUCT CO Ltd
Priority to CN2009101150912A priority Critical patent/CN101508530B/en
Publication of CN101508530A publication Critical patent/CN101508530A/en
Application granted granted Critical
Publication of CN101508530B publication Critical patent/CN101508530B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses luminescence glass and a preparation method thereof. The luminescence glass comprises a main body of the glass, the back side of the main body of the glass is provided with a luminescence strontium layer, and the other side of the luminescence strontium layer is provided with a waterproof layer. The preparation method comprises the following steps that: the back side of the main body of the glass is coated with luminescence strontium coating first, and then the dried luminescence strontium coating is coated with waterproof ink. A method for producing the luminescence strontium coating comprises the following steps that: a plasticizing agent is added into an epoxy resin, the plasticizing agent and the epoxy resin are melted together, then luminescence strontium powder and a curing agent are added into the solution, and the mixture is stirred evenly. The luminescence glass does not need to waste electric energy when providing beautiful nightscape; at the same time, the luminescence glass also reduces the limitation of power supply positions to ensure that the design and installation site of landscape lamps are more flexible and the landscape lamps have safer use.

Description

Luminescence glass and preparation method thereof
Technical field
The present invention relates to a kind of luminescence glass and preparation method thereof.
Background technology
Diversiform Landscape Lamp has been full of the night in city, no matter is that the lines of the tower pavilion in street, the park sketch the contours, or the moulding of font, pattern, the impression of often giving people U.S., the city in the night of dressing up.But such Landscape Lamp is luminous by consumed power often, when bringing beauty, is also expending a large amount of electric energy; People need also to consider that leading of supply lead put and the Electrical Safety problem when carrying out the Landscape Lamp design.Hold the light-storing material of light strontium, have that fluorescent lifetime is long, luminosity is high and advantage such as "dead" material,, can send the light of different colours by mixing different elements as a kind of new and effective green.
Summary of the invention
The purpose of this invention is to provide a kind of luminescence glass and preparation method thereof, can when beauty view at night is provided, also need not to waste electric energy; Reduced the restriction of position of source simultaneously, made that the design of Landscape Lamp and place of erection are more flexible and changeable, used safer.
Technical scheme of the present invention is:
A kind of luminescence glass comprises glass body, and the back side of described glass body is provided with holds light strontium layer, and the described opposite side that holds light strontium layer is provided with waterproof layer.
A kind of preparation method of luminescence glass: at first light strontium coating is held in coating at the glass body back side, and holding on the light strontium coating after doing applies waterproof ink again.
The further technical scheme of the present invention is:
A kind of luminescence glass comprises glass body, and the back side of described glass body is provided with holds light strontium layer, and the described opposite side that holds light strontium layer is provided with waterproof layer; Described waterproof layer is the white waterproof ink lay.
A kind of preparation method of luminescence glass, at first light strontium coating is held in coating at the glass body back side, and holding on the light strontium coating after doing applies waterproof ink again; The described making method of holding light strontium coating is: add fluidizer in Resins, epoxy, add after dissolving together again and hold light strontium powder and solidifying agent is stirred to evenly; Described fluidizer is a butylene phthalate; Described solidifying agent is a polyamide resin; The described light strontium that holds is strontium aluminate or strontium sulfide.
The shared weight percent of each composition is:
Resins, epoxy 32%~35%;
Hold light strontium 43%~50%;
Fluidizer 3%~5%;
Solidifying agent 15%~18%.
Advantage of the present invention is:
1. the light strontium that holds on the glass body of the present invention oneself absorbs luminous energy and savings when light is strong, just weaken and luminous automatically at dark at light, can be used to needs on the long-time luminous glass facility saves energy, environmental protection as urban landscape view etc.
2. the present invention is located between glass body and the waterproof ink layer in holding light strontium layer, be difficult for coming off from glass, simultaneously also with air insulated, be difficult for reacting long service life with other material.
3. waterproof ink layer of the present invention is a white, is holding light strontium layer when luminous, can not absorb light but light is reflected away, and makes luminosity bigger.
Description of drawings
Fig. 1 is the structural representation of luminescence glass specific embodiment of the present invention.
Wherein: 1 glass body; 2 hold light strontium layer; 3 waterproof layers.
Embodiment
Below in conjunction with drawings and Examples the present invention is further described:
Embodiment: as shown in Figure 1, a kind of luminescence glass comprises glass body 1, and the back side of described glass body 1 is provided with holds light strontium layer 2, and the described opposite side that holds light strontium layer 2 is provided with waterproof layer 3.This holds light strontium layer 2 and oneself absorb luminous energy and savings when light is strong, just weaken and luminous automatically at dark at light, can be used to needs on the long-time luminous glass facility saves energy, environmental protection as urban landscape view etc.
Described waterproof layer 3 is the white waterproof ink lay, is holding light strontium layer when luminous, can not absorb light but light is reflected away, and makes luminosity bigger.
A kind of preparation method of luminescence glass: at first light strontium coating is held in coating at glass body 1 back side, and holding on the light strontium coating after doing applies waterproof ink again.
The described making method of holding light strontium coating is: add fluidizer in Resins, epoxy, add after dissolving together again and hold light strontium powder and solidifying agent is stirred to evenly; Wherein the shared umber (by weight) of each composition is:
50 parts of Resins, epoxy;
Hold 60 parts in light strontium;
5 parts of fluidizers;
25 parts in solidifying agent.
Described fluidizer is a butylene phthalate; Described solidifying agent is a polyamide resin.
The described light strontium that holds is a strontium aluminate, and strontium aluminate is different from traditional sulfide type and radioactive rays excitated type noctilucent material fully, does not contain any harmful element, stable performance, and fluorescent lifetime is long.This material is a matrix with the aluminate material, has good Presentation Function at night.
The present invention can also need not to waste electric energy when beauty view at night is provided; Reduced the restriction of position of source simultaneously, made that the design of Landscape Lamp and place of erection are more flexible and changeable, used safer.

Claims (3)

1. luminescence glass, comprise glass body (1), it is characterized in that: the back side of described glass body (1) is provided with holds light strontium layer (2), and the described opposite side that holds light strontium layer (2) is provided with waterproof layer (3), and the described shared weight percent of each composition of light strontium layer (2) coating that holds is:
Resins, epoxy 32%~35%;
Hold light strontium 43%~50%;
Fluidizer 3%~5%;
Solidifying agent 15%~18%;
The described light strontium that holds is strontium aluminate or strontium sulfide;
Described fluidizer is a butylene phthalate; Described solidifying agent is a polyamide resin.
2. luminescence glass according to claim 1 is characterized in that: described waterproof layer (3) is the white waterproof ink lay.
3. the preparation method of the described luminescence glass of claim 1 is characterized in that: at first light strontium coating is held in coating at glass body (1) back side, and holding on the light strontium coating after doing applies waterproof ink again; The described making method of holding light strontium coating is: add fluidizer in Resins, epoxy, add after dissolving together again and hold light strontium powder and solidifying agent is stirred to evenly;
The shared weight percent of each composition is:
Resins, epoxy 32%~35%
Hold light strontium 43%~50%;
Fluidizer 3%~5%;
Solidifying agent 15%~18%;
The described light strontium that holds is strontium aluminate or strontium sulfide;
Described fluidizer is a butylene phthalate; Described solidifying agent is a polyamide resin.
CN2009101150912A 2009-03-16 2009-03-16 Luminescence glass and method of producing the same Expired - Fee Related CN101508530B (en)