CN101456943A - 一种无颗粒塑胶材料 - Google Patents

一种无颗粒塑胶材料 Download PDF

Info

Publication number
CN101456943A
CN101456943A CNA2009100007669A CN200910000766A CN101456943A CN 101456943 A CN101456943 A CN 101456943A CN A2009100007669 A CNA2009100007669 A CN A2009100007669A CN 200910000766 A CN200910000766 A CN 200910000766A CN 101456943 A CN101456943 A CN 101456943A
Authority
CN
China
Prior art keywords
component
percent
primer
mixed
weight ratio
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA2009100007669A
Other languages
English (en)
Other versions
CN101456943B (zh
Inventor
陈跃进
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Jrace Athletic Facilities Co.,Ltd.
Original Assignee
陈跃进
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 陈跃进 filed Critical 陈跃进
Priority to CN2009100007669A priority Critical patent/CN101456943B/zh
Publication of CN101456943A publication Critical patent/CN101456943A/zh
Application granted granted Critical
Publication of CN101456943B publication Critical patent/CN101456943B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种无颗粒塑胶材料,包括底胶和面胶,其组分分为甲、乙组分,甲组分的重量比组成为:聚醚多元醇77.4%,甲苯二异氰酸酯22.57%,苯甲酸氯0.03%;乙组分的重量比组成为:聚醚多元醇19.83%,二苯基甲烷二胺5.33%,喹啉铜0.07%,白炭黑0.36%,高岭土6.67%,滑石粉34.8%,氯化石蜡30%,抗氧化剂0.13%,紫外线吸收剂0.13%,颜料2.67%;上述组分经如下步骤制备:将甲组分按配方比例混合后,在85~90℃条件下反应2~3小时;将乙组分按配方比例混合后研磨成粘稠状胶液;底胶制作:将上述甲组分和乙组分按1∶4的比例混合,加入重量比为甲、乙组分混合物总和的30~35%的黑胶粒和8%的催化剂;面胶制作:将上述甲组分和乙组分按1∶3的比例混合。

Description

一种无颗粒塑胶材料
技术领域
本发明涉及一种无颗粒塑胶材料。
背景技术
目前,在地面上铺装塑胶材料的通常做法是:做底胶→刮面胶→撒防滑胶粒→回收防滑胶粒。这样的方法撒上去的防滑胶粒主要是靠自重粘结,因此用这种方法铺设而成的场地通常存在的问题是:撒防滑胶粒的温度和时间很难控制,即使控制得好,也会有20~25%防滑胶粒很快就脱落下来,影响塑胶场地的使用寿命;如果掌握不好就会造成防滑胶粒局部甚至大面积脱落而影响使用寿命。
发明内容
本发明的目的是为了克服以上不足,提供一种耐老化、施工工期短、质量稳定、耐磨损的无颗粒塑胶材料。
本发明的技术方案是:一种无颗粒塑胶材料,包括底胶和位于底胶上面的面胶,其组成分为甲组分、乙组分,甲组分的重量比组成为:
聚醚多元醇:77.4%
甲苯二异氰酸酯:22.57%
苯甲酸氯:0.03%
乙组分的重量比组成为:
聚醚多元醇:19.83%
二苯基甲烷二胺:5.33%
喹啉铜:0.07%
白炭黑:0.36%
高岭土:6.67%
滑石粉:34.8%
氯化石蜡:30%
抗氧化剂:0.13%
紫外线吸收剂:0.13%
颜料:2.68%
上述组分经如下步骤制备:(1)将甲组分按配方比例混合后,在85~90℃条件下反应2~3小时;(2)将乙组分按配方比例混合后研磨成粘稠状胶液;(3)底胶制作:将上述甲组分和乙组分按1∶4的比例混合,加入重量比为甲、乙组分混合物总和的30~35%的黑胶粒和8%的催化剂;(4)面胶制作:将上述甲组分和乙组分按1∶3的比例混合。
所述催化剂为环氧酸铅与环氧酸锌的等比例混合物。
所述底层的厚度为5~25mm。
所述面层的厚度为2~4mm。
本发明的有益效果是:底胶中的黑胶粒控制在30~35%,增加了塑胶材料的耐磨性和抗老化性,与传统的塑胶材料相比,本发明塑胶材料的使用寿命延长了4~5倍。
具体实施方式
一种无颗粒塑胶材料,包括底胶和位于底胶上面的面胶,其组成分为甲组分、乙组分,甲组分的重量组成为:
聚醚1000:77.4kg
聚醚2000:77.4kg
甲苯二异氰酸酯:45.14kg
苯甲酸氯:0.06kg
乙组分的重量组成为:
聚醚3050:135.31kg
聚醚300:3.5kg
二苯基甲烷二胺:37.31kg
喹啉铜:0.49kg
白炭黑:2.52kg
高岭土:46.69kg
滑石粉:243.6kg
氯化石蜡:210kg
抗氧化剂1010:0.91kg
UV-531:0.91kg
桔红:18.76kg
上述原料经如下步骤制备:(1)将甲组分放进反应釜在85~90℃条件下反应两小时;(2)将乙组分搅拌均匀后,研磨成粘稠状胶液;(3)底胶制作:将上述100kg甲组分和400kg乙组分混合,加入重量比为上述甲、乙组分混合物总和的30%的黑胶粒150kg和8%的催化剂40kg,搅拌均匀,随后将其铺装在施工场地上,用刮扒把胶均匀扒平,使胶浆均匀地覆盖施工场地,所述催化剂为:环氧酸铅与环氧酸锌的等比例混合物;(4)底胶固化后,将其表面打磨平整,并清理残留的胶粉;(5)面胶制作:将上述100kg甲组分和300kg乙组分混合均匀,铺在底胶上,凝固约30分钟后,在柔软的面胶上铺设压花模具,待面胶固化后,将表面的模具去除,这样增加了塑胶材料表面的摩擦系数,同时起到了美化的效果。
本发明塑胶材料可铺装在运动场地上,也可作为室内的装饰地板;本发明底胶中的黑胶粒控制在30~35%,增加了塑胶材料的耐磨性和抗老化性,与传统的塑胶材料相比,本发明塑胶材料的使用寿命延长了4~5倍。
下表是本发明一种无颗粒塑胶材料的物理性能方面的实测结果:
 
实测项目 实测结果
硬度(邵A),度 52
回弹值,% 26
压缩复原率,% 97
抗拉强度,MPa 0.8
扯断伸长率,% 122
阻燃性,级 1

Claims (4)

1.一种无颗粒塑胶材料,包括底胶和位于底胶上面的面胶,其特征是:其组成分为甲组分、乙组分,甲组分的重量比组成为:
聚醚多元醇:77.4%
甲苯二异氰酸酯:22.57%
苯甲酸氯:0.03%
乙组分的重量比组成为:
聚醚多元醇:19.83%
二苯基甲烷二胺:5.33%
喹啉铜:0.07%
白炭黑:0.36%
高岭土:6.67%
滑石粉:34.8%
氯化石蜡:30%
抗氧化剂:0.13%
紫外线吸收剂:0.13%
颜料:2.68%
上述组分经如下步骤制备:(1)将甲组分按配方比例混合后,在85~90℃条件下反应2~3小时;(2)将乙组分按配方比例混合后研磨成粘稠状胶液;(3)底胶制作:将上述甲组分和乙组分按1∶4的比例混合,加入重量比为甲、乙组分混合物总和的30~35%的黑胶粒和8%的催化剂;(4)面胶制作:将上述甲组分和乙组分按1∶3的比例混合。
2.根据权利要求1所述的一种塑胶跑道,其特征是:所述催化剂为环氧酸铅与环氧酸锌的等比例混合物。
3.根据权利要求1所述的一种塑胶跑道,其特征是:所述底层的厚度为5~25mm。
4.根据权利要求1所述的一种塑胶跑道,其特征是:所述面层的厚度为2~4mm。
CN2009100007669A 2009-01-12 2009-01-12 一种无颗粒塑胶材料 Expired - Fee Related CN101456943B (zh)