CN101406743A - 烫金边塑料扑克牌的生产方法 - Google Patents

烫金边塑料扑克牌的生产方法 Download PDF

Info

Publication number
CN101406743A
CN101406743A CNA2008102341240A CN200810234124A CN101406743A CN 101406743 A CN101406743 A CN 101406743A CN A2008102341240 A CNA2008102341240 A CN A2008102341240A CN 200810234124 A CN200810234124 A CN 200810234124A CN 101406743 A CN101406743 A CN 101406743A
Authority
CN
China
Prior art keywords
playing card
playing
thermoprint
blanks
sheet material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2008102341240A
Other languages
English (en)
Inventor
刘权
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YANGZHOU YONGQUAN PRINTING CO Ltd
Original Assignee
YANGZHOU YONGQUAN PRINTING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YANGZHOU YONGQUAN PRINTING CO Ltd filed Critical YANGZHOU YONGQUAN PRINTING CO Ltd
Priority to CNA2008102341240A priority Critical patent/CN101406743A/zh
Publication of CN101406743A publication Critical patent/CN101406743A/zh
Pending legal-status Critical Current

Abstract

本发明公开了扑克牌生产技术领域内的烫金边塑料扑克牌的生产方法,先按设计的牌张规格,在PVC片材上正反两面印刷扑克牌图案;用UV上光油红外线上光,再裁切成扑克牌坯件;然后将若干张扑克牌坯件叠合后,在磨切机上进行磨边加工,使扑克牌坯件尺寸规格一致,边缘光滑;再将磨边后的扑克牌坯件叠合后用夹具夹紧,再在烫金机上进行周边烫金加工,使扑克牌坯件周边形成的平面朝向烫印机的烫印头,直至四面均完成烫印,烫印温度为120-150℃;最后,松开夹具最后进行分牌包装。本发明方法简单易行,烫金边能够与扑克牌良好结合,不易磨损,所得产品抗拉、耐折弯,使用可靠,外表美观。本发明用于扑克牌的生产制造。

Description

烫金边塑料扑克牌的生产方法
技术领域
本发明涉及一种游戏工具的生产方法,特别涉及一种扑克牌的生产方法。
背景技术
现有技术中的扑克牌,一般为纸质,其在纸板上的正反两面分别印制扑克牌图案后,再进行裁切、打蜡处理后获得。其不足之处在于:制造扑克牌的纸板由多层纸制成,使用时相互之间容易剥离,影响使用寿命;此外,现有扑克牌使用一段时间后,牌体周边易变黑,影响美观。
发明内容
本发明的目的是提供一种烫金边塑料扑克牌的生产方法,使生产的扑克牌外形美观,使用寿命长。
本发明提供的烫金边塑料扑克牌的生产方法,依次包括如下步骤:
1)按设计的牌张规格,在PVC片材上正反两面印刷扑克牌图案,其中一面印刷识别图案,另一面印刷背纹图案;
2)将印刷好的PVC片材用UV上光油进行红外线上光;
3)将PVC片材按印刷位置进行裁切,形成若干张扑克牌坯件;
4)将若干张扑克牌坯件叠合在一起,在磨切机上进行磨边加工,使扑克牌坯件尺寸规格一致,边缘光滑;
5)将磨边后的扑克牌坯件若干张叠合整齐后用夹具夹紧,再在烫金机上进行周边烫金加工,烫印加工时,使叠合在一起的扑克牌坯件周边形成的平面朝向烫印机的烫印头,一个平面烫印后翻转扑克牌再烫印其他面,直至四面均完成烫印,烫印温度为120-150℃;
6)松开夹具,将烫印后形成的成品扑克牌进行分牌包装。
本发明方法简单易行,烫金边能够与扑克牌良好结合,不易磨损,牌体由PVC塑料制成,其抗拉、耐折弯,使用可靠,金黄色的烫金层外表美观,可以保护牌体侧面,使其不会变黑,变黄,不会剥离;此外,该扑克牌与现有的扑克牌能形成明显对比,可使用于娱乐竞技场所,防止出现偷换牌现象。
具体实施方式
实施例1
烫金边塑料扑克牌的一种生产方法,依次包括如下步骤:
1)按设计的牌张规格,在PVC片材上正反两面印刷扑克牌图案,其中一面印刷识别图案,另一面印刷背纹图案;
2)将印刷好的PVC片材用UV上光油进行红外线上光;
3)将PVC片材按印刷位置进行裁切,形成若干张扑克牌坯件;
4)将若干张扑克牌坯件叠合在一起,在磨切机上进行磨边加工,使扑克牌坯件尺寸规格一致,边缘光滑;
5)将磨边后的扑克牌坯件若干张叠合整齐后用夹具夹紧,再在烫金机上进行周边烫金加工,烫印加工时,使叠合在一起的扑克牌坯件周边形成的平面朝向烫印机的烫印头,一个平面烫印后翻转扑克牌再烫印其他面,直至四面均完成烫印,烫印温度为120℃;
6)松开夹具,将烫印后形成的成品扑克牌进行分牌包装。
实施例2
烫金边塑料扑克牌的又一种生产方法,依次包括如下步骤:
1)按设计的牌张规格,在PVC片材上正反两面印刷扑克牌图案,其中一面印刷识别图案,另一面印刷背纹图案;
2)将印刷好的PVC片材用UV上光油进行红外线上光;
3)将PVC片材按印刷位置进行裁切,形成若干张扑克牌坯件;
4)将若干张扑克牌坯件叠合在一起,在磨切机上进行磨边加工,使扑克牌坯件尺寸规格一致,边缘光滑;
5)将磨边后的扑克牌坯件若干张叠合整齐后用夹具夹紧,再在烫金机上进行周边烫金加工,烫印加工时,使叠合在一起的扑克牌坯件周边形成的平面朝向烫印机的烫印头,一个平面烫印后翻转扑克牌再烫印其他面,直至四面均完成烫印,烫印温度为150℃;
6)松开夹具,将烫印后形成的成品扑克牌进行分牌包装。

Claims (1)

1、烫金边塑料扑克牌的生产方法,依次包括如下步骤:
1)按设计的牌张规格,在PVC片材上正反两面印刷扑克牌图案,其中一面印刷识别图案,另一面印刷背纹图案;
2)将印刷好的PVC片材用UV上光油进行红外线上光;
3)将PVC片材按印刷位置进行裁切,形成若干张扑克牌坯件;
4)将若干张扑克牌坯件叠合在一起,在磨切机上进行磨边加工,使扑克牌坯件尺寸规格一致,边缘光滑;
5)将磨边后的扑克牌坯件若干张叠合整齐后用夹具夹紧,再在烫金机上进行周边烫金加工,烫印加工时,使叠合在一起的扑克牌坯件周边形成的平面朝向烫印机的烫印头,一个平面烫印后翻转扑克牌再烫印其他面,直至四面均完成烫印,烫印温度为120-150℃;
6)松开夹具,将烫印后形成的成品扑克牌进行分牌包装。
CNA2008102341240A 2008-11-03 2008-11-03 烫金边塑料扑克牌的生产方法 Pending CN101406743A (zh)