CN101377091A - 木塑强化地板 - Google Patents
木塑强化地板 Download PDFInfo
- Publication number
- CN101377091A CN101377091A CNA2008101214411A CN200810121441A CN101377091A CN 101377091 A CN101377091 A CN 101377091A CN A2008101214411 A CNA2008101214411 A CN A2008101214411A CN 200810121441 A CN200810121441 A CN 200810121441A CN 101377091 A CN101377091 A CN 101377091A
- Authority
- CN
- China
- Prior art keywords
- wood
- interlayer
- energy
- insulating layer
- plastic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种木塑强化地板,由耐磨表层和木塑夹层复合构成,木塑夹层包括木塑上夹层和木塑下夹层,在木塑上夹层和木塑下夹层之间填充节能隔热层,节能隔热层的两侧分别形成可相互配合的凹槽和凸缘,节能隔热层采用高分子低发泡材料PVC树脂,耐磨表层采用三聚氰胺装饰材料及水晶高耐磨PVC材料。本发明克服了现有技术中普通木制地板容易变形、开裂、霉变、虫蛀;复合地板的化学成分复杂易膨胀、脱层、霉变、污染环境的缺陷,通过上述设计,木塑夹层和节能隔热层可以一次性挤出成型,不需胶粘剂粘合,减少了污染,具有结构简单、不易变形,耐火防水,环保节能的优点,适合在任何环境中安装使用。
Description
所属技术领域
本发明涉及一种木塑强化地板。
背景技术
传统的木制地板,对使用环境的要求很高,在潮湿的环境下容易膨胀变形、霉变、虫蛀,在干燥的环境下又容易收缩变形、开裂,因此很难大范围地使用。而复合地板的化学成分复杂,特别是含有的甲醛成分释放时间很长,严重影响人体健康,在潮湿的环境下易膨胀脱层。
发明内容
为了克服现有技术中普通木制地板容易变形、开裂、霉变、虫蛀;复合地板的化学成分复杂易膨胀、脱层、霉变、污染环境、其有害物质损害人体健康的问题,本发明提供一种木塑强化地板,该木塑强化地板结构简单、安装方便、不易变形、耐磨性高、耐火防水、环保节能、生产成本较低、适合大范围使用,而且其使用寿命长,可回收利用,在施工过程中不造成环境的二次污染。
本发明解决其技术问题所采用的技术方案是:由耐磨表层和木塑夹层复合构成,木塑夹层包括木塑上夹层和木塑下夹层,在木塑上夹层和木塑下夹层之间填充节能隔热层,节能隔热层的两侧分别形成可相互配合的凹槽和凸缘。
节能隔热层采用高分子低发泡材料PVC树脂。
耐磨表层采用三聚氰胺装饰材料及水晶高耐磨PVC材料。
木塑夹层由混合的塑料粉末和木材纤维加热挤出成型。
本发明通过上述具体设计,木塑夹层和节能隔热层可以一次性挤出成型,不需胶粘剂粘合,减少了污染,具有结构简单、不易变形,耐火防水,环保节能的优点,适合在任何环境中使用。本产品在施工过程中不造成二次污染,边角料可回收再利用。
附图说明
以下结合附图和实施例说明本发明的详细内容。
附图是本发明的结构示意图。
具体实施方式
如图所示,本发明由耐磨表层1和木塑夹层2复合构成,上述复合结构可以采用环保胶的热吻合工艺完成。耐磨表层1采用三聚氰胺防火材料及水晶高耐磨PVC材料,具有耐火防水的使用效果,而且硬度高,耐磨性强。木塑夹层2包括木塑上夹层2A和木塑下夹层2B,木塑夹层2由混合的塑料粉末和木材纤维加热挤出成型。木塑上夹层2A和木塑下夹层2B之间填充节能隔热层3,节能隔热层3的两侧分别形成可相互配合的凹槽4和凸缘5。节能隔热层3采用高分子低发泡材料PVC树脂。木塑夹层2和节能隔热层3通过挤出成型工艺连成一体,不需要胶粘剂粘合,零污染,而且无甲醛等有害化学物质的存在,是一种环保安全的装饰材料。
Claims (4)
1、一种木塑强化地板,其特征是由耐磨表层(1)和木塑夹层(2)复合构成,木塑夹层(2)包括木塑上夹层(2A)和木塑下夹层(2B),在木塑上夹层(2A)和木塑下夹层(2B)之间填充节能隔热层(3),节能隔热层(3)的两侧分别形成可相互配合的凹槽(4)和凸缘(5)。
2、根据权利要求1所述的木塑强化地板,其特征是节能隔热层(3)采用高分子低发泡材料PVC树脂。
3、根据权利要求1所述的木塑强化地板,其特征是耐磨表层(1)采用三聚氰胺装饰材料及水晶高耐磨PVC材料。
4、根据权利要求1或2或3所述的木塑强化地板,其特征是木塑夹层(2)由混合的塑料粉末和木材纤维加热挤出成型。