CN101307576A - 一种耐老化高分子强力绳的制作方法 - Google Patents

一种耐老化高分子强力绳的制作方法 Download PDF

Info

Publication number
CN101307576A
CN101307576A CNA2008100248251A CN200810024825A CN101307576A CN 101307576 A CN101307576 A CN 101307576A CN A2008100248251 A CNA2008100248251 A CN A2008100248251A CN 200810024825 A CN200810024825 A CN 200810024825A CN 101307576 A CN101307576 A CN 101307576A
Authority
CN
China
Prior art keywords
aging
hshm
high molecule
sleeves
aramid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2008100248251A
Other languages
English (en)
Inventor
袁剑峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA2008100248251A priority Critical patent/CN101307576A/zh
Publication of CN101307576A publication Critical patent/CN101307576A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种耐老化高分子强力绳的制作方法,它包括以下步骤:步骤一,准备HSHM-PE纤维,在编织机上将HSHM-PE纤维加工形成承载芯;步骤二,将芳纶通过编织机编织在承载芯的外表面形成芳纶套作为隔热防护套;步骤三,在通过注塑机在芳纶套的外表面注有PVC层作为防老化套。本发明制作的耐老化高分子强力绳的可以大大缓解因老化产生的强力损失从而延长使用寿命。

Description

一种耐老化高分子强力绳的制作方法
技术领域
本发明涉及一种耐老化高分子强力绳的制作方法。
技术背景
目前世界上使用的高分子强力绳的承载部分直接暴露在空气,日光,风雨,盐雾等严酷环境下,因此随着时间的推移强力绳很容易老化,破断拉力下降非常快,因此很容易造成安全事故。
发明内容
本发明提供了一种耐老化高分子强力绳的制作方法,它制作的耐老化高分子强力绳的可以大大提高绳体的强度,延长使用寿命。
本发明采用了以下技术方案:一种耐老化高分子强力绳的制作方法,它包括以下步骤:步骤一,准备HSHM-PE纤维,在编织机上将HSHM-PE纤维加工形成承载芯;步骤二,将芳纶通过编织机编织在承载芯的外表面形成芳纶套作为隔热防护套;步骤三,在通过注塑机在芳纶套的外表面注有PVC层作为防老化套。
本发明步骤三中注塑时的温度为150-200℃。
本发明具有以下有益效果:本发明中承载芯采用HSHM-PE纤维,它具有强度高,重量轻,抗老化指标好,耐磨,耐割,耐酸碱,耐油污等优点,这样可以大大提高吊带的强度和使用寿命。本发明中在承载芯外设有隔热防护套,隔热防护套为芳纶套,它可以有效地阻止制作过程中高温对承载芯的造成伤害,在芳纶套外层设有防老化护套,防老化护套为PVC层,它可以有效隔绝空气,日光,风雨,盐雾等,大大减少了绳体因老化产生的破断拉力下降,有效地延长了绳体的使用寿命,减少了更换周期。
具体实施方式
本发明为一种耐老化高分子强力绳的制作方法,它包括以下步骤:步骤一,准备高分子高模量的HSHM-PE纤维,在编织机上将HSHM-PE纤维加工形成承载芯;步骤二,将芳纶通过编织机编织在承载芯的外表面形成芳纶套作为隔热防护套;步骤三,在通过注塑机在芳纶套的外表面注有PVC层作为防老化套,注塑时的温度为150-200℃。本发明制得的耐老化高分子强力绳,它包括承载芯,承载芯为HSHM-PE承载芯,在承载芯的外套有隔热防护套,隔热防护套为芳纶套,在隔热防护套的外套有防老化护套,防老化护套为PVC套。

Claims (2)

1、一种耐老化高分子强力绳的制作方法,它包括以下步骤:
步骤一,准备HSHM-PE纤维,在编织机上将HSHM-PE纤维加工形成承载芯;
步骤二,将芳纶通过编织机编织在承载芯的外表面形成芳纶套作为隔热防护套;
步骤三,在通过注塑机在芳纶套的外表面注有PVC层作为防老化套。
2、根据权利要求1所述的耐老化高分子强力绳的制作方法,其特征是所述的步骤三中注塑时的温度为150-200℃。
CNA2008100248251A 2008-05-15 2008-05-15 一种耐老化高分子强力绳的制作方法 Pending CN101307576A (zh)