CN101302429A - 焦炉炉门维修方法 - Google Patents
焦炉炉门维修方法 Download PDFInfo
- Publication number
- CN101302429A CN101302429A CNA2008103025715A CN200810302571A CN101302429A CN 101302429 A CN101302429 A CN 101302429A CN A2008103025715 A CNA2008103025715 A CN A2008103025715A CN 200810302571 A CN200810302571 A CN 200810302571A CN 101302429 A CN101302429 A CN 101302429A
- Authority
- CN
- China
- Prior art keywords
- oven door
- door body
- brick
- knife
- maintenance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种效率更高的焦炉炉门维修方法。其不同于常用方法之处在于:将炉门导出到检修架上后,用临时固定件将炉门本体和砖槽固定连接,再松解炉门本体连接螺栓和砖槽连接螺栓;然后对刀边、刀边腹板进行拆卸、检修和重新安装;待炉门本体连接螺栓和砖槽连接螺栓重新紧固后再拆除临时固定件。由于检修中对炉门本体和砖槽不进行拆卸,有针对性地对经常易损坏的刀边和刀边腹板部分进行大修,能够保证检修质量;同时,由于不需要对衬砖进行清理和重新砌装,检修过程中炉门本体的砖槽之间不发生相对位移,方便各拆卸部件的对位和复原安装,又能缩短检修时间,降低维修成本,尤其适合于焦炉炉门大修时应用。
Description
技术领域
本发明涉及焦炉维护技术领域,尤其是一种焦炉炉门维修方法。
背景技术
目前,焦炉的机侧、焦侧炉门多采用悬挂式空冷炉门、弹性刀边、弹簧门栓。该炉门优点是炉门对位位置重复性好,弹性刀边能始终保持一定压力,有效杜绝炉门冒烟冒火。生产过程中,弹性刀边会因操作中的碰撞以及机械磨损等原因损坏,导致砖槽螺栓孔冒烟;炉门刀边腹板会因炉门摘、装操作导致疲劳开裂或开焊,因此须定期对炉门进行整体的维护修理
现有技术中,炉门整体大修多采用“拆装”式修理方法,该方法包括以下步骤:将炉门倒出放到检修架上;清理炉门砖槽及衬砖;将炉门旋转180°,松解炉门本体连接螺栓和砖槽连接螺栓;吊离炉门滑板和刀边腹板;检修砖槽、炉门筋板、刀边腹板、滑块;调节对应的顶压座,拧紧各连接螺栓;将炉门再次旋转180°,清扫炉门砖槽后砌筑炉门衬砖,修复刀边、调节对应的顶压座,将炉门吊装复位。
该方法检修时,能对炉门所有部位进行检修,检修比较全面。但多数情况下,由于砖槽和衬砖部分不易受损,对炉门进行全面修复是不必要的,且炉门衬砖的安装过程复杂,效率不高,原材料和动力能源消耗大。
如在检修过程中对炉门砖槽不加任何保护措施,砖槽与炉门本体分离后,滑槽与砖槽的连接螺栓会松动移位,安装时极难对准位置,造成炉门整体密封不严密,安装过程劳动强度,效率低。
因此,研究开发一种对炉门砖槽、衬砖具有保护性措施,能有效降低劳动强度和操作简单的焦炉炉门维修方法显得十分必要。
发明内容
为了克服现有炉门维修方法效率低的不足,本发明所要解决的技术问题是提供一种效率更高的焦炉炉门维修方法。
本发明解决其技术问题所采用的技术方案是:焦炉炉门维修方法,包括以下步骤:
步骤a:将炉门导出到检修架上;
步骤b:用临时固定件将炉门本体(1)和砖槽(11)相互固定连接,再松解炉门本体连接螺栓(6)和砖槽连接螺栓(7);
步骤c:对刀边腹板(12)进行拆卸、检修和重新安装;
步骤d:重新紧固砖槽连接螺栓(7)和炉门本体连接螺栓(6),拆除步骤a中的临时固定件,再检修刀边(13);
步骤e:调节对应的顶压座,将炉门吊装复位。
本发明的有益效果是:对炉门本体和砖槽不进行拆卸,有针对性地对经常易损坏的刀边和刀边腹板部分进行大修,能够保证检修质量;同时,由于不需要对衬砖进行清理和重新砌装,检修过程中炉门本体的砖槽之间不发生相对位移,方便各拆卸部件的对位和复原安装,又能缩短检修时间,降低维修成本。
附图说明
图1是焦炉炉门的主视图。
图2是图1的俯视图。
图3是本发明的示意图。图中标记为,1-炉门本体,2-门栓,3-刀边及刀边腹板,4-滑槽及滑块,5-顶压座,6-炉门本体连接螺栓,7-砖槽连接螺栓,8-上部砖槽,9-中部砖槽,10-下部砖槽,11-砖槽,12-刀边腹板,13-刀边,14-钢丝绳,15-炉门筋板。
具体实施方式
下面结合附图和实施例对本发明进一步说明。
如图1、图2和图3所示,本发明的焦炉炉门维修方法,包括以下步骤:
步骤a:将炉门导出到检修架上;
步骤b:用临时固定件将炉门本体(1)和砖槽(11)相互固定连接,再松解炉门本体连接螺栓(6)和砖槽连接螺栓(7);
步骤c:对刀边腹板(12)进行拆卸、检修和重新安装;
步骤d:重新紧固砖槽连接螺栓(7)和炉门本体连接螺栓(6),拆除步骤a中的临时固定件,再检修刀边(13);
步骤e:调节对应的顶压座,将炉门吊装复位。
考虑到配备专门设计的固定件成本较高,步骤b中,临时固定件采用常见的钢丝绳14,钢丝绳14将炉门本体1和砖槽11绑定连接,实际绑定作业时,可用手拉葫芦等工具调整其预紧力。
炉门本体1和砖槽11绑定后,为方便作业,还可将炉门本体1和砖槽11固定在检修架上。
另外,步骤a将炉门导出到检修架上之后,步骤b用临时固定件将炉门本体1和砖槽11固定连接之前,可以将炉门整体翻转90°,使炉门衬砖朝下放置,以方便检修作业,即,使需要吊离检修的炉门筋板15和刀边腹板12的退出方向朝上。
实施例
如图1、图2和图3所示,本发明的焦炉炉门维修方法,先将待大修炉门倒出放到检修架上,利用检修架将炉门旋转180°后,将炉门吊出,然后为了后续操作方便可将炉门翻转90°,使炉门衬砖朝下放置;利用钢丝绳14等临时固定件将炉门本体1和砖槽11绑定连接,如用钢丝绳14固定应保证钢丝绳14有预应力,使炉门本体1和砖槽11之间不发生相对位移;再松掉炉门本体连接螺栓6和炉门砖槽螺栓7,将炉门筋板15和刀边腹板12吊出;待刀边腹板12等损坏部位修复好后,依次将刀边腹板12、刀边13、炉门筋板15重新对位安装复原并按顺序逐一拧紧砖槽连接螺栓7和炉门本体连接螺栓6;拆除钢丝绳14等临时固定件;调节对应的炉门顶压座5,将炉门旋转180°并退出检修架;一般还应清扫炉门砖槽11;再修复刀边13,调节对应的顶压座5,将炉门吊装复位。
采用本发明的焦炉炉门维修方法,能够缩短维修时间,提高维修效率。
Claims (4)
1.焦炉炉门维修方法,包括以下步骤:
步骤a:将炉门导出到检修架上;
步骤b:用临时固定件将炉门本体(1)和砖槽(11)相互固定连接,再松解炉门本体连接螺栓(6)和砖槽连接螺栓(7);
步骤c:对刀边腹板(12)进行拆卸、检修和重新安装;
步骤d:重新紧固砖槽连接螺栓(7)和炉门本体连接螺栓(6),拆除步骤a中的临时固定件,再检修刀边(13);
步骤e:调节对应的顶压座,将炉门吊装复位。
2.如权利要求1所述的焦炉炉门维修方法,其特征是:步骤b中的临时固定件采用钢丝绳(14),钢丝绳(14)将炉门本体(1)和砖槽(11)绑定连接。
3.如权利要求2所述的焦炉炉门维修方法,其特征是:炉门本体(1)和砖槽(11)绑定连接后,再与检修架固定连接。
4.如权利要求1、2或3所述的焦炉炉门维修方法,其特征是:步骤a和步骤b之间进行如下步骤:将炉门整体翻转90°,使炉门衬砖朝下放置。