CN101293786A - 一种荒料真空补胶工艺 - Google Patents
一种荒料真空补胶工艺 Download PDFInfo
- Publication number
- CN101293786A CN101293786A CNA2008100387555A CN200810038755A CN101293786A CN 101293786 A CN101293786 A CN 101293786A CN A2008100387555 A CNA2008100387555 A CN A2008100387555A CN 200810038755 A CN200810038755 A CN 200810038755A CN 101293786 A CN101293786 A CN 101293786A
- Authority
- CN
- China
- Prior art keywords
- vacuum
- waste
- glue
- dali
- stone material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明涉及一种荒料真空补胶工艺,可以有效地解决现有技术中所存在的大理石荒料形状不规则、裂缝多、加工困难等问题。本发明可以将大理石荒料在正式加工之前先修补成形状规则、无缝隙的整料,使大理石荒料能够顺利地加工完成。
Description
技术领域
本发明涉及一种建材加工工艺,特别是一种荒料真空补胶工艺。
背景技术
大理石是一种常见的建筑材料,纹理细腻,图案精美,深受广大人民所喜爱,被广泛应用于广场建设、房间装潢、工艺品雕刻等。现有技术的大理石的开采工艺往往都比较简单,采得的大理石荒料一般是不规则的形状,而且荒料上还会产生裂缝或缺口。而加工大理石的机器一般都是为形状规则的荒料准备的,带有裂缝或缺口的荒料在加工时容易产生问题,报废率较高,甚至还会影响机器的寿命,为了使大理石荒料能够顺利地加工完成,就需要将荒料在正式加工之前先修补成形状规则、无缝隙的整料。
发明内容
本发明的目的是解决现有技术中所存在的大理石荒料形状不规则、裂缝多、加工困难等问题,提供一种荒料真空补胶工艺,其特征在于,包括如下步骤:
1)将大理石荒料置于荒料车上;
2)用高压空气枪或者高压水枪将大理石荒料的外表面和裂缝内部清理干净;
3)将清洗后的大理石荒料用荒料车送入烘房内,启动烘干设备,直到大理石荒料被烘干为止;
4)将烘干的大理石荒料用荒料车从烘房内运出,将大理石荒料置于一个与大理石荒料大小相近的无盖容器内;
5)将大理石荒料和无盖容器用荒料车送入真空荒料机内;
6)取若干装有胶水的胶水容器放在真空荒料机外,每个胶水容器开口处设有长导管,长导管与胶水容器连接处密封良好,长导管上的开关为关闭状态;
7)将胶水容器的长导管的前端通过真空荒料机的密封开口置于无盖容器内;
8)用真空泵将真空荒料机内的空气抽出,使得真空荒料机的内部为真空或近似真空;
9)真空荒料机的内部达到一定值的真空度后,打开长导管上的开关,灌入胶水,直到胶水溢过容器中的大理石荒料为止;
10)将真空荒料机打开,使得空气流入真空荒料机内;
11)将补胶后大理石荒料和无盖容器用荒料车运至堆场,在自然条件下静置5-7天,使胶水固化;
12)将无盖容器拆开,大理石荒料补胶完成。
所述的胶水可以为不饱和环氧树脂,所述的胶水容器的数量为一个或一个以上。所述的一定数值的真空度是指真空度数值在-0.08MPa~-0.098MPa之间。本发明的优点在于:本发明简单方便,成本低廉,有效地将大理石荒料的残缺填补完整,便于大理石荒料的加工。
具体实施方式
本发明涉及一种荒料真空补胶工艺,其特征在于,包括如下步骤:
1)将大理石荒料置于荒料车上;
2)用高压空气枪或者高压水枪将大理石荒料的外表面和裂缝内部清理干净;
3)将清洗后的大理石荒料用荒料车送入烘房内,启动烘干设备,直到大理石荒料被烘干为止;
4)将烘干的大理石荒料用荒料车从烘房内运出,将大理石荒料置于一个与大理石荒料大小相近的无盖容器内;
5)将大理石荒料和无盖容器用荒料车送入真空荒料机内;
6)取若干装有胶水的胶水容器放在真空荒料机外,每个胶水容器开口处设有长导管,长导管与胶水容器连接处密封良好,长导管上的开关为关闭状态;
7)将胶水容器的长导管的前端通过真空荒料机的密封开口置于无盖容器内;
8)用真空泵将真空荒料机内的空气抽出,使得真空荒料机的内部为真空或近似真空;
9)真空荒料机的内部达到一定值的真空度后,打开长导管上的开关,灌入胶水,直到胶水溢过容器中的大理石荒料为止;
10)将真空荒料机打开,使得空气流入真空荒料机内;
大气压力将胶水压入大理石荒料的每一条缝隙。
11)将补胶后大理石荒料和无盖容器用荒料车运至堆场,在自然条件下静置5-7天,使胶水固化;
12)将无盖容器拆开,大理石荒料补胶完成。
所述的胶水可以为不饱和环氧树脂,所述的胶水容器的数量为一个或一个以上,具体采用胶水的量取决于大理石荒料的大小和大理石荒料的残缺程度。所述的框架可以为三合板或硬塑料等,防水性能良好。
真空度数值是表示出真空系统内的气体压强实际数值与大气压强的差值,其单位一般选用Pa或MPa。
所述的一定值的真空度是指真空度数值在-0.08MPa~-0.098MPa之间。
本发明采用了在真空条件下完成灌胶的技术,合理利用大气压力将胶水压入大理石荒料的每一条缝隙中,最后得到无缝隙且易加工的大理石材料。
本发明工艺不但适用于大理石荒料,也适用于其他各种石料。
Claims (4)
1、一种荒料真空补胶工艺,其特征在于,包括如下步骤:
1)将大理石荒料置于荒料车上;
2)用高压空气枪或者高压水枪将大理石荒料的外表面和裂缝内部清理干净;
3)将清洗后的大理石荒料用荒料车送入烘房内,启动烘干设备,直到大理石荒料被烘干为止;
4)将烘干的大理石荒料用荒料车从烘房内运出,将大理石荒料置于一个与大理石荒料大小相近的无盖容器内;
5)将大理石荒料和无盖容器用荒料车送入真空荒料机内;
6)取若干装有胶水的胶水容器放在真空荒料机外,每个胶水容器开口处设有长导管,长导管与胶水容器连接处密封良好,长导管上的开关为关闭状态;
7)将胶水容器的长导管的前端通过真空荒料机的密封开口置于无盖容器内;
8)用真空泵将真空荒料机内的空气抽出,使得真空荒料机的内部为真空或近似真空;
9)真空荒料机的内部达到一定值的真空度后,打开长导管上的开关,灌入胶水,直到胶水溢过容器中的大理石荒料为止;
10)将真空荒料机打开,使得空气流入真空荒料机内;
11)将补胶后大理石荒料和无盖容器用荒料车运至堆场,在自然条件下静置5-7天,使胶水固化;
12)将无盖容器拆开,大理石荒料补胶完成。
2、如权利要求1所述的一种荒料真空补胶工艺,其特征在于:所述的胶水为不饱和环氧树脂。
3、如权利要求1所述的一种荒料真空补胶工艺,其特征在于:所述的胶水容器的数量为一个或一个以上。
4、如权利要求1所述的一种荒料真空补胶工艺,其特征在于:所述的一定值的真空度是指真空度数值在-0.08MPa~-0.098MPa之间。