CN101266204B - 纱线绳带耐磨,针织绒线起球,雪尼尔线脱绒测定仪 - Google Patents
纱线绳带耐磨,针织绒线起球,雪尼尔线脱绒测定仪 Download PDFInfo
- Publication number
- CN101266204B CN101266204B CN200710129935XA CN200710129935A CN101266204B CN 101266204 B CN101266204 B CN 101266204B CN 200710129935X A CN200710129935X A CN 200710129935XA CN 200710129935 A CN200710129935 A CN 200710129935A CN 101266204 B CN101266204 B CN 101266204B
- Authority
- CN
- China
- Prior art keywords
- yarn
- chenille
- instrument
- depilating
- balling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明的名称是纱线绳带耐磨,针织绒线起球,雪尼尔线脱绒测定仪。它是纺织领域一种测定纱线等耐磨性能的仪器。目前测定纱线耐磨性能的仪器性能比较单一;只能与砂纸或者与金属摩擦。本发明采用新概念,它通过机械装置使纱线往复运动,采用可更换摩擦介质座,使被测物可与各种介质摩擦,如软木辊、橡胶辊、毛毡辊、钢针等等。可方便模拟生产过程,或服用过程中纱线的耐磨性能。目前测定针织绒线起球与雪尼尔线脱绒,必须先织成布再进行测定,这种方法费工费时准确性差。本发明采用电子探测装置,可以不用织布,直接测定针织绒线起球与雪尼尔线脱绒。本仪器测定结果全部用数字表达、准确度高,具有广泛用途。
Description
技术领域
本发明是一种多功能纺织仪器,用来测试纱线(线带、绳缆)耐磨,毛线、针织绒起球,雪尼尔线脱绒。
背景技术
1、耐磨试验
世界上现有的纱线耐磨测定仪,概括有以下几种:
1、国产LFY-109多功能纱线耐磨测定仪,它的缺点主要是单一性,只能将纱线与砂纸摩擦,不能模拟生产过程中(例如纱线通过织造钢筘时)的磨擦性能,也不能模拟在服用过程中纱线与其它物质(木头、橡胶、金属、皮革、织物)等的磨擦性能。
2、英国锡来研究所(SHIRLEY-SDL)Y027纱线耐磨性测试仪式。这是国际上通用的仪器,它的缺点与上述国产仪器基本相同。
3、新西兰郎兹研究所(WRONZ)纱线耐磨测试仪,采用纱线与金属磨擦,它主要用来模拟纱线在织造过程中通过钢筘的磨擦性能,用途比较单一。
2、起球试验
到目前为止世界上没有发现有直接测定纱线起球的仪器,只有测定织物起球的仪器,也就是说必须把纱线织成织物,然后间接地测定纱的起球性能。
国产有YG511型起球仪,英国ICI起球测试仪,基本原理结构相同。它将待试的织物包在橡胶辊上,放进内壁是软木板的六面体滚筒内自由翻滚。定时取出后对比照片标样,评定等级。此种办法的缺点是
1、占地费时,必须配备各种针号的针织机,还需人工织片。
2、试样用人工目测评定,误差大。
3、目前有机硅大量用于针织物后整理,带有有机硅的织片与滚筒内的软木板磨擦后沾污了软木板,很快使软木板变得十分光滑,失去磨擦力,严重影响测试正确性。
3、雪尼尔线脱绒试验
雪尼尔线(一种像玻璃试管刷子结构的纱线)手感光泽好,保暖等优点,广泛应用于针织物,家用织物。目前我国产量在世界上占绝时优势,大量出口,但是质量参差不齐,许多产品因脱绒严重影响质量,影响信誉,影响出口。因此急需制订标准,控制质量,但找不到测试纱线脱绒的仪器,找不到标准。只能来用织片的办法,通过马丁代尔(Martindale)国产YG401C型织物耐磨仪进行间接测试,刚通过国家试用标准。用此法的缺点是
1、占地费时,由于要织片,实验室需要备有不同规格的针织机,人工织成样片。
2、仪器磨擦时间长,织片面积小(四个头加起来没有女同志的手掌大)试样代表性差。
3、磨后目测和秤重误差大。
4、不同支数,不同混纺纤维,用不同的针织机密度不同,难以制订可行的标准。
5、磨料只能采用英国进口的毛布,价格贵。
发明内容
本发明目的是提供一台多功能纱线测试仪,用它可以分别测试纱线(线带、绳缆)的耐磨性能、毛线、针织绒的起球性能、雪尼尔线的脱绒性能。
基本原理与构造
本仪器的基本原理与构造如图所示
1、驱动马达、2、同步带 3、卷绕滚筒 4、样线 5、导辊 6、可换磨擦介质座,座上共有10(20)头。每头磨擦介质共4个或多个,均匀固定在介质座上。磨擦介质座上有定 位孔,可以精确地方便地固定在面板上,样线通过其间如图所示。7、光电探头组每头一套,由以下部分组成①多级恒定光源②接收器。③转换开关,分别是耐磨、起球、脱绒三挡④一对精确定位导纱器,保证纱线在探头中央通过,导纱器的孔径根据纱支,要作变换。8、专用夹头 9、引线 10、导辊 11、面板 12、感应探头 13、重锤 14、滑槽 15、机座
一、测定纱线的耐磨性能
说明如下:首先将光电探头调节在耐磨挡(光电断开),将样线4用专用夹头8夹住,通过磨擦介质座6上的磨擦介质(假定钢针),通过导纱器经导辊5固定在卷绕滚筒3上。马达1启动后拉动重锤13,重锤13起张力作用同时用它感应感应探头12,产生倒顺转,同时带动样线往复运动。样线运动时,通过固定在机面上的磨擦介质进行磨擦,采用不同的磨擦介质例如织物、橡胶辊、砂辊、毛毡、钢针、皮革等,可以模拟纱线在生产中的磨擦状态,也可以模拟纱线在使用时的磨擦状态。纱线往复运动与磨擦介质磨擦直到磨断为止,由计时器计时,每台仪器同时可以测试10个试样(或20个),等到试样全部磨断仪器停止。通过微处理机可以显示,单头次数、平均数、离散系数等。并可记录打印。采用本机测试纱线耐磨性能与目前国内外现有的仪器相比,它的优点是被试纱线的磨擦距离长50cm,(国内外现有仪器远小于50cm)因此代表性强,精确度高。
1、不是采用单一磨擦介质(砂布或钢针),而是可以方便地采用不同的磨擦介质进行磨擦试验,可以模拟在服用过程中的磨擦状态。也可以模拟在生产过程中的磨擦状态。(例如缝纫线通过针眼、布机经线通过钢筘等)为制订工艺,提高质量,科学研究、提供广阔的空间。
2、利用本仪器的原理,将它“重型化”。则可以测定各种线带、鞋带、缆绳等的耐磨性能。
二、测定毛线、针织绒的起球性能
①更换磨擦介质(例如采用软木辊)②将光电探头的开关调节在起球挡,因纱线较细(光线能射到接收器,仪器能正常运转。③操作步骤与上节耐磨试验相同。经过来回磨擦,纱线渐渐磨毛、起球,当起球达到一定大小时,它通过光电探头组时挡住了光线进入接收器,信号经放大,通知该头的计数器停止计数。当仪器上的10根(20根)试样的计数器全部停止计数时仪器停止来回运转,微处理机能记录每头的次数,平均次数离散系数等,可记录打印。采用本仪器测定毛线、针织绒起球的优点是:1、不用各种规格的针织机,不用织片,节省投资,节省占地,节省人工。2、用纱线直接测试,不用照片标样人工目测,而是直接读数,提高准确度。3、可以方便地更换磨擦介质,同时在测试过程中,试验者可以一目了然地看到起球的过程(而不是目前世界通用的放在滚筒里看不见)这二点对研究起球机理,改进工艺,提高质量,开拓了广阔的空间。
三、测定雪尼尔线脱绒
①更换磨擦介质(例如采用标准6#钢针组)②将光电探头组的开关调节在脱绒挡(因纱线较粗,光线不能射到接收器,仪器正常运转)③操作步骤与耐磨试验相同,试样经过来回磨擦,雪尼尔线渐渐脱绒,当脱绒达到一定程度时,纱线变细,它通过光电控头组时不能挡住光线进入接收器,信号经放大,通知该头的计数器停止计数:
当仪器上的10根(20根)试样的计数器全部停止计数时仪器停止来回运动,微处理机能记录每头的次数、平均数、离散系数等,并可打印。
采用本仪器测定雪尼尔线脱绒的优点是:
1、不用各种规格的针织机,不用人工织片,节省投资,节省占地,节省人工。
2、用10根(20根)纱线直接测试,代表性强,不是间接通过4个小样秤重间接评定,而是直接读数,准确度高。
3、可以方便地更换磨擦介质,同时在测试过程中,试验者可以一目了然地看到脱绒的过程,(而不是放在马尔代尔机器里看不见)这二点对研究防止脱绒,改进工艺,提高质量,开拓了广阔空间。
综上所述
1、纱线耐磨试验:由于本仪器的试样被磨擦距离达到50cm,显著超过于其它同类产品,代表性强。由于本仪器采用可方便更换的磨擦介质座,可直观地模拟纱线在加工过程或在使用过程中的磨擦状态,因此它将为制订新标准,改进工艺,科学研究,开拓新的途径。
利用本仪器的原理,将它“重型化”则可测定线带、鞋带、绳缆等“重型纱线”。它将填补国内外空白。
2、毛线、针织绒起球试验
由于本仪器是国内外唯一直接用来测试纱线起球的仪器,具有精确、直观、方便等优点,它将为制订新标准,改进工艺科学研究开拓新的途径。
3、雪尼尔线脱绒试验
由于本仪器是国内外唯一直接用来测试雪尼尔线脱绒的仪器具有精确、直观、方便等优点,它将为制订新标准,改进工艺,科学研究,开拓新的途径。
4、本机集纱线(线带、绳缆)耐磨、毛线、针织绒起球,雪尼尔线脱绒,三大测试功能于一体,而且性能优于现有的仪器,因此具有较大的使用价值与经济意义。
Claims (3)
1.一种测纱线绳带耐磨,针织绒线起球,雪尼尔线脱绒的仪器,其特征在于:由驱动马达、同步带、卷绕滚筒、样线、导辊、可换摩擦介质座、光电探头组、专用夹头、引线、导辊、感应探头、重锤、滑槽、计数器组成,通过以下联接进行工作;驱动马达通过同步带传动卷绕滚筒,样线的一端固定在卷绕滚筒上,另一端通过导辊→可换摩擦介质座→光电探头组之后用专用夹头夹持,专用夹头的另一端与引线固结,引线的另一端通过导辊→感应探头后与重锤固结,驱动马达启动后拉动装在滑槽内的重锤,重锤上下运动感应感应探头使马达产生倒顺转,同时带动样线往复运动,样线运动时,通过固定在机台上的磨擦介质进行摩擦。
2.根据权利要求1所述的一种测定纱线绳带耐磨,针织绒线起球,雪尼尔线脱绒的仪器,具有可更换磨擦介质座,采用织物、软木辊、橡胶辊、砂辊、毛毡、钢针、皮革作为磨擦介质,用来模拟生产过程或服用过程。
3.根据权利要求1所述的一种测定纱线绳带耐磨,针织绒线起球,雪尼尔线脱绒的仪器,该仪器有光电探头组,光电探头组由以下部分组成:多级恒定光源、接收器、转换开关和一对精确定位导纱器,其中,转换开关分别有耐磨、起球、脱绒三档;一对精确定位导纱器保证纱线在探头中央通过,精确定位导纱器的孔径要根据纱支作变换;测定纱线耐磨时,将光电探头组的开关调节在耐磨挡;测定针织绒线起球时,将开关调节在起球挡;测定雪尼尔线脱绒时将开关调节在脱绒挡。