CN101116988A - Method for preparation of - Google Patents

Method for preparation of Download PDF

Info

Publication number
CN101116988A
CN101116988A CNA2007100727571A CN200710072757A CN101116988A CN 101116988 A CN101116988 A CN 101116988A CN A2007100727571 A CNA2007100727571 A CN A2007100727571A CN 200710072757 A CN200710072757 A CN 200710072757A CN 101116988 A CN101116988 A CN 101116988A
Authority
CN
China
Prior art keywords
color changing
temperature sensing
sensing color
floor
temperature
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2007100727571A
Other languages
Chinese (zh)
Inventor
孙英瀚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA2007100727571A priority Critical patent/CN101116988A/en
Publication of CN101116988A publication Critical patent/CN101116988A/en
Pending legal-status Critical Current

Abstract

The manufacturing method of temperature sensing color changing floor boards relates to a manufacturing technique of floor boards. Floor boards are produced by the following procedures: the plain floor board is dyed with painting liquid containing temperature sensing color changing color masterbatch according to the conventional process, thus the temperature sensing color changing color masterbatch is obtained. The floor boards made by the method has the visual effect when the temperature changes which is demonstrated by color changing, when the floor boards sense the change of temperature; while when the temperature restores to the normal temperature and the color also returns. Therefore, the original artistic vein is maintained, which enhances the beauty; meanwhile, the color varies with the temperature grade. The method can be applied to floor boards made of solid wood, compound floe boards of solid wood (three or two layers), intensified compound floor boards, which not only preserves the original technique but also provides the floor boards with practicability. The floor boards can be applied under the condition that the original technique is preserved.

Description

The manufacture method of temperature sensing color changing floor
Technical field
The present invention relates to a kind of manufacturing process of floor, be specifically related to a kind of manufacturing process of temperature sensing color changing floor.
Background technology
The floor color of production and processing both at home and abroad is generally natural wood color, or to the timber processing of dyeing, can not change substantially during use after the oil paint coating color is qualitative, and the heating floor variations in temperature does not have the vision sense organ.
Summary of the invention
The purpose of this invention is to provide a kind of manufacture method that can make the floor when temperature changes, have the temperature sensing color changing floor of visual perception's effect.
Technical solution of the present invention can have following five kinds:
One, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing water-based look mother and aqueous priming paint, temperature sensing color changing water-based look mother's volumetric concentration≤39%, the ratio that addition accounts for the mixed liquor cumulative volume is no more than 75%, coating weight≤12g/m 2, baking temperature is below 200 ℃.
Two, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing oiliness look mother and banana oil, temperature sensing color changing oiliness look mother's volumetric concentration≤30%, the ratio that addition accounts for the mixed liquor cumulative volume is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
Three, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, the staining procedure specific requirement is as follows: application liquid is the temperature sensing color changing water paint, volumetric concentration≤30% of temperature hydronasty coating, the ratio that temperature sensing color changing water-based look mother accounts for the water paint cumulative volume is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
Four, it makes the floor according to following steps: ground laminin plate → dyeing → finish paint, the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing oil paint and natural oil or UV oil, volumetric concentration≤30% of temperature sense oil paint, the ratio that temperature sensing color changing oiliness look mother's content accounts for the mixed liquor cumulative volume is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
Five, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing oiliness look mother and oil primer, temperature sensing color changing oiliness look mother's volumetric concentration≤30%, the ratio that addition accounts for mixed liquor is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
Technique effect of the present invention is: this method is administered to and can makes the floor that visual perception's effect is arranged when variations in temperature on the various floors, variable color behind the temperature-sensitive of floor, and temperature returns to color restoration behind the normal temperature, has kept the attractive in appearance of the former texture of timber, has improved aesthetic measure; And can make color color when thermograde changes in floor have the depth to change.This method can be applied to solid wooden floor board, solid wooden compound floor (three layers, multilayer), reinforced composite floorboard, has not only kept original technology but also can use simultaneously, can use under the immovable situation of original technology.
Description of drawings
Fig. 1 is the embodiment of the present invention process chart.
The specific embodiment
The specific embodiment one: it is example that present embodiment adds the aqueous priming paint application with temperature sensing color changing water-based look mother, and it makes temperature sensing color changing floor according to following steps:
Aqueous priming paint manufacturer both domestic and external is a lot, and character is the same substantially, and be divided into two kinds substantially: a kind of is water-based priming paint, and a kind of is the UV aqueous priming paint.According to must color the depth temperature sensing color changing water-based look mother of all kinds that doses varying number.Common versicolor temperature sensing color changing water-based look mother's volumetric concentration≤39%.Temperature sensing color changing water-based look female shared volume ratio can not surpass 75% in the mixed liquor of temperature sensing color changing water-based look mother and water-based priming paint, and the shared volume ratio of variable color water-based look mother can not surpass 30% in the mixed liquor of temperature sensing color changing water-based look mother and UV aqueous priming paint.Influence PASS as surpassing than regular meeting.Coating process can adopt methods such as roller coat, manual obliterating, brushing, spraying or showering.Coating weight≤12g/m 2
As shown in the figure, carry out drying after the dyeing of floor, temperature sensing color changing water-based look mother must use below 200 ℃.According to conventional method priming paint, finish paint application are carried out in the floor then, can make temperature sensing color changing floor.This method is applicable to solid wooden floor board, solid wooden compound floor (three layers, multilayer), reinforced composite floorboard.
The specific embodiment two: it is example that present embodiment adds the banana oil application with temperature sensing color changing oiliness look mother, and it makes temperature sensing color changing floor according to following steps:
Banana oil is that common chemical products are domestic all a sale.Versicolor temperature sensing color changing oiliness look parent volume concentrations≤30%, dose the temperature sensing color changing oiliness look mother of varying number according to shade, the mixed liquor of temperature sensing color changing oiliness look mother and banana oil wherein temperature sensing color changing oiliness look female shared volume ratio can not surpass 30%, influence PASS as surpassing than regular meeting.Can roller coat, method application such as manual obliterating or brushing, spraying, showering.Coating weight≤10g/m 2
As shown in the figure, carry out drying after the dyeing of floor, temperature sensing color changing oiliness look mother must use below 200 ℃.According to conventional method priming paint, finish paint application are carried out in the floor then, can make temperature sensing color changing floor.This method is applicable to solid wooden floor board, solid wooden compound floor (three layers, multilayer), reinforced composite floorboard.
The specific embodiment three: it is example that present embodiment adds the clear water application with temperature sensing color changing water-based look mother, and it makes temperature sensing color changing floor according to following steps:
According to the also directly application of purchasing shades of colour temperature sensing color changing look female ratio difference.Common versicolor temperature sensing color changing water-based look mother's volumetric concentration≤39%.Also can add clear water and mix the back application, variable color water-based look female shared volume ratio can not surpass 30% in the mixed liquor.Coating process can roller coat, manual obliterating or brushing, spraying, showering etc.Coating weight≤12g/m 2
As shown in the figure, carry out drying after the dyeing of floor, temperature sensing color changing water-based look mother must use below 200 ℃.According to conventional method priming paint, finish paint application are carried out in the floor then, can make temperature sensing color changing floor.This method is applicable to solid wooden floor board, solid wooden compound floor (three layers, multilayer), reinforced composite floorboard.
The specific embodiment four: it is example that present embodiment adds the application of natural oil, UV oil with the temperature sensing color changing oil paint, and it makes temperature sensing color changing floor according to following steps:
Natural oil, UV oil manufacturer both domestic and external is a lot, can buy.Owing to natural oil, UV oil are so that oily matter must be dosed temperature sensing color changing oiliness look mother.The mixed liquor of temperature sensing color changing oiliness look mother and natural oil wherein temperature sensing color changing oiliness look female shared volume ratio can not surpass 30%, influences oily adhesive force as surpassing than regular meeting.Can roller coat, method application such as manual obliterating or brushing, spraying, showering.Coating weight≤10g/m 2
As shown in the figure, carry out drying after the dyeing of floor, temperature sensing color changing look mother must use below 200 ℃.According to conventional method the finish paint application is carried out on the floor then, can be made temperature sensing color changing floor.This method is applicable to solid wooden floor board, solid wooden compound floor (three layers, multilayer), reinforced composite floorboard.
The specific embodiment five: it is example that present embodiment adds the oiliness primer painting with temperature sensing color changing oiliness look mother, and it makes temperature sensing color changing floor according to following steps:
Oil primer manufacturer both domestic and external is a lot, can buy.Because oil primer is so that oily matter must be dosed temperature sensing color changing oiliness look mother.The mixed liquor of temperature sensing color changing oiliness look mother and oil primer wherein temperature sensing color changing oiliness look female shared volume ratio can not surpass 30%, influences oily adhesive force as surpassing than regular meeting.Can roller coat, method application such as manual obliterating or brushing, spraying, showering.Coating weight≤10/gm 2
As shown in the figure, drying is carried out in floor dyeing place, and temperature sensing color changing oiliness look mother must use below 200 ℃.According to conventional method priming paint, finish paint application are carried out in the floor then, can make temperature sensing color changing floor.This method is applicable to solid wooden floor board, solid wooden compound floor (three layers, multilayer), reinforced composite floorboard.
Temperature sensing color changing oiliness look mother also can add in UV finish paint, UV face oil, natural face oil, the PU lacquer, can roller coat, method applications such as manual obliterating or brushing, spraying, showering.Coating weight≤10g/m 2, but influencing drying and adhesive force, color is also unstable.
The specific embodiment six: the water-based temperature allochroic paint (pink colour) that present embodiment adopts is produced for New Prismatic Enterprise Co., Ltd., its volumetric concentration is 15%, directly manual embrocating on ground laminin plate, dry then (air dry) temperature is carried out application by the normal process of floor UV roller coat then less than 200 ℃.
The specific embodiment seven: the oiliness temperature allochroic paint (pink colour) that present embodiment adopts is produced for New Prismatic Enterprise Co., Ltd., its volumetric concentration is 20%, sneaking into UV oil central roll is coated on the ground laminin plate, use UV lamp drying then, finish paint sander light weight sand (No. 320, sand paper) is coated with face oil at last, with UV lamp drying.

Claims (7)

1. the manufacture method of temperature sensing color changing floor, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, it is characterized in that the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing water-based look mother and aqueous priming paint, temperature sensing color changing water-based look mother's volumetric concentration≤39%, the ratio that its addition accounts for the mixed liquor cumulative volume is no more than 75%, coating weight≤12g/m 2, baking temperature is below 200 ℃.
2. the manufacture method of temperature sensing color changing floor according to claim 1 is characterized in that described aqueous priming paint is water-based priming paint or UV aqueous priming paint.
3. the manufacture method of temperature sensing color changing floor according to claim 2, when it is characterized in that described aqueous priming paint is the UV aqueous priming paint, the ratio that temperature sensing color changing water-based look mother accounts for the mixed liquor cumulative volume is no more than 30%.
4. the manufacture method of temperature sensing color changing floor, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, it is characterized in that the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing oiliness look mother and banana oil, temperature sensing color changing oiliness look mother's volumetric concentration≤30%, the ratio that its addition accounts for the mixed liquor cumulative volume is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
5. the manufacture method of temperature sensing color changing floor, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, it is characterized in that the staining procedure specific requirement is as follows: application liquid is the temperature sensing color changing water paint, volumetric concentration≤30% of temperature hydronasty coating, the ratio that temperature sensing color changing water-based look mother accounts for the water paint cumulative volume is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
6. the manufacture method of temperature sensing color changing floor, it makes the floor according to following steps: ground laminin plate → dyeing → finish paint, it is characterized in that the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing oil paint and natural oil or UV oil, volumetric concentration≤30% of temperature sense oil paint, the ratio that temperature sensing color changing oiliness look mother's content accounts for the mixed liquor cumulative volume is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
7. the manufacture method of temperature sensing color changing floor, it makes the floor according to following steps: ground laminin plate → dyeing → priming paint → finish paint, it is characterized in that the staining procedure specific requirement is as follows: application liquid is the mixed liquor of temperature sensing color changing oiliness look mother and oil primer, temperature sensing color changing oiliness look mother's volumetric concentration≤30%, the ratio that its addition accounts for mixed liquor is no more than 30%, coating weight≤10g/m 2, baking temperature is below 200 ℃.
CNA2007100727571A 2007-09-03 2007-09-03 Method for preparation of Pending CN101116988A (en)