CN101089061A - 一种内墙环保涂料及其制备方法 - Google Patents

一种内墙环保涂料及其制备方法 Download PDF

Info

Publication number
CN101089061A
CN101089061A CN 200610044821 CN200610044821A CN101089061A CN 101089061 A CN101089061 A CN 101089061A CN 200610044821 CN200610044821 CN 200610044821 CN 200610044821 A CN200610044821 A CN 200610044821A CN 101089061 A CN101089061 A CN 101089061A
Authority
CN
China
Prior art keywords
polyvinyl alcohol
wall paint
stir
reactor
add
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200610044821
Other languages
English (en)
Inventor
高伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200610044821 priority Critical patent/CN101089061A/zh
Publication of CN101089061A publication Critical patent/CN101089061A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种内墙环保涂料及其制备方法,由下述重量配比的原料制成:聚乙烯醇5~15、水60~90、0.4%(重量)四硼酸钠溶液1~2、钠基膨润土2~6、灰钙粉18~30、白水泥10~20、白木炭8~12、SKANEM.8防霉剂0.1~0.4、NATROSOL 250增稠剂0.1~0.20。本发明还公开了上述内墙环保涂料的制备方法。本发明涂料在潮湿时,会吸收潮气,在干燥的时候,它会把吸收了的潮湿发放出来,从而出色地发挥调节湿度的作用。此外,还能消除房间里的气味和有害物质等。

Description

一种内墙环保涂料及其制备方法
所属技术领域
本发明涉及一种用于建筑行业的化工涂料,尤其还涉及一种内墙环保涂料及其制备方法
背景技术
木炭是木材或木质原料经过不完全燃烧,或者在隔绝空气的条件下热解,所残留的深褐色或黑色多孔固体燃料。是保持木材原来构造和孔内残留焦油的不纯的无定形碳。中国商代的青铜器和春秋战国时代铁器的冶炼都用木炭,利用其吸湿性来观测气候变化等。现在除仍作生活燃料外,还用作金属冶炼、食品和轻工业的燃料,电炉冶炼的还原剂,金属精制时用作覆盖剂保护金属不被氧化。在化学工业上常作二硫化碳和活性炭等的原料。此外还在研磨、绘画、化妆、医药、火药、渗碳、粉末合金等各方面应用。木炭上有着纵横无数的洞孔,这些洞孔具有吸附各种各样的物质以及发放出吸附着的物质的功能,所以,人们用它作除湿剂。在潮湿时,木炭会吸收潮气,在干燥的时候,它会把吸收了的潮湿发放出来,从而出色地发挥调节湿度的作用。此外,木炭还能消除房间里的气味和有害物质等。现在市面上用于室内墙体、天花板装饰的仿瓷涂料、刚化涂料、干粉涂料等,大都是没有功能或功能过于单调,本发明增加了一种内墙环保涂料,扩大了涂料应用范围。
发明内容
本发明的目的在于提供一种内墙环保涂料在潮湿时,会吸收潮气,在干燥的时候,它会把吸收了的潮湿发放出来,从而出色地发挥调节湿度的作用。此外,还能消除房间里的气味和有害物质等。本发明的另一目的在于提供该内墙环保涂料的制备方法。
本发明提供的内墙环保涂料,由下述重量配比的原料制成:聚乙烯醇5~15、水60~90、0.4%(重量)四硼酸钠溶液1~2、钠基膨润土2~6、灰钙粉18~30、白水泥10~20、白木炭8~12、SKANEM.8防霉剂0.1~0.4、NATROSOL250增稠剂0.1~0.20。将上述原料制备本发明内墙环保墙衬涂料的方法,依次包括以下步骤:
(1)将聚乙烯醇加入反应锅内,然后加入水,搅拌,加热水温至90~100℃,使反应锅内聚乙烯醇完全溶解;
(2)将四硼酸钠溶液在不断搅拌下以细流方式慢慢滴入反应锅内与聚乙烯醇发生交联反应;
(3)滴完四硼酸钠溶液后,保持70~80℃温度反应30~50分钟,使聚乙烯醇凝胶化;
(4)反应完后,用冷却水冷却反应锅,使其温度降至20~30℃,过滤,得无色胶水;
(5)将上述无色胶水加入搅拌机内,再加入钠基膨润土、灰钙粉、白木炭及白水泥,开机搅拌,50~70分钟后,加入SKANEM.8防霉剂,继续搅拌5~15分钟后,加入NATROSOL250增稠剂,然后再搅拌;
(6)搅拌均匀后,放入研磨机研磨,即制得本发明内墙环保涂料。现有的各种仿瓷、刚化涂料,大都是没有功能或功能过于单调,
本发明增加了一种内墙环保涂料,扩大了涂料应用范围。
下面结合具体实施方式对本发明作进一步的说明。
实施例
将60kg聚乙烯醇加入反应锅内,然后加入7kg水,搅拌,加热水温至90℃,使反应锅内聚乙烯醇完全溶解;将1kg重量百分浓度为0.4%的四硼酸钠溶液在不断搅拌下以细流方式慢慢滴入反应锅内与聚乙烯醇发生交联反应;滴完四硼酸钠溶液后,保持75℃温度反应40分钟,使聚乙烯醇凝胶化;反应完后,用冷却水冷却反应锅,使其温度降至22℃,过滤,得无色胶水;将上述无色胶水加入搅拌机内,再加入6kg钠基膨润土、22kg灰钙粉、10kg白木炭、及11kg白水泥,开机搅拌,50分钟后,加入0.1kgSKANEM一8防霉剂,继续搅拌8分钟后,加入0.1kgNATROSOL250增稠剂,然后再搅拌,搅拌均匀后,放入研磨机研磨,即制得本发明防水墙衬涂料。

Claims (2)

1、一种内墙环保涂料,其特征在于由下述重量配比的原料制成:聚乙烯醇5~15、水60~90、0.4%(重量)四硼酸钠溶液1~2、钠基膨润土2~6、灰钙粉18~30、白水泥10~20、白木炭8~12、SKANEM.8防霉剂0.1~0.4、NATROSOL250增稠剂0.1~0.20。
2、权利要求1所述的内墙环保墙衬涂料的制备方法,依次包括以下步骤:
(1)将聚乙烯醇加入反应锅内,然后加入水,搅拌,加热水温至90~100℃,使反应锅内聚乙烯醇完全溶解:
(2)将四硼酸钠溶液在不断搅拌下以细流方式慢慢滴入反应锅内与聚乙烯醇发生交联反应;
(3)滴完四硼酸钠溶液后,保持75~80℃温度反应40~60分钟,使聚乙烯醇凝胶化;
(4)反应完后,用冷却水冷却反应锅,使其温度降至20~30℃,过滤,得无色胶水;
(5)将上述无色胶水加入搅拌机内,再加入钠基膨润土、灰钙粉、白木炭及白水泥,开机搅拌,50~70分钟后,加入SKANEM-8防霉剂,继续搅拌5~15分钟后,加入NATROSOL250增稠剂,然后再搅拌;
(6)搅拌均匀后,放入研磨机研磨,即制得本发明内墙环保涂料。
CN 200610044821 2006-06-16 2006-06-16 一种内墙环保涂料及其制备方法 Pending CN101089061A (zh)