- Prior art keywords
- printing
- color printing
- weight
- ink
- paint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Links
Landscapes
- Inks, Pencil-Leads, Or Crayons (AREA)
Abstract
一种彩印底料涂料及其制造方法,所述彩印底料涂料按重量比5∶10∶3包括白墨、撤淡剂和连结料;所述连结料按重量比1∶1包括调墨油和稀释剂;所述彩印底料涂料的制造方法为,先将调墨油和稀释剂按重量比1∶1使用搅拌机进行搅拌至均质制成连结料,再将白墨、撤淡剂和所述连结料按重量比5∶10∶3使用搅拌机进行搅拌至均质。在对白版纸进行彩印之前,在白版纸的印刷面上先附着一层该涂料打底,待干后再在其上进行常规印刷,可弥补纸质不足引起的印迹不清晰以及出现小斑点等现象,同时又起到隔离油墨和纸张中不良物质的作用,达到印刷色泽、色相的统一和稳定,从而保证彩面印刷质量的稳定性和效果。
Description
技术领域
本发明涉及一种印刷用彩印底层涂料及其制造方法。
技术背景
在白版纸上进行彩色印刷时,由于纸张往往由于加填的原因造成厚薄不均,从而在印刷过程中会因此造成印迹不清晰以及出现小斑点等现象,无法保障彩面印刷的效果。
发明内容
本发明的目的在于提供一种在对白版纸上进行彩色印刷前,对白版纸进行预处理的涂料,以弥补纸质的不足,消除因纸质不足而在印刷过程中产生的印迹不清晰以及出现小斑点等现象,达到印刷色泽、色相的统一和稳定,从而保证彩面印刷质量的稳定性和效果。
为达到上述目的,本发明采用一种彩印底层涂料,所述彩印底层涂料按重量比5∶10∶3包括以下组分,白墨、撤淡剂和连结料;所述连结料按重量比1∶1包括调墨油和稀释剂。
为达到上述目的,本发明一种彩印底层涂料的制造方法是先将调墨油和稀释剂按重量比1∶1使用搅拌机进行搅拌至均质制成连结料,再将白墨、撤淡剂和所述连结料按重量比5∶10∶3使用搅拌机进行搅拌至均质。
在对白版纸进行彩印之前,先在白版纸的印刷面上附着一层上述涂料打底,待干后再在其上进行常规印刷。
具体实施方式
以下通过具体实施例对本发明作进一步的描述。
本发明彩印底层涂料实施例如下:由上海牡丹油墨厂生产的05-40型白墨、杭华油墨厂生产的B0-600型撤淡剂、调墨油和稀释剂组成,其中,调墨油和稀释剂按重量比1∶1组成连结料,白墨、撤淡剂和连结料按重量比5∶10∶3组成本发明的彩印底层涂料。
本发明彩印底层涂料的制造方法实施例如下:使用杭华油墨厂生产的调墨油和稀释剂,按重量比1∶1使用搅拌机进行搅拌至均质后制成连结料待用;再使用上海牡丹油墨厂生产的05-40型白墨和杭华油墨厂生产的B0-600型撤淡剂同上述预制的连结料按重量比5∶10∶3使用搅拌机进行搅拌至均质,制成本发明的印刷用彩印底层涂料。
在对白版纸进行彩印之前,在白版纸的印刷面上先附着一层上述涂料打底,待干后再在其上进行常规印刷。通过本发明彩印底层涂料的使用,一方面弥补了纸质不足引起的印迹不清晰以及出现小斑点等现象,同时又起到隔离油墨和纸张中不良物质的作用,达到印刷色泽、色相的统一和稳定,从而保证彩面印刷质量的稳定性和效果。
Claims (2)
1.一种白版纸彩印底层涂料,其特征在于,所述彩印底层涂料按重量比5∶10∶3由以下组分组成:白墨、撤淡剂和连结料;所述连结料按重量比1∶1由调墨油和稀释剂组成。
2.一种如权利要求1所述的白版纸彩印底层涂料的制造方法,其特征在于,先将调墨油和稀释剂按重量比1∶1使用搅拌机进行搅拌至均质制成连结料,再将白墨、撤淡剂和所述连结料按重量比5∶10∶3使用搅拌机进行搅拌至均质。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CNB2004100537003A CN100458012C (zh) | 2004-08-13 | 2004-08-13 | 一种彩印底层涂料及其制造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CNB2004100537003A CN100458012C (zh) | 2004-08-13 | 2004-08-13 | 一种彩印底层涂料及其制造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
CN1734017A CN1734017A (zh) | 2006-02-15 |
CN100458012C true CN100458012C (zh) | 2009-02-04 |
Family
ID=36076608
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CNB2004100537003A Active CN100458012C (zh) | 2004-08-13 | 2004-08-13 | 一种彩印底层涂料及其制造方法 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN100458012C (zh) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103273751B (zh) * | 2013-05-08 | 2016-08-10 | 温太平 | 一种纸张印刷覆膜方法 |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2002211630A (ja) * | 2001-01-15 | 2002-07-31 | Toppan Printing Co Ltd | イージーピール蓋材 |
-
2004
- 2004-08-13 CN CNB2004100537003A patent/CN100458012C/zh active Active
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2002211630A (ja) * | 2001-01-15 | 2002-07-31 | Toppan Printing Co Ltd | イージーピール蓋材 |
Non-Patent Citations (6)
Title |
---|
如何做好金银卡纸的底色印刷. 孟宪志.广东印刷,第5期. 2003 |
如何做好金银卡纸的底色印刷. 孟宪志.广东印刷,第5期. 2003 * |
油墨辅助剂的性能及使用方法. 汤杰.印刷杂志,第10期. 2003 |
油墨辅助剂的性能及使用方法. 汤杰.印刷杂志,第10期. 2003 * |
浅谈油墨助剂的类型及其应用. 郭建中.广东印刷,第1期. 2002 |
浅谈油墨助剂的类型及其应用. 郭建中.广东印刷,第1期. 2002 * |
Also Published As
Publication number | Publication date |
---|---|
CN1734017A (zh) | 2006-02-15 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
WO2009087789A1 (ja) | 水変色性布帛シート | |
CN109094991B (zh) | 一种揭显全息彩印防伪膜及其制作方法 | |
CN103725089B (zh) | 一种用于碰击布面料的伞用水性油墨及其涂覆方法 | |
JP2001030611A (ja) | 水性グラビアインキを用いて行うグラビア印刷方法及びこの印刷方法の実施に用いられる版胴並びにこの印刷方法により印刷された印刷物 | |
CN107325640A (zh) | 一种水性喷墨油墨在接装纸数码印刷工艺中的应用 | |
CN103725088B (zh) | 一种用于色丁类面料的伞用水性油墨及其涂覆方法 | |
CN103897492A (zh) | 一种皮革用喷墨墨水以及打印在皮革上形成图案的方法 | |
CN100469850C (zh) | 一种能产生彩色花纹的水性涂料及其制备方法 | |
CN107828278A (zh) | 一种包装盒印刷用环保型水性油墨及其生产工艺 | |
CN100458012C (zh) | 一种彩印底层涂料及其制造方法 | |
US7799380B2 (en) | Ink for silk-screen printing and corresponding printing technique | |
CN106394035A (zh) | 一种服装吊牌的印刷工艺 | |
CN105385234A (zh) | 一种可用于光盘打印的墨水及其制备方法 | |
CN106170519A (zh) | 黑色油墨组合物 | |
CN104149533A (zh) | 一种木雕上色工艺 | |
CN108864970B (zh) | 一种揭显全息彩印防伪胶带及其制作方法 | |
CN107488376A (zh) | 一种用于香烟包印刷领域的高光耐磨uv油墨 | |
CN106739586B (zh) | 一种低迁移量的环保印刷方法 | |
CN101096833A (zh) | 对白版纸进行预处理的涂料制造方法 | |
CN104893396B (zh) | 金色薄膜的调色方法 | |
CN103660760A (zh) | 一种喷绘画的制作方法 | |
CN103525201B (zh) | 一种艺术水性感光涂料 | |
CN111996835A (zh) | 一种用于纸类卡牌的涂料及其使用方法 | |
CN100336973C (zh) | 一种用于涂布彩色纱管面纸的涂料及其制备方法 | |
CN103121370A (zh) | 瓷器上绘制彩色图案的方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
C14 | Grant of patent or utility model | ||
GR01 | Patent grant |