CA2309233A1 - Methode de fabrication de ciment a partir de fines de steriles ou de roches renfermant des silicates ou des composes siliceux - Google Patents
Methode de fabrication de ciment a partir de fines de steriles ou de roches renfermant des silicates ou des composes siliceux Download PDFInfo
- Publication number
- CA2309233A1 CA2309233A1 CA002309233A CA2309233A CA2309233A1 CA 2309233 A1 CA2309233 A1 CA 2309233A1 CA 002309233 A CA002309233 A CA 002309233A CA 2309233 A CA2309233 A CA 2309233A CA 2309233 A1 CA2309233 A1 CA 2309233A1
- Authority
- CA
- Canada
- Prior art keywords
- tailings
- pozzolan
- cement
- portland cement
- ground
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02P40/00—Technologies relating to the processing of minerals
- Y02P40/10—Production of cement, e.g. improving or optimising the production methods; Cement grinding
Landscapes
- Processing Of Solid Wastes (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US13740399P | 1999-06-01 | 1999-06-01 | |
US60/137403 | 1999-06-01 |
Publications (1)
Publication Number | Publication Date |
---|---|
CA2309233A1 true CA2309233A1 (fr) | 2000-12-01 |
Family
ID=22477273
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CA002309233A Abandoned CA2309233A1 (fr) | 1999-06-01 | 2000-05-24 | Methode de fabrication de ciment a partir de fines de steriles ou de roches renfermant des silicates ou des composes siliceux |
Country Status (1)
Country | Link |
---|---|
CA (1) | CA2309233A1 (fr) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN108298886A (zh) * | 2018-05-03 | 2018-07-20 | 南京御森建筑科技发展有限公司 | 一种旱强混凝土及其制备方法 |
CN114671644A (zh) * | 2022-03-24 | 2022-06-28 | 江苏奥莱特新材料股份有限公司 | 一种高早强低回弹的高性能喷射混凝土及其制备方法 |
-
2000
- 2000-05-24 CA CA002309233A patent/CA2309233A1/fr not_active Abandoned
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN108298886A (zh) * | 2018-05-03 | 2018-07-20 | 南京御森建筑科技发展有限公司 | 一种旱强混凝土及其制备方法 |
CN114671644A (zh) * | 2022-03-24 | 2022-06-28 | 江苏奥莱特新材料股份有限公司 | 一种高早强低回弹的高性能喷射混凝土及其制备方法 |
CN114671644B (zh) * | 2022-03-24 | 2023-06-23 | 江苏奥莱特新材料股份有限公司 | 一种高早强低回弹的高性能喷射混凝土及其制备方法 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Qaidi et al. | Recycling of mine tailings for the geopolymers production: A systematic review | |
Tokyay | Cement and concrete mineral admixtures | |
Murari et al. | Use of waste copper slag, a sustainable material | |
CA2352926C (fr) | Liant pour residus miniers | |
De Brito et al. | Recycled aggregate in concrete: use of industrial, construction and demolition waste | |
US5749962A (en) | Method of making cement from base metal smelter slag | |
Malatse et al. | The viability of using the Witwatersrand gold mine tailings for brickmaking | |
CN106660873A (zh) | 包含粉煤灰和改良剂的胶凝材料用火山灰质组合物 | |
KR20060102756A (ko) | 폐광미를 활용한 콘크리트 혼화재 및 그 제조 방법 | |
WO2018156380A1 (fr) | Compositions durcissables comprenant des cendres volantes dépolluées (remediated fly ash - rfa) et procédés de cimentation dans des formations souterraines | |
Maruthupandian et al. | Recycling mine tailings as precursors for cementitious binders–Methods, challenges and future outlook | |
Singh et al. | Utilization of Linz–Donawitz slag from steel industry for waste minimization | |
Mymrin et al. | Potential application of acid jarosite wastes as the main component of construction materials | |
CN113045226A (zh) | 一种低成本的固废基胶凝材料 | |
Fronek | Feasibility of expanding the use of steel slag as a concrete pavement aggregate | |
CA2856155A1 (fr) | Procede et compositions pour liants pouzzolaniques derives de laitiers non ferreux de fonderie | |
US6033467A (en) | Method of making cement or mine backfill from base metal smelter slag | |
KR101638079B1 (ko) | 심층혼합공법용 고화재 | |
Ban et al. | Advances in the use of recycled non-ferrous slag as a resource for non-ferrous metal mine site remediation | |
US20020033120A1 (en) | Method of making cement from tailings or rock fines containing silicate or siliceous compounds | |
Hammond | Mining and quarrying wastes: a critical review | |
CA2309233A1 (fr) | Methode de fabrication de ciment a partir de fines de steriles ou de roches renfermant des silicates ou des composes siliceux | |
US5968258A (en) | Method of making cement from base metal smelter slag | |
Akhmetova et al. | STATE-OF-THE-ART AND ANALYSIS OF CHARACTERISTICS, PROPERTIES, SIGNIFICANCE, AND APPLICATION PROSPECTS OF METALLURGICAL SLAGS. | |
Anawar et al. | Recovery of value-added materials from iron ore waste and steel processing slags with zero-waste approach and life cycle assessment |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
FZDE | Dead |