CA1036979A CA199,442A CA199442A CA1036979A CA 1036979 A CA1036979 A CA 1036979A CA 199442 A CA199442 A CA 199442A CA 1036979 A CA1036979 A CA 1036979A
Authority
CA
Canada
Prior art keywords
anode
titanium
coated
coated titanium
height
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
CA199,442A
Other languages
French (fr)
Other versions
CA199442S (en
Inventor
Konrad Koziol
Baptist Zenk
Karl-Heinz Sieberer
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SIEBERER KARL HEINZ
Original Assignee
SIEBERER KARL HEINZ
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SIEBERER KARL HEINZ filed Critical SIEBERER KARL HEINZ
Application granted granted Critical
Publication of CA1036979A publication Critical patent/CA1036979A/en
Expired legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C25ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
    • C25BELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR
    • C25B11/00Electrodes; Manufacture thereof not otherwise provided for
    • C25B11/02Electrodes; Manufacture thereof not otherwise provided for characterised by shape or form

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Electrochemistry (AREA)
  • Materials Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Electrodes For Compound Or Non-Metal Manufacture (AREA)
  • Electrolytic Production Of Metals (AREA)
  • Physical Vapour Deposition (AREA)

Abstract

Abstract of the Disclosure The anode is particularly designed for use at anodic densities DA
greater than 10 kA/m2, and comprises substantially horizontally extending coated anode segments having a clear spacing of at least 1.5 mm from each other and upwardly extending lateral surfaces. Each segment has an active coated part higher than 5 mm and not exceeding 20 mm, measured from the hori-zontal undersurface of the anode. The actual active surface of the parts, up to heights of 5 mm, 7.5 mm, 10 mm and 15 mm, respectively, exceeds at least 2.5, 3.33, 4 and 4.7 times, respectively, the projected anode area which latter is the total area bounded by the periphery of the anode. At least half the actual active surface extends upwardly relative to the horizontal base area of the anode.

Description

~3697~

The present invention relates to El coated titanium anode for electrically highly loaded amalgam cells. The large amounts of chlorine gas developing on the anode in the high current loaded chlorine alkali electrol-ysis cells must be conducted away from the electrode range as quickly as possible, for energy conservation reasons.
As is well known, dwelling of the chlorine gas bubbles in the electrode range causes a substantial increase in cell voltage and a decrease of the current efficiency. This phenomenon, which has become known by the collective term "gas bubble effect", has, in past years, led to design changes in the graphite anode. For example, the horizontally arranged anode plates were provided with numerous slots and gas outlet openings, which did provide the desired effect up to current densities of DA = 10 kA/m2. However, the ceramic-like graphite anode of conventional design is beginning to be in the way of a further increase of the current density. Thus, at very high current densities, DA, greater than 10 kA/m2, it is difficult to remove the developed chlorine gas rapidly from the underside of the horizontal anode plate that itself is generously slotted and provided with very many gas outlet openings.
The result is higher overvoltage on the graphite and greater voltage losses in the electrolyte enriched with chlorine gas bubbles. MoreoverJ with the number of slots and gas outlet openings, the inner resistanceJ the graphite loss and the sensitivity to transport of the anodes increase. It has been attempted to avoid this restriction by utilizing the graphite anode described in the German application No. 2,029,640 published October 12, 1972. This is an anode which is provided with a number of thin, vertical graphite plates, and in which the graphite plates are disposed transversely to the flow direction of the mercury density, corresponding in length to the cathode widthJ are slotted in comb-like manner on their undersideJ and are provided on their upper side with sunk contact sleeves of anodic resistant material and, with the inter-connection of trough-configured bellows of corrosion resistant elastomerJ are connected with current distributor rails in such a ~369"~9 manner that, with the exception of the graphite plate provided with sleeves, all current conducting parts remain excluded from the inside of the cell.
Mercury cells equipped with this anode design and operated at current den-sities DA of 10 to 13 kA/m2, really did let the voltage coefficient (k-value) drop below 0.11 VkA ~ which appeared impossible for amalgam cells provided with electrographite anodes. Thus, the anodes in German published application No. 2,029,640 took a step toward the objective of making possible the inten-sified chlorine alkali electrolysis in modern amalgam cells with low voltage.
However, an exact analysis of the wearing out picture of this anode simul-taneously led to the conclusion that voltage coefficients k smaller than 0.10 will remain unattainable in spite of further improvements of the graphite anode. The ridges (teeth) having a width of 12.5 mm and obtained by slotting the graphite plate having a thickness of 40 mm have become so pointed, as a result of the NaCl-electrolysis conducted at current densities at between 10 and 13 kA/m2, that the anode part facing the Hg-cathode soon has only prismatic teeth of a width of the sharply processed profile of about 10 mm and a profile height of about 15 mm. The anode ranges still further removed .
from the cathode also showed unusually strong traces of electrochemical attack. This wearing down appearance at a simultaneously favourable k-value ---is exceedingly surprising, considering it is similar to the wearing down appearance, which in many cases is briefly termed "Haifischzahne" (shark teeth), of horizontal graphite anode plates in NaCl-electrolytes contaminated by bringing in alkali, which always provides for high cell voltage in spite of strong pressing of the anodes. It must be concluded therefrom that the anode construction for high loaded amalgam cells, according to German published application No. 2,029,640, on account of its better chlorine gas bubble dis-charge, will distribute the electric current far better than the conventional stamp-configured, horizontally arranged anode plate provided with slots and gas discharge openings. It is still very effective in electrolysis, conducted at high current densities, down to great surface ranges, that is to surface
- 2 -~36979 ranges that are 15 mm and more away from the ridge tips.
~his important finding has to be taken fully into account in the development of an improved coated titanium anode for electrically highly loaded amalgam cells, particularly for utilization with anodic current den-sities DA greater than lO kA/m2.
Metal anodes for amalgam cells are well known in which the active part consists of coated titanium in the form of perforated sheet r metal mesh. These anodes lack the height and large surface necessary for good current distribution.
Moreover, metal anodes are known in which the active coating is applied onto a horizontally disposed parallel row of round titanium rods, which are held together by uncoated transverse ribs. Such anodes of thin, ; round titanium rods also lack the height necessary for good current distribution. Although anodes produced from thick round rods do have the necessary height, the upper half of the activated rod surface, however, is in a position unfavourable relative to the mercury cathode, as it is in the shadow of the lower rod half. Current distribution to the activated surface of the upper rod half is further made difficult or, respectively, is entirely prevented by the extensive enrichment of the electrolyte, with chlorine gas bubbles in the narrow range of the gap between the round rods. Technical electrolysis tests with metal anodes, the active part of which consisted of completely coated titanium rods of a diameter greater than 5 mm, have shown, in the current density range, DA, of lO to 15 kA/m2, that the anode process takes place almost exclusively on the rod surface facing the mercury cathode, and that by increasing the spacing between the round rods current distribution could not be substantially improved.
Furthermore, metal anodes are known in which the active part consists of thin titanium strips, which are disposed either perpendicularly or at any other angle relative to the chathode and which are provided on at least a part of their surfaces, with a coating consisting of a metal of the platinum
- 3 -1~?3~ 9 metal group. For example, Belgium Patent No. 645,039 discloses titanium anodes coated with platinum metal, the active part of which is present in the form of ribs or plates, respectively> which are disposed perpendicularly to the mercury cathode and parallel to the main direction of flow of the electric current and in the vicinity of which gas outlets or, respectively, gaps are disposed. The platinum metal coating is applied preferably or exclusively on the perpendicular area of the ribs or, respectively, plates wherein at least half of the coated area and preferably at least 80% of the total coated area is arranged perpendicularly to the amalgam cathode, so that this coated area is about 4 times the area of the horizontal part of the coating. This measure is to counteract the danger of damage of the sensitive platinum metal coating by the amalgam in case of contact with the cathode.
It also is to make possible operation of the anode at a spacing increased by about 1 mm from the cathode with the same cell voltage than with an anode produced from wire mesh, thus also reducing the danger of short circuiting.
The important drawbacks of the suggested anodes include the small height of the active coating, amounting to only 2.54 mm the unfavourable relation be-tween the actual active surface of the anode and the projected surface of the anode at small distances with respect to the counterelectrode being at a maximum 2.03:1 and resulting from that construction of the anode, a complete absence of any active surface within the middle range and long distance range with respect to the amalgam cathode and, finally, the use of a collecting bar - of titanium which has, because of its deep cross-slotting, only very small electrical conductivity, and the small actual active surface at small dis-tances with respect to the counterelectrode.
It is therefore a feature of the invention to provide an improved titanium anode for electrically highly loaded amalgam cells, particularly for use at anodîc currect densities DA greater than 10 kA/m2 having a large height of the active coated part of the anode.
One embodiment of the invention provides such an anode having an .

~Q3~979 extraordinarily large active coated area in the small distance range, the middle distance range and the long distance range, with respect to the counterelectrode.
Another embodiment provides such an anode having predominantly up-wardly extending active coated lateral surfaces with respect to the amalgam cathode.
A further embodiment provides such an anode having sufficiently large free space between the active surfaces that chlorine gas bubbles are not prevented from passing therethrough.
; 10 Another embodiment of the invention provides such an anode having short current paths, low internal resistance and uniform current distribution.
Another embodiment of the invention provides such an anode having a long life of its basic construction and its coating even if under high current overload.
A further embodiment provides such an anode possessing good emer-gency operation conditions and re-use even after possible short circuits.
Yet another embodiment of the invention provides such an anode possessing the ability of coating and re-coating without any problems, as well as the advantages of simplicity and inexpensiveness.
These features are attained in a particularly advantageous manner by a coated titanium anode for electrically highly loaded amalgam cells, par-ticularly for use at anodic currect densities DA greater than lOkA/m2, said anode comprising substantially horizontally extending completely coated anode segments having a clear lateral spacing of at least 1.5 mm and upwardly ex-tending lateral surfaces, and each having an active coated upwardly extending part extending to a height of more than 5 mm and not exceeding 20 mm, measured from the horizontal undersurface of the anode, wherein the actual active sur-face of said upwardly extending parts, up to heights thereof of 5 mm, 7.5 mm, 10 mm, and 15 mm, respectively, exceeds at least 2.5, 3.33, 4 and 4.5 times, respectively, the projected horizontal anode area which is the total area ~ _ 5 _ ~)3~979 bounded by the periphery of the anode, and wherein at least half the actual active surface extends upwardly relative to the horizontal base area of the _ Sa -,~,....

~3~9~i9 anode.
For an understanding of the principles of the invention, reference is made to the following description of typical embodiments thereof as illustrated in the accompanying drawings. In the drawings, Figures 1, 2, 3 and 4 are perspective views of anodes embodying the invention, Figure 5 is a sectional view disassembled taken on the line V-V of Figure 4, and Figures 6 and 7 are graphical illustrations of the relation of the cell voltage to the anodic current density of anodes embodying the invention.
Figure 1 shows an anode, the active part 1 of which consists of completely coated, horizontally extending, vertically oriented, titanium bands or strips of 1 mm thickness and 20 mm height. The spacing between the coated titanium bands, strips or segments amounts to 2 mm. The bands are connected with one another on their upper edges by several transversely extending welding seams 2. Current distribution is effected by a welded-on transverse bar 3 of uncoated titanium, and which is provided with a titanium protective tube 4 of the current feed line.
This design results in the following ratios of the actual active surface to the anode area to be projected: height 5 mm, 3.67:1; height 7.5 mm, 5.33:1; height 10 mm, 7:1; height 15 mm, 10.33:1; and height 20 mm, 14:1.
More than 95% of the actual active surface is in this case, disposed per-pendicular to the base area of the anode.
Figure 2 shows an anode with a projected area 400 x 400 mm, the active part 1 of which consists of slotted and completely coated titanium sheet having a thickness of 12 mm. The width of the slots and segments amounts to 2.5 mm. The uncut center range of the active part, which simul-taneously serves for current distribution, has a width of 60 mm and is pro- ;
vided on its underside with grooves having a width of 2.5 mm and depth of 2.5 mm. In the center thereof, the screw contact for the copper-current feed line is disposed, only the titanium protective sleeve 4 of which is visible.

~(~369~79 In this case, the ratio of the actual active surface to the pro-jected anode area amounts to 5.13:1 and about 80% of the active actual surface is disposed perpendicular to the base area of the anode.
Figure 3 shows an anode, the active part 1 of which, similarly to that of Figure 1, is provided with perpendicularly oriented completely coated titanium bands or segments, having a clear spacing of 2 mm. The titanium bands, having a height of 7.5 mm and a thickness of 2 mm, are welded to retaining ribs, which, in part, are connected, through titanium rods 9 of larger cross-section, with the contact sleeve in the center of the anode.
This star-configured current distribution ensures a uniform load on the anode ; surface. From this anode a ratio of the actual active surface to the pro-jected anode surface of 4.75:1 results.
The titanium anode shown in Figure 4, and provided with completely coated titanium bands or segments of a height of 20 mm and a thickness of 1.5 mm disposed at a clear spacing of 2.5 mm, includes a central titanium sleeve 7 having a current distribution track 8 of titanium-plated copper to which the bands are welded. For safety reasons, the height ratio of the current distribution track to the height of the titanium band amounts to ` 0.75:1.
Figure 5 shows a section through the anode according to Figure 4 in which the type of contacting of the copper current lead rod 5, through a closed titanium threaded member 6 having a flange and titanium protective tube 4, with the central titanium sleeve 7 of the anode, is shown in detail.
The parts 6 and 7 have a thread with a large angle of thread or pitch, as according to German Patent No. 1,237,482. Due to this design, the active part of the anode can be re-used by merely being unscrewed from the current feed means relative to the cathode. This is of particular advantage in case damage due to short circuits occurs on the anode underside, as well as also after a longer period of operation of the anode, in the course of which the active coating, in the zones disposed closer to the cathode, have been more ~()3~'7~

extensively or entirely used up. The active coating of the upper zones which, in such cases is made less use of or, respectively, due to remoteness from the cathode is less used up, can still carry on the anode process for a long period of time after turning over the anode whereas, with conventional anodes, recoating will then have to be effected immediately.
Due to its features, the anode according ~o the invention for the first time provides for the possibility of a very extensive utilization of the current distribution and reduction of the anodic current density, thus result-ing in a corresponding decrease of cell voltage.
Figure 6 shows a diagram of the cell voltage depending upon the anodic current density DA for three types of titanium anodes activated with the same substances of the type Me(I) ca 0.5 Pt30~, wherein the curve designated I was obtained with titanium anodes of bands of 1 mm thickness and 10 mm height with a 3 mm wide gap between the bands and a coating height of 2 mm, and the curves designated II and III were obtained with titanium anodes with bands of 1 mm thickness and 15 mm height with the same gap and a coating height of 5 or, respectively, 10 mm. In each case, the spacing between the anode and the mercury cathode amounted to 3 mm.
In the diagram shown in Figure 7, there is disclosed the fact that the dependence of the cell voltage upon the anodic current density can be substantially improved by increasing the actual active surface in the range close to and remote from the cathode. Curve II corresponds to anodes whose active part consists of entirely coated titanium bands or segments having a 2 mm thickness and a 12 mm height with a 2 mm wide gap between the bands, whereas curve I concerns the same anode type as in Figure 6 with a coating of 10 mm height.
The reduction in current density by increasing the actual active - surface further effects a corresponding increase in the life of the active anode coating. The large height of the electrochemically active part of the anode and the relatively small anode base area, and the primarily perpendic-rg~ ~ 8 -1~36~79 ular arrangement of the active actual surface assure good emergency operation properties, also in the case of possible short circuits, and a rapid discharge of the chlorine gas bubbles. Finally, the large height permits accommodation of the current distribution within the active anode part, and thus the anode can, in a very simple manner, be used on both sides. The anode according to the invention thus meets entirely all requirements of secure and economical high current load operations.

;

g _

Claims (7)

THE EMBODIMENTS OF THE INVENTION IN WHICH AN EXCLUSIVE
PROPERTY OR PRIVILEGE IS CLAIMED ARE DEFINED AS FOLLOWS:
1. A coated titanium anode for electrically highly loaded amalgam cells, particularly for use at anodic current densities DA greater than 10 kA/m2, said anode comprising substantially horizontally extending completely coated anode segments having a clear lateral spacing of at least 1.5 mm and upwardly extending lateral surfaces, and each having an active coated upwardly extending part extending to a height of more than 5 mm and not exceeding 20 mm, measured from the horizontal undersurface of the anode, wherein the actual active surface of said upwardly extending parts, up to heights thereof of 5 mm, 7.5 mm, 10 mm and 15 mm, respectively, exceeds at least 2.5, 3.33, 4 and 4.5 times, respectively, the projected horizontal anode area which is the total area bounded by the periphery of the anode, and wherein at least half the actual active surface extends upwardly relative to the horizontal base area of the anode.
2. A coated titanium anode according to claim 1, in which the current distribution takes place within the active coated part, and which is provided with contact means for a current feed, the contact means having a structure such that both horizontal surfaces of the anode may be used by inverting the anode.
3. A coated titanium anode according to claim 1, in which said anode segments comprise coated, vertically oriented titanium bands having a thick-ness of 1 mm and a height of 20 mm, the clear space between said coated titanium bands being 2 mm.
4. A coated titanium anode according to claim 3, wherein said bands are connected with one another on their upper edges by several transversely extending welding seams, and wherein the current distribution is effected by a welded-on transverse bar of uncoated titanium.
5. A coated titanium anode according to claim 4, wherein said trans-verse bar of uncoated titanium is provided with a titanium protective tube of a current feed line.
6. A coated titanium anode according to claim 1, consisting of a slotted and coated titanium sheet.
7. A coated titanium anode according to claim 6, wherein said titanium sheet has a thickness of 12 mm, and the width of said slots is 2.5 mm.
CA199,442A 1973-05-10 1974-05-09 Coated titanium anode for amalgam heavy duty cells Expired CA1036979A (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
DE2323497A DE2323497B2 (en) 1973-05-10 1973-05-10 Coated titanium anode for amalgam high-load cells

Publications (1)

Publication Number Publication Date
CA1036979A true CA1036979A (en) 1978-08-22

Family

ID=5880451

Family Applications (1)

Application Number Title Priority Date Filing Date
CA199,442A Expired CA1036979A (en) 1973-05-10 1974-05-09 Coated titanium anode for amalgam heavy duty cells

Country Status (17)

Country Link
JP (1) JPS5730910B2 (en)
AT (1) AT331821B (en)
BE (1) BE814829A (en)
CA (1) CA1036979A (en)
CH (1) CH571579A5 (en)
DE (1) DE2323497B2 (en)
ES (1) ES426103A1 (en)
FI (1) FI59269C (en)
FR (1) FR2228542B1 (en)
GB (1) GB1454603A (en)
IE (1) IE39255B1 (en)
IT (1) IT1012275B (en)
NL (1) NL166728C (en)
NO (1) NO140504C (en)
SU (1) SU833176A3 (en)
YU (1) YU42135B (en)
ZA (1) ZA743002B (en)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE2949495C2 (en) * 1979-12-08 1983-05-11 Heraeus-Elektroden Gmbh, 6450 Hanau Electrode for electrolytic cells
DE3008116A1 (en) * 1980-03-03 1981-09-17 Conradty GmbH & Co Metallelektroden KG, 8505 Röthenbach GAS-DEVELOPING METAL ELECTRODE FOR ELECTROCHEMICAL PROCESSES

Also Published As

Publication number Publication date
ES426103A1 (en) 1976-07-01
NL7406364A (en) 1974-11-12
BE814829A (en) 1974-09-02
JPS5041800A (en) 1975-04-16
FR2228542B1 (en) 1977-06-24
IE39255B1 (en) 1978-08-30
IT1012275B (en) 1977-03-10
GB1454603A (en) 1976-11-03
SU833176A3 (en) 1981-05-23
JPS5730910B2 (en) 1982-07-01
NO140504C (en) 1979-09-12
FR2228542A1 (en) 1974-12-06
CH571579A5 (en) 1976-01-15
NL166728C (en) 1984-03-16
NO140504B (en) 1979-06-05
ZA743002B (en) 1975-05-28
ATA373974A (en) 1975-12-15
FI59269B (en) 1981-03-31
IE39255L (en) 1974-11-10
YU124774A (en) 1982-05-31
NL166728B (en) 1981-04-15
FI59269C (en) 1981-07-10
DE2323497A1 (en) 1974-11-28
DE2323497B2 (en) 1978-10-12
NO741667L (en) 1974-11-12
YU42135B (en) 1988-06-30
AT331821B (en) 1976-08-25

Similar Documents

Publication Publication Date Title
US4022679A (en) Coated titanium anode for amalgam heavy duty cells
DD243516A5 (en) MONOPOLAR AND BIPOLAR CHLORIN CELLS AND ELECTRODE STRUCTURES FOR THESE
CA1123378A (en) Electrode assembly
EP0189535A1 (en) Electrolysis apparatus
IE41068L (en) Electrochemical cell
US3839179A (en) Electrolysis cell
CA1156183A (en) Electrolytic cell
AU612126B2 (en) Permanent anode for high current density galvanizing processes
DE2059868A1 (en) Electrode plate for electrolysis
PL128858B1 (en) Electrolyser electrode
DE2645121C3 (en) Electrolytic cell
CA1036979A (en) Coated titanium anode for amalgam heavy duty cells
US3853738A (en) Dimensionally stable anode construction
DE1592012A1 (en) Improvements to electrolytic diaphragm cells
US4364811A (en) Electrodes for electrolytic cells
US3271289A (en) Mercury cathode electrolytic cell having an anode with high corrosionresistance and high electrical and heat conductivity
US5225061A (en) Bipolar electrode module
US4379742A (en) Gas-generating metal electrode for electrochemical processes
US4401544A (en) Composite electrodes for diaphragmless electrolytic cells for the production of chlorates and hypochlorites II
DE3013043A1 (en) Rectangular bipolar fuel cell battery - with porous carbon or graphite paper forming gas spaces
CA1143334A (en) Composite electrodes for diaphragmless electrolytic cells for the production of chlorates and hypochlorites i
DE2148337A1 (en) BIPOLAR MULTIPLE ELECTROLYSIS CELL WITH DIAPHRAGMA
JPS57101692A (en) Horizontal electroplating method by insoluble electrode
GB2180556A (en) Apertured electrode for electrolysis
DE812546C (en) Electrolytic cell