Prior art keywords
sheets
sheet
thin
rolling
cold
Prior art date
Application number
Other languages
English (en)
French (fr)
Publication of BE341908A publication Critical patent/BE341908A/fr

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B21MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL
    • B21BROLLING OF METAL
    • B21B1/00Metal-rolling methods or mills for making semi-finished products of solid or profiled cross-section; Sequence of operations in milling trains; Layout of rolling-mill plant, e.g. grouping of stands; Succession of passes or of sectional pass alternations
    • B21B1/38Metal-rolling methods or mills for making semi-finished products of solid or profiled cross-section; Sequence of operations in milling trains; Layout of rolling-mill plant, e.g. grouping of stands; Succession of passes or of sectional pass alternations for rolling sheets of limited length, e.g. folded sheets, superimposed sheets, pack rolling

Landscapes

  • Engineering & Computer Science (AREA)
  • Mechanical Engineering (AREA)
  • Soft Magnetic Materials (AREA)
BE341908D BE341908A (enrdf_load_html_response)

Publications (1)

Publication Number Publication Date
BE341908A true BE341908A (enrdf_load_html_response)

Family

ID=18466

Family Applications (1)

Application Number Title Priority Date Filing Date
BE341908D BE341908A (enrdf_load_html_response)

Country Status (1)

Country Link
BE (1) BE341908A (enrdf_load_html_response)

Similar Documents

Publication Publication Date Title
US5222282A (en) Method for reducing thickness of a high-strength low-ductility metal foil on thin strip element
WO2017163115A1 (fr) Procédé de fabrication de tôles d'aciers laminées à froid et soudées, et tôles ainsi produites
JP4759499B2 (ja) 組み立てスラブの圧延におけるせん断とクロップロスを減ずる方法
Xu et al. Effect of annealing and cold rolling on interface microstructure and properties of Ti/Al/Cu clad sheet fabricated by horizontal twin-roll casting
US2645842A (en) Multiple rolling of strip
BE341908A (enrdf_load_html_response)
JP2009501635A (ja) 中断なしの鋼板の製造方法及びプラント
CN114433625B (zh) 一种双层金属复合板波-平铸轧装置及方法
JPH0623406A (ja) 鋼片の連続熱間圧延方法
RU2677397C2 (ru) Способ бесконечной горячей прокатки высококачественной стали
CN103842104B (zh) 热连轧中的薄板坯的接合方法
RU84763U1 (ru) Биметаллическая заготовка
RU2234385C1 (ru) Способ изготовления прокаткой стального слоистого материала
JP2001239313A (ja) 電縫鋼管の製造方法および設備列
JPS6250202B2 (enrdf_load_html_response)
BE385932A (enrdf_load_html_response)
JPH11169946A (ja) 鋼管の製造方法
TH2301007163A (th) แผ่นอะลูมิเนียม 5xxx สำหรับการทำกระป๋อง
JP3323073B2 (ja) 鋼片の連続熱間圧延方法
Lee et al. A NEW ON-LINE BAR JOINING TECHNOLOGY FOR ENDLESS HOT ROLLING
BE341886A (enrdf_load_html_response)
Babu et al. Processing and properties of 3-layer laminated composites based on ultra high carbon steel and mild steel
JPS61159285A (ja) 熱間圧延における鋼片の接合方法
JPH0671307A (ja) 鋼片の連続熱間圧延方法
JPH0569162A (ja) クラツド鋼板の製造方法