AU507706B2 - Strengthening chemically a glass container - Google Patents
Strengthening chemically a glass containerInfo
- Publication number
- AU507706B2 AU507706B2 AU25833/77A AU2583377A AU507706B2 AU 507706 B2 AU507706 B2 AU 507706B2 AU 25833/77 A AU25833/77 A AU 25833/77A AU 2583377 A AU2583377 A AU 2583377A AU 507706 B2 AU507706 B2 AU 507706B2
- Authority
- AU
- Australia
- Prior art keywords
- potassium
- glass
- glass container
- aqueous solution
- mixed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C21/00—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C21/001—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface in liquid phase, e.g. molten salts, solutions
- C03C21/002—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface in liquid phase, e.g. molten salts, solutions to perform ion-exchange between alkali ions
Landscapes
- Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Geochemistry & Mineralogy (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Surface Treatment Of Glass (AREA)
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6456376A JPS52148519A (en) | 1976-06-04 | 1976-06-04 | Chemical tempering process for glass vessel |
| JPJP64563/76 | 1976-06-04 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| AU2583377A AU2583377A (en) | 1978-12-07 |
| AU507706B2 true AU507706B2 (en) | 1980-02-21 |
Family
ID=13261815
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| AU25833/77A Expired AU507706B2 (en) | 1976-06-04 | 1977-06-03 | Strengthening chemically a glass container |
Country Status (6)
| Country | Link |
|---|---|
| JP (1) | JPS52148519A (enExample) |
| AU (1) | AU507706B2 (enExample) |
| BE (1) | BE888585Q (enExample) |
| DE (1) | DE2718977C2 (enExample) |
| FR (1) | FR2353501A1 (enExample) |
| GB (1) | GB1533686A (enExample) |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE4335462A1 (de) * | 1993-10-18 | 1995-04-20 | Dragon Werk Georg Wild Gmbh & | Chemisch gehärteter abriebfester Mahlkörper |
| CN100588634C (zh) * | 2005-11-07 | 2010-02-10 | 比亚迪股份有限公司 | 用于对玻璃进行强化的组合物及强化方法 |
| US11145143B2 (en) | 2017-01-31 | 2021-10-12 | Honda Motor Co., Ltd. | Unmanned work system, management server, and unmanned work machine |
| WO2018142483A1 (ja) | 2017-01-31 | 2018-08-09 | 本田技研工業株式会社 | 無人作業システム、管理サーバー、及び無人作業機 |
| EP3779629B1 (en) | 2018-03-30 | 2022-10-12 | Honda Motor Co., Ltd. | Autonomous running working machine and control system |
| CN116535107B (zh) * | 2023-05-22 | 2024-10-29 | 温州市康尔微晶器皿有限公司 | 一种高Tg点玻璃的高温固相化学钢化方法 |
| CN120923152B (zh) * | 2025-10-15 | 2026-01-27 | 东华大学 | 一种玻璃容器的化学强化方法 |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3498773A (en) * | 1966-02-23 | 1970-03-03 | Owens Illinois Inc | Method of strengthening glass by ion exchange |
| GB1286516A (en) * | 1968-12-10 | 1972-08-23 | Brockway Glass Co Inc | Method of strengthening glass and increasing the scratch resistance of the surface thereof |
| US3751238A (en) * | 1970-02-25 | 1973-08-07 | Corning Glass Works | Method of chemically strengthening a silicate article containing soda |
| DE2239307A1 (de) * | 1972-08-10 | 1974-02-21 | Owens Illinois Inc | Verfahren zur verstaerkung von festen glasgegenstaenden und nach dem verfahren hergestellte gegenstaende |
| JPS5012377A (enExample) * | 1973-06-08 | 1975-02-07 | ||
| JPS50123717A (enExample) * | 1974-02-28 | 1975-09-29 | ||
| JPS51114414A (en) * | 1975-04-02 | 1976-10-08 | Yamamura Glass Co Ltd | Method of chemically strengthening glass articles which have been treated to have hardwearing properties |
-
1976
- 1976-06-04 JP JP6456376A patent/JPS52148519A/ja active Granted
-
1977
- 1977-04-18 GB GB1600677A patent/GB1533686A/en not_active Expired
- 1977-04-28 DE DE19772718977 patent/DE2718977C2/de not_active Expired
- 1977-06-03 FR FR7717152A patent/FR2353501A1/fr active Granted
- 1977-06-03 AU AU25833/77A patent/AU507706B2/en not_active Expired
-
1981
- 1981-04-28 BE BE2/59130A patent/BE888585Q/fr not_active IP Right Cessation
Also Published As
| Publication number | Publication date |
|---|---|
| AU2583377A (en) | 1978-12-07 |
| JPS5529947B2 (enExample) | 1980-08-07 |
| BE888585Q (fr) | 1981-08-17 |
| DE2718977A1 (de) | 1977-12-15 |
| GB1533686A (en) | 1978-11-29 |
| DE2718977C2 (de) | 1984-09-13 |
| FR2353501B1 (enExample) | 1982-06-04 |
| FR2353501A1 (fr) | 1977-12-30 |
| JPS52148519A (en) | 1977-12-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4206253A (en) | Method of strengthening chemically a glass container | |
| US3791809A (en) | Method of strengthening glass articles using powdered salts for ion exchange | |
| US3498773A (en) | Method of strengthening glass by ion exchange | |
| US3607172A (en) | Tripotassium phosphate treatment for strengthening glass | |
| US4164402A (en) | Strengthening of thin-walled, light glass containers | |
| EP2925699B1 (en) | Surface treatment process for glass containers | |
| US3296173A (en) | Lubricous coating for glass containing polyvinyl alcohol, polyolefin emulsion and ammonium chloride | |
| CA1041846A (en) | Surface treatment of glass containers | |
| US3860438A (en) | Flux and method of coating ferrous article | |
| CA1092358A (en) | Method of strengthening glass articles with potassium fluoride-metal acetate | |
| CN105392750A (zh) | 化学强化玻璃和化学强化玻璃的制造方法 | |
| TW202330432A (zh) | 化學強化玻璃之製造方法、化學強化玻璃、覆蓋玻璃及顯示裝置 | |
| AU2583377A (en) | Strengthening chemically a glass container | |
| JP2001026466A (ja) | 抗菌ガラスの製造方法 | |
| US3535070A (en) | Method of inducing stress in glass containers and container made with a stressed zone | |
| JPH11278866A (ja) | ガラス容器の抗菌処理方法 | |
| JPH0323494B2 (enExample) | ||
| US4273832A (en) | Glass article strengthened by ion exchange substitution | |
| US4702760A (en) | Method for strengthening glass articles through electrostatic ionic interchange | |
| US3628983A (en) | Coating method for strengthening vitreous and vitrocrystalline bodies | |
| PL168238B1 (pl) | Sposób obróbki powierzchni wyrobu wykonanego z materialu o strukturze szklistej PL | |
| US3661545A (en) | Method for treating a molten salt with water vapor | |
| KR800001189B1 (ko) | 유리용기의 화학적 강화법 | |
| US4448809A (en) | Method of silver plating stainless steel vacuum bottle surfaces | |
| US3875763A (en) | Method of strengthening glass containers |