ATE337T1 - METHOD OF IMPROVING THE HEAT RADIATION CHARACTERISTICS OF AN X-RAY TUBE ROTARY ANODE. - Google Patents
METHOD OF IMPROVING THE HEAT RADIATION CHARACTERISTICS OF AN X-RAY TUBE ROTARY ANODE.Info
- Publication number
- ATE337T1 ATE337T1 AT80200370T AT80200370T ATE337T1 AT E337 T1 ATE337 T1 AT E337T1 AT 80200370 T AT80200370 T AT 80200370T AT 80200370 T AT80200370 T AT 80200370T AT E337 T1 ATE337 T1 AT E337T1
- Authority
- AT
- Austria
- Prior art keywords
- anode
- ray tube
- heat radiation
- tungsten layer
- except
- Prior art date
Abstract
In an X-ray tube rotary anode having a supporting body (1) of molybdenum alloy, a target (2) of tungsten alloy, and a rough tungsten layer, applied by flame spraying to the whole surface of the anode except the focal path (4), for improving heat radiation, the rough tungsten layer does not adhere well to the tungsten alloy target, and particles of the rough tungsten layer may become detached in use, degrading the performance of the X-ray tube. To alleviate this problem, the whole surface of the anode, except the focal path (4), is blasted with steel grit, steel grit particles embedded in the anode are removed with acid, and the whole surface of the anode, except the target (2), is coated with a rough tungsten layer (3) by plasma spraying.
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| NL7903389A NL7903389A (en) | 1979-05-01 | 1979-05-01 | METHOD FOR IMPROVING THE HEAT-DRAWING PROPERTIES OF A ROTARY TURNAROOD AND SO THAT TURNAROUNDED. |
| EP80200370A EP0018685B1 (en) | 1979-05-01 | 1980-04-23 | Method of improving the heat radiation properties of an x-ray tube rotary anode |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| ATE337T1 true ATE337T1 (en) | 1981-11-15 |
Family
ID=19833074
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| AT80200370T ATE337T1 (en) | 1979-05-01 | 1980-04-23 | METHOD OF IMPROVING THE HEAT RADIATION CHARACTERISTICS OF AN X-RAY TUBE ROTARY ANODE. |
Country Status (6)
| Country | Link |
|---|---|
| US (1) | US4320323A (en) |
| EP (1) | EP0018685B1 (en) |
| JP (1) | JPS55148356A (en) |
| AT (1) | ATE337T1 (en) |
| DE (1) | DE3060045D1 (en) |
| NL (1) | NL7903389A (en) |
Families Citing this family (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| NL8300251A (en) * | 1983-01-25 | 1984-08-16 | Philips Nv | METHOD OF MANUFACTURING A TURNING ANOD FOR ROENTGEN TUBES AND ANODE THAT OBTAINED |
| US4731805A (en) * | 1984-06-08 | 1988-03-15 | Boyarina Maiya F | Rotary anode for an x-ray tube and an x-ray tube having such anode |
| AT381805B (en) * | 1984-07-16 | 1986-12-10 | Plansee Metallwerk | X-RAY TURNING ANODE WITH SURFACE COATING |
| NL8402828A (en) * | 1984-09-14 | 1986-04-01 | Philips Nv | METHOD FOR MANUFACTURING A ROTARY TURNAROUND AND ROTARY TURNAROOD MANUFACTURED BY THE METHOD |
| US4943989A (en) * | 1988-08-02 | 1990-07-24 | General Electric Company | X-ray tube with liquid cooled heat receptor |
| US5008918A (en) * | 1989-11-13 | 1991-04-16 | General Electric Company | Bonding materials and process for anode target in an x-ray tube |
| DE4443074C1 (en) * | 1994-12-03 | 1995-12-14 | Winter & Sohn Ernst | Surface disc with abrasive cladding |
| US5629970A (en) * | 1996-01-11 | 1997-05-13 | General Electric Company | Emissivity enhanced x-ray target |
| US6863930B2 (en) | 2002-09-06 | 2005-03-08 | Delphi Technologies, Inc. | Refractory metal mask and methods for coating an article and forming a sensor |
| DE102005003445B4 (en) * | 2005-01-21 | 2009-06-04 | H.C. Starck Hermsdorf Gmbh | Metal substrate material for the anode plates of rotary anode X-ray tubes, method for producing such a material and method for producing an anode plate using such a material |
| US20090060139A1 (en) * | 2007-08-28 | 2009-03-05 | Subraya Madhusudhana T | Tungsten coated x-ray tube frame and anode assembly |
| US9159523B2 (en) | 2007-08-28 | 2015-10-13 | General Electric Company | Tungsten oxide coated X-ray tube frame and anode assembly |
| CN111415852B (en) * | 2020-05-06 | 2024-02-09 | 上海联影医疗科技股份有限公司 | Anode assembly of X-ray tube, X-ray tube and medical imaging equipment |
| US12183536B2 (en) * | 2021-12-21 | 2024-12-31 | GE Precision Healthcare LLC | X-ray cathode focusing element |
Family Cites Families (11)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US2376219A (en) * | 1944-01-28 | 1945-05-15 | Gen Electric | Fabrication of quartz resonators |
| DE1050457B (en) * | 1956-03-15 | 1959-02-12 | Compagnie Generale De Radiologie, Paris | X-ray tube with preferably rotating the high-temperature-resistant anode |
| FR73772E (en) * | 1958-06-24 | 1960-09-05 | Radiologie Cie Gle | Improvement of X-ray tubes |
| US3188776A (en) * | 1962-08-20 | 1965-06-15 | Wheelabrator Corp | Surface treatment of steel |
| BE635133A (en) * | 1963-07-19 | |||
| US3400010A (en) * | 1964-09-28 | 1968-09-03 | Standard Internat Corp | Method of making a composite metal article |
| US3731128A (en) * | 1972-03-08 | 1973-05-01 | Siemens Ag | X-ray tube with rotary anodes |
| US3753021A (en) * | 1972-04-03 | 1973-08-14 | Machlett Lab Inc | X-ray tube anode target |
| JPS5120763Y2 (en) * | 1972-04-14 | 1976-05-29 | ||
| US4038786A (en) * | 1974-09-27 | 1977-08-02 | Lockheed Aircraft Corporation | Sandblasting with pellets of material capable of sublimation |
| DE7807119U1 (en) | 1978-03-09 | 1978-06-29 | N.V. Philips' Gloeilampenfabrieken, Eindhoven (Niederlande) | Layered X-ray rotating anode with a layer that improves heat radiation |
-
1979
- 1979-05-01 NL NL7903389A patent/NL7903389A/en not_active Application Discontinuation
-
1980
- 1980-03-31 US US06/135,964 patent/US4320323A/en not_active Expired - Lifetime
- 1980-04-23 EP EP80200370A patent/EP0018685B1/en not_active Expired
- 1980-04-23 DE DE8080200370T patent/DE3060045D1/en not_active Expired
- 1980-04-23 AT AT80200370T patent/ATE337T1/en not_active IP Right Cessation
- 1980-04-28 JP JP5704880A patent/JPS55148356A/en active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| NL7903389A (en) | 1980-11-04 |
| JPH0145704B2 (en) | 1989-10-04 |
| DE3060045D1 (en) | 1981-12-24 |
| JPS55148356A (en) | 1980-11-18 |
| US4320323A (en) | 1982-03-16 |
| EP0018685B1 (en) | 1981-10-21 |
| EP0018685A1 (en) | 1980-11-12 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ATE337T1 (en) | METHOD OF IMPROVING THE HEAT RADIATION CHARACTERISTICS OF AN X-RAY TUBE ROTARY ANODE. | |
| BR8202386A (en) | SOLID PARTICLES CONTAINING A METALLIC PEROXIDE PROCESS FOR THE PREPARATION OF PARTICLES AND PROCESS FOR CORRECTION OF SOILS | |
| EP0064101A3 (en) | High rate resist polymerization method and apparatus | |
| JPS6439021A (en) | X-ray mask | |
| SE7705088L (en) | X-RAY ANSURE WITH ALLOY SURFACE AND PROCEDURE FOR MANUFACTURE THEREOF | |
| EP0031940A3 (en) | Molybdenum substrate for high power density tungsten focal track x-ray targets | |
| DE2964640D1 (en) | Method of making a master replicating tool | |
| SE8501521L (en) | PROCEDURE FOR PREPARING A COATING | |
| ATE27930T1 (en) | PROCEDURE FOR ATTACHING A PIECE OF DIAMOND TO METAL. | |
| JPS527879A (en) | Method of forming high hardness film on carbon tool steel or alloy too l steel | |
| JPS5761644A (en) | Cover glass having diamond coating layer and its preparation | |
| DE3878444D1 (en) | METHOD FOR MARKING THE SURFACE OF A ROLLER. | |
| JPS5518575A (en) | Surface treating method | |
| JPS52115684A (en) | X-ray tube | |
| ATE127613T1 (en) | METHOD FOR FINE ADJUSTMENT OF AN ELECTRON BEAM CHARACTERISTICS IN A CATHODE RAY TUBE AFTER ITS PRODUCTION AND ADJUSTED TUBE. | |
| JPS5753847A (en) | Production of video disk stylus | |
| JPS5456906A (en) | Method of tightening surface layer of sintered body | |
| JPS5665926A (en) | Manufacture of cylinder liner | |
| JPS54111296A (en) | X ray generating device | |
| JPS5685828A (en) | Electrostatic wafer holder | |
| JPS5297458A (en) | Surface treating method of heat radiation body for boiling and cooling | |
| JPS5431050A (en) | Corrosion prevention shielded welding method for turbine blade | |
| JPS5689354A (en) | Surface treatment of grid body mold for lead storage battery | |
| Baily et al. | A new technique for radiation shielding in superficial X-ray therapy | |
| JPS51147953A (en) | Method of manufacturing cathode ray tube |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| UEP | Publication of translation of european patent specification | ||
| REN | Ceased due to non-payment of the annual fee |