WO2023218601A1 - 同軸ケーブルの処理方法 - Google Patents

同軸ケーブルの処理方法 Download PDF

Info

Publication number
WO2023218601A1
WO2023218601A1 PCT/JP2022/020059 JP2022020059W WO2023218601A1 WO 2023218601 A1 WO2023218601 A1 WO 2023218601A1 JP 2022020059 W JP2022020059 W JP 2022020059W WO 2023218601 A1 WO2023218601 A1 WO 2023218601A1
Authority
WO
WIPO (PCT)
Prior art keywords
coaxial cable
insulator
shield wire
gap
processing method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/JP2022/020059
Other languages
English (en)
French (fr)
Inventor
拓郎 岸田
央記 大塚
宇野 往道
治生 長
奈緒人 上西
朝是 大城
雄太 宮▲崎▼
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shimadzu Corp
Original Assignee
Shimadzu Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shimadzu Corp filed Critical Shimadzu Corp
Priority to JP2024520178A priority Critical patent/JP7677537B2/ja
Priority to US18/835,064 priority patent/US20250336574A1/en
Priority to CN202280084825.9A priority patent/CN118435317A/zh
Priority to PCT/JP2022/020059 priority patent/WO2023218601A1/ja
Publication of WO2023218601A1 publication Critical patent/WO2023218601A1/ja
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Abstract

飛行時間型質量分析装置(10)に電圧を印加するための同軸ケーブル(60)の処理方法であって、折り返し処理工程S2と、埋設処理工程S3とを含む。折り返し処理工程S2では、中心導体(62)と、中心導体(62)の周囲に設けられた絶縁体(64)と、絶縁体(64)の周囲に設けられたシールド線(66)と、シールド線(66)の周囲に設けられた外部シース(68)とを有する同軸ケーブル(60)に対して、シールド線(66)の先端部を外部シース(68)側に折り返すことにより折り返し部(66a)を形成する。埋設処理工程S3では、折り返し部(66a)と絶縁体(64)との間に形成された隙間(72)に、絶縁性又は半導電性を有する埋設部材(74)を配置する。

Description

同軸ケーブルの処理方法
 本発明は、飛行時間型質量分析装置に電圧を印加するための同軸ケーブルの処理方法に関するものである。
 飛行時間型質量分析装置(TOFMS:Time of Flight Mass Spectrometer)においては、分析対象であるイオンがイオン射出部から射出され、そのイオンが中空状のフライトチューブ内を飛行した後、検出器で検出される。これにより、検出器に到達するまでのイオンの飛行時間が測定され、その飛行時間に基づいてイオンの質量が識別される(例えば、下記特許文献1参照)。
 このような、飛行時間型質量分析装置では、所定のコンポーネントに対し同軸ケーブルを介して電圧が印加される。例えば、上記コンポーネントとしてのリフレクトロン及びフライトチューブ等には、同軸ケーブルを介して高電圧が印加される。
特開2017-59385号公報
 飛行時間型質量分析装置において測定されるイオンの飛行時間は、上記コンポーネントに印加される電圧の影響を受けるため、当該電圧の安定性は測定精度を維持する上で重要である。そのため、飛行時間型質量分析装置に用いられる同軸ケーブルとしては、ノイズ対策のためにシールド線が設けられた高電圧用同軸ケーブルを用いることが好ましい。この種の同軸ケーブルは、中心導体と、中心導体の周囲に設けられた絶縁体と、絶縁体の周囲に設けられたシールド線と、シールド線の周囲に設けられた外部シースとを有する。
 高電圧用同軸ケーブルをコンポーネントに対して電気的に接続する際には、まず、外部シースの先端部が除去されることにより、シールド線が露出される。そして、必要な沿面距離を確保するようにシールド線が絶縁体から剥離される。シールド線は、沿面距離に対応する長さ分だけ先端側から剥離され、外部シース側に折り返される。そして、折り返されたシールド線の外側から、金属製のクランプを介して同軸ケーブルを固定することにより、当該クランプを介してシールド線をグランド(アース)に接続することができる。
 上記のようにシールド線を外部シース側に折り返した場合、シールド線の折り返し部において、絶縁体とシールド線との間に隙間が生じる場合がある。本願発明者らは、鋭意検討の結果、シールド線の折り返し部と絶縁体との間に隙間が生じた状態で同軸ケーブルに電圧が印加されると、その隙間において電界が乱れ、局所的な電界集中が起きることにより、微小放電が生じることを見出すに至った。シールド線の折り返し部と絶縁体との間に隙間を有する同軸ケーブルを介して所定のコンポーネントに電圧が印加されると、その電圧には、微小放電の発生に伴うノイズが含まれる可能性がある。この場合、同軸ケーブルを介して電圧が印加されるコンポーネントにおいては、ノイズに起因する悪影響が生じる可能性がある。
 たとえば、リフレクトロン及びフライトチューブ等のコンポーネントについては、印加される電圧がイオンの飛行時間に影響するため、これらのコンポーネントに対して、シールド線の折り返し部と絶縁体との間に隙間を有する同軸ケーブルを介して電圧が印加される場合、測定結果に悪影響が生じる可能性がある。
 本発明は、上記実情に鑑みてなされたものであり、同軸ケーブルにおけるシールド線の折り返し部と絶縁体との間の隙間に起因する微小放電の発生を低減することができる同軸ケーブルの処理方法を提供することを目的とする。
 本発明の態様は、飛行時間型質量分析装置に電圧を印加するための同軸ケーブルの処理方法であって、折り返し処理工程と、埋設処理工程とを含む。前記折り返し処理工程では、中心導体と、前記中心導体の周囲に設けられた絶縁体と、前記絶縁体の周囲に設けられたシールド線と、前記シールド線の周囲に設けられた外部シースとを有する前記同軸ケーブルに対して、前記シールド線の先端部を前記外部シース側に折り返すことにより折り返し部を形成する。前記埋設処理工程では、前記折り返し部と前記絶縁体との間に形成された隙間に、絶縁性又は半導電性を有する埋設部材を配置する。
 本発明によれば、同軸ケーブルにおけるシールド線の折り返し部と絶縁体との間の隙間に起因する微小放電の発生を低減することができる。
本実施形態に係る飛行時間型質量分析装置の構成の一例を示す概略図である。 本実施形態に係る同軸ケーブルの一例を示す概略断面図である。 本実施形態に係る同軸ケーブルの処理方法の一例を示すフロー図である。 本実施形態に係る同軸ケーブルの処理方法を説明するための図である。 本実施形態に係る同軸ケーブルの処理方法を説明するための図である。 本実施形態に係る同軸ケーブルの処理方法を説明するための図である。 本実施形態に係る埋設処理工程による効果を説明するためのグラフである。
1.飛行時間型質量分析装置の全体構成
 図1は、本実施形態に係る飛行時間型質量分析装置(TOFMS:Time of Flight Mass Spectrometer)10の構成の一例を示す概略図である。飛行時間型質量分析装置10は、筐体12を備えており、イオン化室14、第1中間室16、第2中間室18、第3中間室20及び分析室22等が筐体12の内部に形成されている。イオン化室14内は、略大気圧となっている。第1中間室16、第2中間室18、第3中間室20及び分析室22は、それぞれ真空ポンプ(図示は省略)の駆動により真空状態(負圧状態)とされる。また、イオン化室14、第1中間室16、第2中間室18、第3中間室20及び分析室22は、互いに連通しており、この順序に従って段階的に真空度が高くなるように構成されている。
 イオン化室14には、例えばESI(Electro Spray Ionization)スプレーからなるスプレー24が設けられている。液体クロマトグラフ装置(図示は省略)から供給される試料中の各成分を含む試料液は、スプレー24により、電荷が付与されながらイオン化室14内に噴霧される。これにより、試料中の各成分由来のイオンが生成される。ただし、飛行時間型質量分析装置10で用いられるイオン化法は、ESIに限らず、例えばAPCI(Atmospheric Pressure Chemical Ionization)又はPESI(Probe Electro Spray Ionization)などの他のイオン化法が用いられてもよい。
 第1中間室16は、小径の管からなる加熱キャピラリ26を介して、イオン化室14に連通している。また、第2中間室18は、小孔からなるスキマー28を介して、第1中間室16に連通している。第1中間室16及び第2中間室18には、それぞれイオンを収束させつつ後段へ送るためのイオンガイド30、32が設けられている。
 第3中間室20には、例えば四重極マスフィルタ34及びコリジョンセル36などが設けられている。コリジョンセル36の内部には、アルゴン又は窒素などのCID(Collision Induced Dissociation)ガスが連続的又は間欠的に供給される。コリジョンセル36内には、多重極イオンガイド38が設けられている。
 第2中間室18から第3中間室20に流入するイオンは、四重極マスフィルタ34により質量電荷比に応じて分離され、特定の質量電荷比を有するイオンのみが四重極マスフィルタ34を通過する。四重極マスフィルタ34を通過したイオンは、プリカーサイオンとしてコリジョンセル36内に導入され、CIDガスと接触して開裂されることにより、プロダクトイオンが生成される。生成されたプロダクトイオンは、多重極イオンガイド38により一時的に保持され、所定のタイミングでコリジョンセル36から放出される。
 第3中間室20及び分析室22には、これらの室内を跨るようにトランスファー電極部40が設けられている。トランスファー電極部40は、第3中間室20に設けられた1つ又は複数の第1電極40aと、分析室22に設けられた1つ又は複数の第2電極40bとを含む。第1電極40a及び第2電極40bは、それぞれ環状に形成され、同軸上に並べて配置されている。コリジョンセル36から放出されたイオン(プロダクトイオン)は、トランスファー電極部40において第1電極40a及び第2電極40bの内側を通過することにより収束される。
 分析室22には、第2電極40bの他、直交加速部42、加速電極部44、リフレクトロン46、検出器48及びフライトチューブ50等が設けられている。フライトチューブ50は、例えば両端部が開放された中空状の部材であり、その内部にリフレクトロン46が配置されている。
 直交加速部42には、トランスファー電極部40から出射するイオンが入射する。直交加速部42は、互いに間隔を隔てて対向する1対の電極42a、42bを備えている。1対の電極42a、42bは、トランスファー電極部40からのイオンの入射方向に対して平行に延びており、これらの電極間には直交加速領域52が形成されている。
 一方の電極42bは、複数の開口を有するグリッド電極により構成されている。直交加速領域52に入射するイオンは、そのイオンの入射方向に対して直交方向に加速され、一方の電極42bの開口を通過して、加速電極部44へと導かれる。本実施形態において、直交加速部42は、分析対象となるイオンを射出するイオン射出部を構成している。直交加速部42から射出されるイオンは、加速電極部44によりさらに加速され、フライトチューブ50内に導入される。
 フライトチューブ50内に設けられたリフレクトロン46は、1つ又は複数の第1電極46aと、1つ又は複数の第2電極46bとを含む。第1電極46a及び第2電極46bは、それぞれイオンが通過する貫通穴を有し、フライトチューブ50の軸線に沿って同軸上に並べて配置されている。第1電極46a及び第2電極46bには、それぞれ異なる電圧が印加される。
 フライトチューブ50内に導入されたイオンは、そのフライトチューブ50内に形成された飛行空間内に導かれ、その飛行空間内を飛行した後に検出器48に入射する。具体的には、フライトチューブ50内に導入されたイオンは、第1電極46aの内側に形成された第1領域(第1ステージ)54で減速された後、第2電極46bの内側に形成された第2領域(第2ステージ)56で反射されることにより、U字状に折り返されて検出器48に入射する。
 イオンが直交加速部42から射出された時点から、検出器48に入射するまでの飛行時間は、イオンの質量電荷比に依存する。したがって、直交加速部42から射出される各イオンの飛行時間に基づいて、各イオンの質量電荷比を算出し、マススペクトルを作成することができる。
2.同軸ケーブル
 飛行時間型質量分析装置10では、所定のコンポーネントに対し同軸ケーブルを介して電圧が印加される。たとえば、印加される電圧がイオンの飛行時間に影響する、すなわち、印加される電圧が測定結果に影響するコンポーネントには、同軸ケーブルを介して電圧が印加される。
 印加される電圧がイオンの飛行時間に影響するコンポーネントとしては、リフレクトロン46及びフライトチューブ50等が挙げられる。なお、飛行時間型質量分析装置10の各種コンポーネントに電圧を印加するための電源については、図示を省略する。
 図2は、本実施形態に係る同軸ケーブル60の一例を示す概略断面図である。なお、図2では、同軸ケーブル60の一部を示す。同軸ケーブル60は、中心導体62、絶縁体64、シールド線66及び外部シース68を備える。絶縁体64は、中心導体62の周囲に設けられる。シールド線66は、絶縁体64の周囲に設けられる。外部シース68は、シールド線66の周囲に設けられる。
 中心導体62は、直線状に延びる1本の金属線により構成されている。絶縁体64は、筒状に形成されたポリエチレンなどの絶縁性の部材であり、内部を中心導体62が貫通している。シールド線66は、複数本の金属線を含み、これらの金属線がメッシュ状に絶縁体64を覆うように配置される。外部シース68は、筒状に形成された絶縁性の部材であり、シールド線66を覆って保護する機能を有している。
 なお、図2に示す同軸ケーブル60については、外部シース68の外径が3~7mm、具体的には5mm程度とされる。また、中心導体62の外径は0.7~1.5mm、具体的には1mm程度とされる。ただし、中心導体62は、複数本の金属線により構成されていてもよい。また、シールド線66は、中心導体62を介して印加される電圧にノイズが生じることを抑制できるような構成であれば、上記のような構成に限られるものではない。
3.同軸ケーブルに対する処理
 図3は、本実施形態に係る同軸ケーブル60の処理方法の一例を示すフロー図である。本実施形態では、飛行時間型質量分析装置10において、同軸ケーブル60を所定のコンポーネントに接続する際、露出処理工程(ステップS1)、折り返し処理工程(ステップS2)、埋設処理工程(ステップS3)及びカバー処理工程(ステップS4)がこの順に沿って実施される。以下、これらの工程について、図4、図5及び図6を参照して説明する。
 図4は、本実施形態に係る同軸ケーブル60の処理方法を説明するための図である。また、図4は、同軸ケーブル60の端部を示す概略断面図である。さらに、図4は、露出処理工程及び折り返し処理工程が実施された後の同軸ケーブル60を示す。
 露出処理工程は、外部シース68の一部(先端部)を除去することで、同軸ケーブル60のシールド線66を露出させる工程である。折り返し処理工程は、シールド線66の先端部、具体的には、シールド線66の露出している部分を外部シース68側に折り返すことにより折り返し部66aを形成する工程である。なお、折り返し部66aとは、シールド線66が折り返された部分、すなわち、折り返されたシールド線66における最も同軸ケーブル60の先端側に位置する部分を意味している。
 図4に示す例では、シールド線66が、導電性を有する金属製のクランプ70を介してグランド(アース)に接続される。具体的には、必要な沿面距離に対応する長さ分だけシールド線66が先端側から剥離され、外部シース68の表面に沿うように折り返される。そして、折り返されたシールド線66の外側から、クランプ70を介して同軸ケーブル60を固定することにより、クランプ70を介してシールド線66をグランドに接続することができる。なお、シールド線66が端子等を介してグランドに接続されるのであれば、折り返し処理工程は、シールド線66を180度折り返す工程に限らず、90度以上、180度未満の角度で折り返す工程であってもよい。
 図5は、本実施形態に係る同軸ケーブル60の処理方法を説明するための図である。また、図5は、同軸ケーブル60の折り返し部66aの周辺を拡大した概略断面図である。同軸ケーブル60に対して折り返し処理工程が実施されると、図5に示すように、折り返し部66a及び絶縁体64の間に隙間72が形成される。なお、絶縁体の厚みd1は、隙間の厚みd2よりも大きい。
 絶縁体64の誘電率ε1は、空気の誘電率ε2よりも高いため、絶縁体64における電界E1よりも、隙間72における電界E2が大きくなる。したがって、飛行時間型質量分析装置10において、同軸ケーブル60の中心導体62を介して所定のコンポーネントに電圧が印加された場合、隙間72において電界が乱れ、局所的な電界集中が起きることにより、その隙間72で微小放電が生じる可能性がある。
 たとえば、リフレクトロン46及びフライトチューブ50等のコンポーネントについては、同軸ケーブル60を介して、数kv~数十kvの高電圧が印加されることがあり、このような場合、隙間72において数百mV程度の微小放電が生じる可能性がある。
 シールド線66の折り返し部66aと絶縁体64との間に隙間72を有する同軸ケーブル60を介して印加される電圧には、その隙間72に起因する微小放電に伴い、ノイズが含まれることになる。特に、リフレクトロン46及びフライトチューブ50等のコンポーネントは、印加される電圧がイオンの飛行時間に影響するため、その電圧にノイズが含まれると、測定結果に悪影響が生じる。
 また、飛行時間型質量分析装置10では、測定対象のイオンの極性を変更するために、電圧の極性、すなわち、正負を反転させることがあり、このような場合においても隙間72において微小放電が生じる可能性がある。電圧の極性の反転に伴って、隙間72で微小放電が生じるのであれば、隙間72における電界が安定し、微小放電が収まるまでの時間を要する。つまり、測定対象のイオンの極性を変更するために電圧の極性を反転させる際は、次の質量分析を行うまでの待機時間が長くなる可能性がある。
 そのため、本実施形態では、同軸ケーブル60に対して埋設処理工程を実施する。図6は、本実施形態に係る同軸ケーブル60の処理方法を説明するための図である。また、図6は、同軸ケーブル60の端部を示す概略断面図である。さらに、図6は、埋設処理工程及びカバー処理工程が実施された後の同軸ケーブル60を示す。
 埋設処理工程は、折り返し部66a及び絶縁体64の間に形成された隙間72に、絶縁性又は半導電性を有する埋設部材74を配置する工程である。絶縁性とは、導電性を全く有しないことを意味しており、半導電性とは、絶縁性よりも導電性を若干有し、たとえば体積抵抗率が103~1012Ω・cm程度であることを意味している。
 また、本実施形態では、埋設部材74としてテープ状の部材を用いるのであれば、埋設処理工程は、図3に示すように、巻き付け処理工程(ステップS3a)及び押し込み処理工程(ステップS3b)を含み、この順に沿って実施される。
 巻き付け処理工程は、折り返し部66aに対して同軸ケーブル60の先端側における絶縁体64の外周面に、テープ状の埋設部材74を巻き付ける工程である。押し込み処理工程は、絶縁体64の外周面に巻き付けられたテープ状の埋設部材74を、折り返し部66a側に向かって押し込む工程である。テープ状の埋設部材74の厚みは、隙間72の厚みd2(図5参照)よりも小さい。巻き付け処理工程では、テープ状の埋設部材74が、隙間72に入り込むように絶縁体64に巻き付けられることが好ましい。ただし、テープ状の埋設部材74が隙間72の外側(同軸ケーブル60の先端側)に巻き付けられた後、押し込み処理工程で埋設部材74が押し込まれることにより、埋設部材74が隙間72に入り込んでもよい。
 巻き付け処理工程によれば、埋設部材74を隙間72に簡単に配置することができ、押し込み処理工程によれば、埋設部材74が隙間72に押し込まれるため、隙間72をなるべく多く埋めることが可能とされる。
 なお、埋設部材74については、絶縁性又は半導電性を有し、隙間72に配置することが可能であれば、形状は特に限定されない。そのため、埋設部材74としては、たとえば、樹脂製又はシリコン製等の接着材を用いることもできる。
 また、本実施形態では、埋設部材74は、自己融着性を有していてもよい。自己融着性を有するテープ状の埋設部材74を絶縁体64の外周面に巻き付ける場合には、積層される埋設部材74同士が融着するため、粘着材を用いることなく埋設部材74を簡単に巻き付けることができる。また、埋設部材74として、自己融着性を有する部材を用いた場合、隙間72を簡単に埋めることが可能とされる。さらに、自己融着性を有する埋設部材74によれば、埋設部材74内に空気層を生じさせることなく、隙間72を埋めることができる。
 たとえば、埋設部材74として、自己融着性を有する絶縁テープを用いた場合、埋設部材74を隙間72に簡単に配置しつつ、隙間72をなるべく多く埋めることができる。さらに、絶縁テープ同士が融着するため、重なり合う絶縁テープ間における空気層を生じさせることなく、隙間72を埋めることができる。
 また、本実施形態では、埋設部材74の保護の観点から、埋設処理工程の後にカバー処理工程を実施する。ただし、カバー処理工程は、図6に示すように、シールド線66が外部シース68の表面に沿うように折り返されている場合に実施が可能とされる。
 カバー処理工程は、埋設部材74の周囲にカバー部材76を配置する工程である。カバー部材76としては、チューブ状又はテープ状の部材を用いることができ、たとえば熱収縮チューブが好適に用いられる。カバー処理工程によれば、埋設部材74を保護するだけでなく、埋設部材74が同軸ケーブル60から離れるのを防止することができる。
 また、カバー部材76を埋設部材74の周囲に配置した場合、装置の製造前などに複数本の同軸ケーブル60を並べて保管する際、各同軸ケーブル60の埋設部材74同士が接触するのを防止することができる。たとえば、埋設部材74として、自己融着性を有する部材が使用される場合においては、各同軸ケーブル60の埋設部材74同士が融着するのを防止することができる。
 カバー処理工程については、図6に示すように、カバー部材76の一部が折り返し部66aの周囲に位置するようにカバー部材76を配置するのが好ましい。カバー部材76の一部が折り返し部66aの周囲に位置するのであれば、埋設部材74が同軸ケーブル60の長さ方向に沿って移動するのを防止することができる。
 カバー部材76については、埋設部材74の周囲に配置することが可能であれば、特に限定されないが、熱収縮性を有する部材を用いるのが好ましい。カバー部材76として、熱収縮性を有する部材を用いるのであれば、カバー処理工程には、埋設部材74の周囲に配置されたカバー部材76に熱を加える工程を含む。
 熱収縮性を有するカバー部材76によれば、そのカバー部材76が埋設部材74の周囲に密着した状態で配置される。つまり、熱収縮性を有するカバー部材76によれば、埋設部材74が同軸ケーブル60、具体的には、絶縁体64に対して強固に固定される。また、このことから、カバー部材76の一部が折り返し部66aの周囲に位置するのであれば、埋設部材74が折り返し部66aに対して強固に固定される。
4.測定結果
 図7は、本実施形態に係る埋設処理工程による効果を説明するためのグラフである。また、図7は、部分放電測定器を使用し、隙間72における放電を測定した結果を示すグラフである。図7は、同軸ケーブル60に電圧を印加した際の放電電荷量を示しており、横軸が印加電圧、縦軸が放電電荷量を示す。放電電荷量が多いほど、隙間72に起因する微小放電の発生量が多いことを意味している。同軸ケーブル60に印加される電圧は、直流電圧であってもよいし、交流電圧であってもよい。なお、ここでの交流電圧には、電圧の極性が正負に交互に切り換えられることにより、電圧が矩形波を示す場合が含まれる。
 具体的に、実線は、埋設処理工程が実施されていない同軸ケーブル60に対応する放電電荷量を示し、破線は、埋設処理工程が実施済みの同軸ケーブル60に対応する放電電荷量を示す。なお、図7における電圧Vbの値は、電圧Vaの値よりも大きく、放電電荷量Qaの値は、放電電荷量Qbの値よりも大きい。
 埋設処理工程が実施されていない同軸ケーブル60においては、電圧Vaが印加された場合、放電電荷量が急激に増加する、すなわち、隙間72において微小放電が発生する。また、電圧Vaよりも高い電圧が同軸ケーブル60に印加されると、それに併せて、放電電荷量は、Qaまで増加する。
 一方、埋設処理工程が実施済みの同軸ケーブル60に電圧Vaが印加された場合、放電電荷量は安定している、すなわち、隙間72において微小放電は生じていない。また、埋設処理工程が実施済みの同軸ケーブル60に電圧Vbが印加された場合、放電電荷量が急激に増加するが、放電電荷量がQbまでしか増加しない。
 つまり、埋設処理工程によれば、隙間72における微小放電の発生が低減される。また、隙間72において、微小放電が生じたとしても、その放電電荷量が少ないため、印加電圧におけるノイズの含有率が低減される。たとえば、埋設処理工程が実施済みの同軸ケーブル60を介して、リフレクトロン46及びフライトチューブ50等のコンポーネントに電圧が印加されるのであれば、測定結果において微小放電の発生に伴う悪影響が低減される。
 また、埋設処理工程により、隙間72における微小放電の発生が低減されるのであれば、飛行時間型質量分析装置10において、測定対象のイオンの極性を変更するために電圧の極性を反転させる際に、微小放電が収まるまでの待機時間が長くなるのを防止することができる。
 なお、図3において図示は省略しているが、本実施形態では、露出処理工程及び折り返し処理工程等に加え、同軸ケーブル60を所定のコンポーネントに接続するために必要な工程、たとえば、中心導体62を露出させる工程等も実施される。また、本実施形態で挙げた具体的な構成及び方法等は一例であり、実際の製品に応じて適宜変更することが可能である。さらに、本実施形態で示したフロー図の各ステップは、同じ結果が得られるのであれば、処理される順番は適宜変更することが可能である。
5.態様
 上述した例示的な実施形態は、以下の態様の具体例であることが当業者により理解される。
 (第1項)一態様に係る同軸ケーブルの処理方法は、
 飛行時間型質量分析装置に電圧を印加するための同軸ケーブルの処理方法であって、
 中心導体と、前記中心導体の周囲に設けられた絶縁体と、前記絶縁体の周囲に設けられたシールド線と、前記シールド線の周囲に設けられた外部シースとを有する前記同軸ケーブルに対して、前記シールド線の先端部を前記外部シース側に折り返すことにより折り返し部を形成する折り返し処理工程と、
 前記折り返し部と前記絶縁体との間に形成された隙間に、絶縁性又は半導電性を有する埋設部材を配置する埋設処理工程とを含んでもよい。
 第1項に記載の同軸ケーブルの処理方法によれば、同軸ケーブルにおけるシールド線の折り返し部と絶縁体との間の隙間に、絶縁性又は半導電性を有する埋設部材が配置されるため、当該隙間に起因する微小放電の発生を低減することができる。同軸ケーブルにおける微小放電の発生が低減されるのであれば、飛行時間型質量分析装置において、測定結果に生じる悪影響を低減することができる。また、同軸ケーブルにおける微小放電の発生が低減されるのであれば、飛行時間型質量分析装置において、測定対象のイオンの極性を変更するために電圧の極性を反転させる際に、微小放電が収まるまでの待機時間が長くなるのを防止することができる。
(第2項)第1項に記載の同軸ケーブルの処理方法において、
 前記埋設処理工程は、前記折り返し部に対して前記同軸ケーブルの先端側における前記絶縁体の外周面に、テープ状の前記埋設部材を巻き付ける工程を含んでもよい。
 第2項に記載の同軸ケーブルの処理方法によれば、シールド線の折り返し部と絶縁体との間の隙間に埋設部材を簡単に配置することができる。
(第3項)第2項に記載の同軸ケーブルの処理方法において、
 前記埋設処理工程は、前記絶縁体の外周面に巻き付けられたテープ状の前記埋設部材を、前記折り返し部側に向かって押し込む工程を含んでもよい。
 第3項に記載の同軸ケーブルの処理方法によれば、シールド線の折り返し部と絶縁体との間の隙間に埋設部材が押し込まれるため、その隙間をなるべく多く埋めることができる。したがって、同軸ケーブルにおけるシールド線の折り返し部と絶縁体との間の隙間に起因する微小放電の発生をより低減することができる。
(第4項)第2項に記載の同軸ケーブルの処理方法において、
 前記埋設部材は、自己融着性を有していてもよい。
 第4項に記載の同軸ケーブルの処理方法によれば、シールド線の折り返し部と絶縁体との間の隙間を簡単に埋めることができ、さらに、埋設部材内に空気層を生じさせることなく、隙間を埋めることができる。したがって、同軸ケーブルにおけるシールド線の折り返し部と絶縁体との間の隙間に起因する微小放電の発生をより低減することができる。
(第5項)第1項に記載の同軸ケーブルの処理方法において、
 前記埋設部材の周囲にカバー部材を配置するカバー処理工程をさらに含んでいてもよい。
 第5項に記載の同軸ケーブルの処理方法によれば、埋設部材を保護しつつ、その埋設部材が同軸ケーブルから離れるのを防止することができる。また、このような処理方法によれば、各同軸ケーブルにおいて、互いの埋設部材が接触するのを防止することができる。
(第6項)第5項に記載の同軸ケーブルの処理方法において、
 前記カバー処理工程では、前記カバー部材の一部が前記折り返し部の周囲に位置するように前記カバー部材を配置してもよい。
 第6項に記載の同軸ケーブルの処理方法によれば、埋設部材が同軸ケーブルの長さ方向に沿って移動するのを防止することができる。
(第7項)第5項に記載の同軸ケーブルの処理方法において、
 前記カバー部材は、熱収縮性を有し、
 前記カバー処理工程は、前記埋設部材の周囲に配置された前記カバー部材に熱を加える工程を含んでいてもよい。
 第7項に記載の同軸ケーブルの処理方法によれば、埋設部材の周囲に密着した状態のカバー部材を配置することできる。したがって、埋設部材を同軸ケーブルに対して強固に固定することができる。
10   飛行時間型質量分析装置
60   同軸ケーブル
62   中心導体
64   絶縁体
66   シールド線
66a  折り返し部
68   外部シース
72   隙間
74   埋設部材
76   カバー部材
S2   折り返し処理工程
S3   埋設処理工程
S4   カバー処理工程

Claims (7)

  1.  飛行時間型質量分析装置に電圧を印加するための同軸ケーブルの処理方法であって、
     中心導体と、前記中心導体の周囲に設けられた絶縁体と、前記絶縁体の周囲に設けられたシールド線と、前記シールド線の周囲に設けられた外部シースとを有する前記同軸ケーブルに対して、前記シールド線の先端部を前記外部シース側に折り返すことにより折り返し部を形成する折り返し処理工程と、
     前記折り返し部と前記絶縁体との間に形成された隙間に、絶縁性又は半導電性を有する埋設部材を配置する埋設処理工程とを含む、同軸ケーブルの処理方法。
  2.  前記埋設処理工程は、前記折り返し部に対して前記同軸ケーブルの先端側における前記絶縁体の外周面に、テープ状の前記埋設部材を巻き付ける工程を含む、請求項1に記載の同軸ケーブルの処理方法。
  3.  前記埋設処理工程は、前記絶縁体の外周面に巻き付けられたテープ状の前記埋設部材を、前記折り返し部側に向かって押し込む工程を含む、請求項2に記載の同軸ケーブルの処理方法。
  4.  前記埋設部材は、自己融着性を有する、請求項2に記載の同軸ケーブルの処理方法。
  5.  前記埋設部材の周囲にカバー部材を配置するカバー処理工程をさらに含む、請求項1に記載の同軸ケーブルの処理方法。
  6.  前記カバー処理工程では、前記カバー部材の一部が前記折り返し部の周囲に位置するように前記カバー部材を配置する、請求項5に記載の同軸ケーブルの処理方法。
  7.  前記カバー部材は、熱収縮性を有し、
     前記カバー処理工程は、前記埋設部材の周囲に配置された前記カバー部材に熱を加える工程を含む、請求項5に記載の同軸ケーブルの処理方法。
PCT/JP2022/020059 2022-05-12 2022-05-12 同軸ケーブルの処理方法 Ceased WO2023218601A1 (ja)