WO2021131218A1 - Dispositif d'affichage d'image flexible et corps optique multicouche utilisé dans celui-ci - Google Patents

Dispositif d'affichage d'image flexible et corps optique multicouche utilisé dans celui-ci Download PDF

Info

Publication number
WO2021131218A1
WO2021131218A1 PCT/JP2020/037606 JP2020037606W WO2021131218A1 WO 2021131218 A1 WO2021131218 A1 WO 2021131218A1 JP 2020037606 W JP2020037606 W JP 2020037606W WO 2021131218 A1 WO2021131218 A1 WO 2021131218A1
Authority
WO
WIPO (PCT)
Prior art keywords
adhesive
layer
window
image display
layers
Prior art date
Application number
PCT/JP2020/037606
Other languages
English (en)
Japanese (ja)
Inventor
康隆 石原
孝伸 矢野
翔 寳田
Original Assignee
日東電工株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from JP2020159585A external-priority patent/JP6903804B1/ja
Application filed by 日東電工株式会社 filed Critical 日東電工株式会社
Priority to CN202080024732.8A priority Critical patent/CN113632235B/zh
Priority to KR1020217025545A priority patent/KR102401803B1/ko
Publication of WO2021131218A1 publication Critical patent/WO2021131218A1/fr

Abstract

La présente invention concerne un dispositif d'affichage d'image flexible qui est pourvu d'un élément de fenêtre, d'un premier élément, d'un premier corps multicouche ou d'un premier élément de panneau équipé d'un capteur tactile, et d'une pluralité de couches adhésives. Le premier corps multicouche est obtenu par l'empilement d'un deuxième élément et d'un troisième élément A. Dans les cas où ce dispositif d'affichage d'image flexible est pourvu du premier corps multicouche, l'un du premier élément et du deuxième élément est un film optique, tandis que l'autre est un film optique ou un capteur tactile ; et la pluralité de couches adhésives comprennent au moins trois couches qui sont disposées entre les éléments. Dans les cas où ce dispositif d'affichage d'image flexible est pourvu de l'élément de panneau doté d'un capteur tactile, la pluralité de couches adhésives comprend au moins deux couches qui sont disposées entre les éléments. De plus, l'expression E0 × T0 > 0,32 (où E0 représente le module d'élasticité (GPa) de l'élément de fenêtre et T0 représente l'épaisseur (mm) de l'élément de fenêtre) est satisfaite. Au moins l'une des couches adhésives possède une épaisseur de 20 µm ou plus ; et au moins l'une de la nième couche adhésive et de la (n +1)ième couche adhésive à partir du côté de l'élément de fenêtre possède une épaisseur de 10 µm ou plus.
PCT/JP2020/037606 2019-12-27 2020-10-02 Dispositif d'affichage d'image flexible et corps optique multicouche utilisé dans celui-ci WO2021131218A1 (fr)

Priority Applications (2)

Application Number Priority Date Filing Date Title
CN202080024732.8A CN113632235B (zh) 2019-12-27 2020-10-02 柔性图像显示装置以及用于其的光学层叠体
KR1020217025545A KR102401803B1 (ko) 2019-12-27 2020-10-02 플렉서블 화상 표시 장치 및 그에 이용하는 광학 적층체

Applications Claiming Priority (4)

Application Number Priority Date Filing Date Title
JP2019239513 2019-12-27
JP2019-239513 2019-12-27
JP2020-159585 2020-09-24
JP2020159585A JP6903804B1 (ja) 2019-12-27 2020-09-24 フレキシブル画像表示装置およびそれに用いる光学積層体

Publications (1)

Publication Number Publication Date
WO2021131218A1 true WO2021131218A1 (fr) 2021-07-01

Family

ID=76575876

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2020/037606 WO2021131218A1 (fr) 2019-12-27 2020-10-02 Dispositif d'affichage d'image flexible et corps optique multicouche utilisé dans celui-ci

Country Status (4)

Country Link
JP (1) JP6903830B1 (fr)
KR (1) KR102401803B1 (fr)
TW (1) TWI753601B (fr)
WO (1) WO2021131218A1 (fr)

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2019517974A (ja) * 2016-03-17 2019-06-27 コーニング インコーポレイテッド 曲げられる電子デバイスモジュールおよび物品、並びにそれを製造するための結合方法
JP2019197235A (ja) * 2017-11-10 2019-11-14 住友化学株式会社 円偏光板
WO2019244499A1 (fr) * 2018-06-22 2019-12-26 日東電工株式会社 Couche d'agent adhésif pour dispositif d'affichage d'image souple, corps stratifié pour dispositif d'affichage d'image souple, et dispositif d'affichage d'image souple

Family Cites Families (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6867539B1 (en) * 2000-07-12 2005-03-15 3M Innovative Properties Company Encapsulated organic electronic devices and method for making same
JP2007233215A (ja) * 2006-03-03 2007-09-13 Nippon Zeon Co Ltd 偏光板
JP2012158153A (ja) * 2011-02-02 2012-08-23 Nitto Denko Corp ガラス用保護シート
KR102069286B1 (ko) * 2015-11-20 2020-01-22 동우 화인켐 주식회사 플렉서블 표시 장치
KR101827614B1 (ko) * 2015-12-21 2018-03-23 성균관대학교산학협력단 방수 특성이 향상된 배리어 및 이를 포함하는 oled
KR102494986B1 (ko) 2016-01-11 2023-02-03 삼성디스플레이 주식회사 폴더블 표시장치
CN110249376B (zh) * 2017-01-06 2021-08-24 大日本印刷株式会社 光学膜和图像显示装置
KR101903888B1 (ko) * 2017-05-10 2018-10-02 동우 화인켐 주식회사 광학 적층체 및 이를 포함하는 플렉서블 디스플레이
KR102318145B1 (ko) * 2017-09-15 2021-10-26 동우 화인켐 주식회사 플렉시블 디스플레이 장치
KR102436547B1 (ko) * 2017-09-29 2022-08-29 삼성디스플레이 주식회사 전자 장치
KR20190044267A (ko) * 2017-10-20 2019-04-30 동우 화인켐 주식회사 플렉시블 디스플레이 장치

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2019517974A (ja) * 2016-03-17 2019-06-27 コーニング インコーポレイテッド 曲げられる電子デバイスモジュールおよび物品、並びにそれを製造するための結合方法
JP2019197235A (ja) * 2017-11-10 2019-11-14 住友化学株式会社 円偏光板
WO2019244499A1 (fr) * 2018-06-22 2019-12-26 日東電工株式会社 Couche d'agent adhésif pour dispositif d'affichage d'image souple, corps stratifié pour dispositif d'affichage d'image souple, et dispositif d'affichage d'image souple

Also Published As

Publication number Publication date
KR20210106573A (ko) 2021-08-30
JP6903830B1 (ja) 2021-07-14
JP2021107924A (ja) 2021-07-29
TWI753601B (zh) 2022-01-21
KR102401803B1 (ko) 2022-05-26
TW202124144A (zh) 2021-07-01

Similar Documents

Publication Publication Date Title
CN115312672B (zh) 挠性图像显示装置用层叠体及挠性图像显示装置
TW202325815A (zh) 可撓性圖像顯示裝置用黏著劑組合物、可撓性圖像顯示裝置用黏著劑層、可撓性圖像顯示裝置用積層體及可撓性圖像顯示裝置
WO2021066191A1 (fr) Dispositif d'affichage et corps stratifié de matériau de base
JP6934996B2 (ja) フレキシブル画像表示装置およびそれに用いる光学積層体
JP6858912B2 (ja) フレキシブル画像表示装置およびそれに用いる光学積層体
JP2021152657A (ja) 表示装置及び基材積層体
WO2021131152A1 (fr) Corps stratifié décoratif, corps stratifié optique, et dispositif d'affichage d'image flexible
JP6903804B1 (ja) フレキシブル画像表示装置およびそれに用いる光学積層体
JP6903830B1 (ja) フレキシブル画像表示装置およびそれに用いる光学積層体
CN114502367A (zh) 显示装置及基材层叠体
JP2021173773A (ja) 偏光フィルム、光学積層体、および画像表示装置

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 20908251

Country of ref document: EP

Kind code of ref document: A1

ENP Entry into the national phase

Ref document number: 20217025545

Country of ref document: KR

Kind code of ref document: A

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 20908251

Country of ref document: EP

Kind code of ref document: A1