WO2008131329A1 - Différentiel d'énergie de surface de moule à lentille ophtalmique - Google Patents

Différentiel d'énergie de surface de moule à lentille ophtalmique Download PDF

Info

Publication number
WO2008131329A1
WO2008131329A1 PCT/US2008/061004 US2008061004W WO2008131329A1 WO 2008131329 A1 WO2008131329 A1 WO 2008131329A1 US 2008061004 W US2008061004 W US 2008061004W WO 2008131329 A1 WO2008131329 A1 WO 2008131329A1
Authority
WO
WIPO (PCT)
Prior art keywords
mold
lens
mold part
thermal plastic
surface energy
Prior art date
Application number
PCT/US2008/061004
Other languages
English (en)
Inventor
Changhong Yin
Scott F. Ansell
Original Assignee
Johnson & Johnson Vision Care, Inc.
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from US11/753,198 external-priority patent/US20080290534A1/en
Application filed by Johnson & Johnson Vision Care, Inc. filed Critical Johnson & Johnson Vision Care, Inc.
Priority to AU2008242679A priority Critical patent/AU2008242679A1/en
Priority to BRPI0810237-6A2A priority patent/BRPI0810237A2/pt
Priority to EP08746429A priority patent/EP2152503A1/fr
Priority to CA002684870A priority patent/CA2684870A1/fr
Priority to JP2010504307A priority patent/JP2010524729A/ja
Publication of WO2008131329A1 publication Critical patent/WO2008131329A1/fr

Abstract

L'invention concerne des parties de moule améliorées façonnées à partir d'une résine thermoplastique mélangée avec un additif pour réduire l'énergie de surface de la partie de moule (à moins de 30 mN/m). Les parties de moule peuvent être utilisées dans des procédés de fabrication, tels que, par exemple : les procédés continus, en ligne ou discontinus de moule à lentille ophtalmique.
PCT/US2008/061004 2007-04-20 2008-04-21 Différentiel d'énergie de surface de moule à lentille ophtalmique WO2008131329A1 (fr)

Priority Applications (5)

Application Number Priority Date Filing Date Title
AU2008242679A AU2008242679A1 (en) 2007-04-20 2008-04-21 Ophthalmic lens mold surface energy differential
BRPI0810237-6A2A BRPI0810237A2 (pt) 2007-04-20 2008-04-21 Energia de superfície diferencial de molde de lente oftálmica
EP08746429A EP2152503A1 (fr) 2007-04-20 2008-04-21 Différentiel d'énergie de surface de moule à lentille ophtalmique
CA002684870A CA2684870A1 (fr) 2007-04-20 2008-04-21 Differentiel d'energie de surface de moule a lentille ophtalmique
JP2010504307A JP2010524729A (ja) 2007-04-20 2008-04-21 眼科レンズ用鋳型表面エネルギー差

Applications Claiming Priority (4)

Application Number Priority Date Filing Date Title
US91307807P 2007-04-20 2007-04-20
US60/913,078 2007-04-20
US11/753,198 2007-05-24
US11/753,198 US20080290534A1 (en) 2007-05-24 2007-05-24 Ophthalmic lens mold surface energy differential

Publications (1)

Publication Number Publication Date
WO2008131329A1 true WO2008131329A1 (fr) 2008-10-30

Family

ID=39671408

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/US2008/061004 WO2008131329A1 (fr) 2007-04-20 2008-04-21 Différentiel d'énergie de surface de moule à lentille ophtalmique

Country Status (10)

Country Link
EP (1) EP2152503A1 (fr)
JP (1) JP2010524729A (fr)
KR (1) KR20100017185A (fr)
AR (1) AR066116A1 (fr)
AU (1) AU2008242679A1 (fr)
BR (1) BRPI0810237A2 (fr)
CA (1) CA2684870A1 (fr)
RU (1) RU2009142845A (fr)
TW (1) TW200912424A (fr)
WO (1) WO2008131329A1 (fr)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2009073076A1 (fr) * 2007-12-06 2009-06-11 Johnson & Johnson Vision Care, Inc. Libération de lentille ophtalmique améliorée
WO2016097152A3 (fr) * 2014-12-17 2016-11-24 Dsm Ip Assets B.V. Matière plastique pour dispositif de formage industriel
US10386653B2 (en) 2012-12-21 2019-08-20 Johnson & Johnson Vision Care, Inc. Variable optic ophthalmic device including liquid crystal elements

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104115053B (zh) * 2011-12-23 2016-04-20 庄臣及庄臣视力保护公司 包括液晶元件的可变光学眼科装置

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2001070490A2 (fr) * 2000-03-22 2001-09-27 Johnson & Johnson Vision Care, Inc. Moules destines a la fabrication de dispositifs ophtalmiques
EP1752281A2 (fr) * 2005-08-09 2007-02-14 CooperVision Inc. Moule pour la fabrication de lentilles de contact et systèmes et procédés pour leur fabrication

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2001070490A2 (fr) * 2000-03-22 2001-09-27 Johnson & Johnson Vision Care, Inc. Moules destines a la fabrication de dispositifs ophtalmiques
EP1752281A2 (fr) * 2005-08-09 2007-02-14 CooperVision Inc. Moule pour la fabrication de lentilles de contact et systèmes et procédés pour leur fabrication

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2009073076A1 (fr) * 2007-12-06 2009-06-11 Johnson & Johnson Vision Care, Inc. Libération de lentille ophtalmique améliorée
US10386653B2 (en) 2012-12-21 2019-08-20 Johnson & Johnson Vision Care, Inc. Variable optic ophthalmic device including liquid crystal elements
WO2016097152A3 (fr) * 2014-12-17 2016-11-24 Dsm Ip Assets B.V. Matière plastique pour dispositif de formage industriel
EP3479985A3 (fr) * 2014-12-17 2019-06-05 DSM IP Assets B.V. Matière plastique pour formeur industriel
US11224997B2 (en) 2014-12-17 2022-01-18 Dsm Ip Assets B.V. Plastic material for industrial former

Also Published As

Publication number Publication date
JP2010524729A (ja) 2010-07-22
AR066116A1 (es) 2009-07-22
CA2684870A1 (fr) 2008-10-30
TW200912424A (en) 2009-03-16
EP2152503A1 (fr) 2010-02-17
BRPI0810237A2 (pt) 2014-10-29
RU2009142845A (ru) 2011-05-27
AU2008242679A1 (en) 2008-10-30
KR20100017185A (ko) 2010-02-16

Similar Documents

Publication Publication Date Title
EP1629960B1 (fr) Procédé et Moules pour la fabrication de lentilles ophthalmiques& xA;
US20080290534A1 (en) Ophthalmic lens mold surface energy differential
JP6010832B2 (ja) 眼科学デバイス成型用金型及び関連する方法
EP2136987A1 (fr) Moules avec élastomères thermoplastiques pour production de lentilles ophtalmiques
JP5236653B2 (ja) 眼用レンズ製造の間の余分な重合体リングの除去
EP1857246A1 (fr) Moule pour un dispositif biomédical
US20070284770A1 (en) Decreased lens delamination during ophthalmic lens manufacture
WO2008131329A1 (fr) Différentiel d'énergie de surface de moule à lentille ophtalmique
TW200824881A (en) Electrostatic charge during ophthalmic lens manufacture
CN101663158A (zh) 眼科镜片模具表面能差
US20090146329A1 (en) Lens release

Legal Events

Date Code Title Description
WWE Wipo information: entry into national phase

Ref document number: 200880012790.8

Country of ref document: CN

121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 08746429

Country of ref document: EP

Kind code of ref document: A1

WWE Wipo information: entry into national phase

Ref document number: 2008242679

Country of ref document: AU

WWE Wipo information: entry into national phase

Ref document number: 3578/KOLNP/2009

Country of ref document: IN

WWE Wipo information: entry into national phase

Ref document number: 2010504307

Country of ref document: JP

WWE Wipo information: entry into national phase

Ref document number: 2684870

Country of ref document: CA

NENP Non-entry into the national phase

Ref country code: DE

ENP Entry into the national phase

Ref document number: 2008242679

Country of ref document: AU

Date of ref document: 20080421

Kind code of ref document: A

ENP Entry into the national phase

Ref document number: 20097024210

Country of ref document: KR

Kind code of ref document: A

WWE Wipo information: entry into national phase

Ref document number: 2009142845

Country of ref document: RU

Ref document number: 2008746429

Country of ref document: EP

ENP Entry into the national phase

Ref document number: PI0810237

Country of ref document: BR

Kind code of ref document: A2

Effective date: 20091020