- Publication number
- US20230034282A1 US20230034282A1 US17/964,900 US202217964900A US2023034282A1 US 20230034282 A1 US20230034282 A1 US 20230034282A1 US 202217964900 A US202217964900 A US 202217964900A US 2023034282 A1 US2023034282 A1 US 2023034282A1
- Authority
- US
- United States
- Prior art keywords
- disposed
- area
- pattern
- electrode
- substrate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
An organic light-emitting diode panel for a lighting device includes a substrate including an array area having an emission area and a dummy area disposed outside the array area, an auxiliary wiring pattern, a first electrode, a passivation pattern, an OLED emission structure, a second electrode, an adhesive layer, and an encapsulation layer. The passivation pattern and the adhesive layer have an uneven boundary surface therebetween in the dummy area. Alternatively, a lower surface of the adhesive layer has a 3D structure. Thus, a moisture intrusion path between the passivation pattern and the adhesive layer of the dummy area of the substrate may be increased. Thus, degradation of the OLED emission structure due to external moisture intrusion may be reduced or prevented.
Description
- This application is a division of U.S. patent application Ser. No. 16/209,344, filed on Dec. 4, 2018, which claims priority under 35 U.S.C. § 119 to Korean Application No. 10-2017-0172831, filed on Dec. 15, 2017, whose entire disclosure is herein incorporated by reference.
- The present disclosure relates to a light-emitting panel for a lighting device, and more particularly, to an organic light-emitting diode (OLED) panel having an excellent moisture intrusion delay effect and excellent life characteristics.
- Fluorescent lamps or incandescent lamps are mainly used as lighting devices. For incandescent lamps, a color rendering index is high, but energy efficiency is very low. For fluorescent lamps, while energy efficiency is high, a color rendering index is low. Furthermore, since a fluorescent lamp contains mercury, an environmental problem occurs.
- Recently, light-emitting diode (LED) based lighting devices have been suggested. LEDs are formed in a stack structure of a nitride semiconductor such as GaN. LEDs have the highest emission efficiency in a blue wavelength range, and the emission efficiency gradually decreases toward a red wavelength range and a green wavelength range having the maximum luminous efficacy. Accordingly, when a white light is emitted by combining a red emission diode, a green emission diode, and a blue emission diode, the emission efficiency may deteriorate. Furthermore, when a red emission diode, a green emission diode, and a blue emission diode are in use, color rendering characteristics may deteriorate because the width of an emission peak of each diode is narrow.
- To solve the above problem, instead of combining a red emission diode, a green emission diode, and a blue emission diode, a lighting device that outputs a white light by combining a blue emission diode and yellow phosphor has been suggested. The lighting device configured as above has been suggested because it is more efficient to use only the blue emission diode having relatively high emission efficiency, instead of using the green emission diode having relatively low emission efficiency, and to use, for the other colors, a phosphor substance emitting a yellow light by receiving a blue light.
- However, in the lighting device that outputs a white light by combining a blue emission diode and a yellow phosphor, the phosphor substance for emitting a yellow light has poor emission efficiency. Thus, there has been a limitation in improving the emission efficiency of a lighting device.
- In particular, in the case of a nitride semiconductor LED based lighting device, a heat dissipation device is disposed on a rear surface of a lighting device due to a lot of heat generated from a light-emitting diode. Furthermore, for high-quality growth of nitride semiconductor, an expensive sapphire substrate is used.
- Furthermore, in the case of a nitride semiconductor light-emitting diode based lighting device, there are many processes including an epitaxy growth for growing nitride semiconductor, a chip process for manufacturing individual light-emitting diode chips, and a mounting process for mounting individual light-emitting diode chips on a circuit board.
- To solve the above problems of the nitride semiconductor light-emitting diode based lighting device, much research has been conducted on organic light-emitting diode (OLED) based lighting devices.
- Since organic light-emitting diodes can be made in a large area, surface emission is available. Also, an expensive sapphire substrate for forming a nitride semiconductor light-emitting diode is not necessary. Furthermore, not much heat is generated compared to the nitride semiconductor light-emitting diode.
- However, in an OLED based lighting device, an OLED is vulnerable to moisture. In the OLED, intrusion of moisture occurs in a dummy area at an edge side of a substrate, mostly through a boundary surface between a passivation pattern and an adhesive layer for forming an encapsulation layer. As the intrusion of moisture continues in the OLED, the OLED may deteriorate and light emission performance may be degraded. Accordingly, the life characteristics of a lighting device may deteriorate.
- An embodiment of the present disclosure provides an organic light-emitting diode (OLED) panel.
- Another embodiment of the present disclosure provides an OLED panel which may prevent deterioration of an OLED light-emitting structure due to intrusion of moisture by increasing a moisture intrusion path.
- The present disclosure is not limited to the above-described embodiments, and other embodiments and advantages can be appreciated by those skilled in the art from the following descriptions.
- In accordance with a first aspect of the present disclosure, an OLED panel for a lighting device according to an embodiment includes an array area having an emission area and a dummy area disposed outside the array area, and comprises a substrate, an auxiliary wiring pattern, a first electrode, a passivation pattern, an OLED emission structure, a second electrode, and an adhesive layer.
- The auxiliary wiring pattern may be disposed on the substrate. The first electrode may be disposed on the substrate where the auxiliary wiring pattern is disposed. The passivation pattern may be disposed on the substrate where the first electrode is disposed, and may surround the auxiliary wiring pattern and the first electrode in the dummy area. The OLED emission structure may be disposed on the substrate where the passivation pattern is disposed in the array area. The second electrode may be disposed on the substrate where the OLED emission structure is disposed. The adhesive layer may be disposed on the substrate where the second electrode is disposed and may contact the passivation pattern in the dummy area. An optional encapsulation layer may be disposed on the adhesive layer.
- In an OLED panel for a lighting device according to the present disclosure, the passivation pattern and the adhesive layer may have an uneven boundary surface therebetween in the dummy area. The uneven boundary surface between the passivation pattern and the adhesive layer in the dummy area increases a path along which moisture intrudes, and thus degradation of the OLED emission structure due to external moisture intrusion may be prevented. Furthermore, the uneven boundary surface between the passivation pattern and the adhesive layer in the dummy area may act as a barrier to the moisture intrusion. Accordingly, the uneven boundary surface between the passivation pattern and the adhesive layer in the dummy area may improve life characteristics of the OLED panel.
- Also, one or more dummy structure patterns may be arranged in the dummy area of the substrate, and the passivation pattern in the dummy area may have an uneven surface corresponding to the surface of the substrate where the dummy structure pattern is arranged. When the dummy structure pattern is arranged in the dummy area of the substrate, the auxiliary wiring pattern, the first electrode, and the passivation pattern, which are provided thereon in a deposition method, may also have an uneven surface corresponding to the surface of the substrate where the dummy structure pattern is arranged. As a result, an uneven surface boundary may be formed between the passivation pattern and the adhesive layer in the dummy area.
- The dummy structure pattern to form the uneven surface boundary between the passivation pattern and the adhesive layer in the dummy area may include a light extraction material. To increase light extraction efficiency of a lighting device, a light extraction pattern may be generally arranged in the array area on the substrate. The light extraction pattern may be formed by inkjet coating. When the light extraction pattern is also arranged in the dummy area on the substrate, the dummy structure pattern including the light extraction material may be formed.
- In another example, the dummy structure pattern to form the uneven surface boundary between the passivation pattern and the adhesive layer in the dummy area may include the same material as the auxiliary wiring pattern. The auxiliary wiring pattern may be arranged in the entire area of the substrate except an emission area by depositing metal in the entire area of the substrate except a part of a pad area, and etching the emission area. Alternatively, the auxiliary wiring pattern may be arranged in the entire area of the substrate except an emission area by depositing metal in the entire area of the substrate and etching the emission area. Alternatively, the auxiliary wiring pattern may be arranged in the entire area of the substrate except an emission area and a part of a pad area by depositing metal in the entire area of the substrate except a part of the pad area, and etching the emission area. Alternatively, metal may be deposited in the entire area of the substrate, and a part of the pad area and the emission area of the array area is etched and thus the auxiliary wiring pattern may be arranged in the entire area, except the etched areas. In this state, when etching is performed on a part of the auxiliary wiring pattern in the dummy area, the dummy structure pattern may be formed.
- Furthermore, the capping layer formed of an organic material and/or an inorganic material may be further provided on the second electrode. As the capping layer is provided on the second electrode, the intrusion of moisture into the OLED emission structure from above may be effectively prevented, and the light generated from the OLED emission structure may be effectively extracted.
- In accordance with a second aspect of the present disclosure, an OLED panel for a lighting device according to another embodiment, like the above-described embodiment, includes the auxiliary wiring pattern, the first electrode, the passivation pattern, the OLED emission structure, the second electrode, the adhesive layer, and the encapsulation layer, which are sequentially disposed on the substrate. In the present embodiment, a lower surface of the adhesive layer in the dummy area may have a three-dimensional (3D) structure. Preferably, one or more grooves penetrating through the passivation pattern arranged in the dummy area of the substrate may be provided, and a part of the adhesive layer may be provided in the groove.
- Through the groove penetrating through the passivation pattern arranged in the dummy area of the substrate, the lower surface of the adhesive layer in the dummy area may have a 3D structure. Accordingly, the path along which moisture intrudes may be increased, and thus degradation of the OLED emission structure due to external moisture intrusion may be prevented. Furthermore, the passivation pattern between the grooves may act as a barrier to the moisture intrusion.
- Preferably, the groove may further penetrate through the first electrode and the auxiliary wiring pattern arranged under the passivation pattern in the dummy area of the substrate. Furthermore, the side wall of the groove may have a step shape. Since the height and the step-shaped structure of the groove may further increase the path of the moisture intrusion, high moisture intrusion delay effect may be obtained.
- In accordance with a third aspect of the present disclosure, similar to the above-described embodiment of the first aspect, an OLED panel for a lighting device according to another embodiment, which includes an array area having an emission area and a pad area disposed near the array area, comprising the auxiliary wiring pattern, the first electrode, the passivation pattern, the OLED emission structure, the second electrode, and the optional adhesive layer and the optional encapsulation layer, which are sequentially disposed on the substrate. In the present embodiment, a pad including the same material as the auxiliary wiring pattern is disposed on the substrate in the pad area and contacts the passivation pattern, and the passivation pattern and the pad have an uneven boundary surface therebetween.
- The uneven boundary surface between the passivation pattern and the pad increases a path along which moisture intrudes, and thus degradation of the OLED emission structure due to external moisture intrusion may be prevented. Furthermore, the uneven boundary surface between the passivation pattern and the pad may act as a barrier to the moisture intrusion. Accordingly, the uneven boundary surface between the passivation pattern and the pad may improve life characteristics of the OLED panel.
-
FIG. 1 is a schematic plan view of an OLED panel for a lighting device according to an embodiment of the present disclosure. -
FIG. 2 is a cross-sectional view taken along line I-I′ ofFIG. 1 -
FIG. 3 is an example of a cross-sectional view taken along line II-II′ ofFIG. 1 . -
FIG. 4 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . -
FIG. 5 is a schematic plan view illustrating an example of a dummy structure pattern. -
FIG. 6 is a schematic plan view illustrating another example of a dummy structure pattern. -
FIG. 7 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . -
FIG. 8 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . -
FIG. 9 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . -
FIG. 10 is a schematic plan view of an OLED panel for a lighting device according to another embodiment of the present disclosure. -
FIG. 11 is a cross-sectional view taken along line III-III′ ofFIG. 10 . - Hereinafter, an OLED panel for a lighting device according to embodiments of the present disclosure, and a manufacturing method thereof, will be described in detail with reference to the accompanying drawings.
- Terms such as “first” and “second” are used herein merely to describe a variety of constituent elements, but the constituent elements are not limited by the terms. Such terms are used only for the purpose of distinguishing one constituent element from another constituent element.
- Furthermore, in the present disclosure, when a constituent element is disposed “above” or “on” to another constituent element, the constituent element may be not only directly on the other constituent element, but also above the other constituent element in a non-contact manner through at least one of other constituent elements, e.g., a third constituent element.
-
FIG. 1 is a schematic plan view of an OLED panel for a lighting device according to an embodiment of the present disclosure.FIG. 2 is a cross-sectional view taken along line I-I′ ofFIG. 1 , showing an array area.FIG. 3 is an example of a cross-sectional view taken along line II-II′ ofFIG. 1 , showing a dummy area. - Referring to
FIGS. 1 to 3 , the OLED panel for a lighting device according to the present disclosure may include asubstrate 110, an auxiliary wiring pattern 120 (indicated by dotted lines inFIG. 1 ), afirst electrode 130, apassivation pattern 140, an OLED emission structure 150 (not shown inFIG. 1 ), asecond electrode 160, an adhesive layer 167 (not shown inFIG. 1 ), and an encapsulation layer 170 (not shown inFIG. 1 ). - The
substrate 110 may be a glass substrate. Furthermore, thesubstrate 110 may be formed of a polymer material such as polyimide (PI), poly(ethylene naphthalate) (PEN), or poly(ethylene terephthalate) (PET) to exhibit flexibility characteristics. When thesubstrate 110 is formed of a polymer material, a flexible OLED panel for a lighting device may be manufactured by a roll-to-roll process. - Referring to
FIGS. 1 and 3 , thesubstrate 110 may include an array area AA and a dummy area DA outside the array area AA. Although inFIGS. 1 and 3 the array area AA and the dummy area DA are divided with respect to thesecond electrode 160, this is a mere example and the present disclosure is not limited thereto. For example, the array area AA and the dummy area DA may be divided with respect to theOLED emission structure 150. - As shown in
FIG. 1 , the array area AA may include one or more emission areas EA in which the OLED emission structure 150 (seeFIG. 3 ) emits light. The emission area may be defined to be an area in the array area AA in which a lower surface of theOLED emission structure 150 contacts thefirst electrode 130, for example, an anode electrode, and an upper surface of theOLED emission structure 150 contacts thesecond electrode 160, for example, a cathode electrode. - Although not illustrated, a barrier layer may be provided on an upper surface of the
substrate 110. The barrier layer may restrict a reaction between thesubstrate 110 and theauxiliary wiring pattern 120 and a reaction between thesubstrate 110 and thefirst electrode 130. The barrier layer may include an inorganic material such as SiO2 or SiNx, but the present disclosure is not limited thereto. - Furthermore, referring to
FIG. 2 , alight extraction pattern 115 may be disposed on thesubstrate 110, for example, between thesubstrate 110 and theauxiliary wiring pattern 120, in the array area AA. Thelight extraction pattern 115 may include a light extraction material. The light extraction material may be light scattering particles having high refraction indexes such as TiO2, BaTiO3, ZrO2, ZnO, or SiO2. Thelight extraction pattern 115 may be in the form of a film, and preferably an inkjet print pattern. Thelight extraction pattern 115 may contribute to obtaining light extraction efficiency. - The
auxiliary wiring pattern 120 is disposed on thesubstrate 110. Theauxiliary wiring pattern 120 functions as follows. Thefirst electrode 130 may be generally formed of a transparent conductive oxide (TCO) material such as indium tin oxide (ITO) or fluorine-doped tin oxide (FTO). The transparent conductive oxide material may have a merit of transmitting the light emitted from theOLED emission structure 150 and also have a demerit of having very high electrical resistance compared to metal. Accordingly, when a large sized OLED panel for a lighting device is manufactured, a distribution of applied voltages is irregular across the overall first electrode due to high resistance of a transparent conductive oxide. Such irregular voltage distribution may deteriorate luminance uniformity of a large sized lighting device. - Accordingly, the
auxiliary wiring pattern 120 is formed of a material having resistance lower than that of the transparent conductive oxide which is used to make thefirst electrode 130, for example, metal such as Cu or Al. Thus, theauxiliary wiring pattern 120 functions to allow the distribution of a voltage applied to thefirst electrode 130 that is provided in contact with theauxiliary wiring pattern 120 to be entirely uniform over thefirst electrode 130. - Although the
auxiliary wiring pattern 120 may have a net shape as illustrated inFIG. 1 , the present disclosure is not limited thereto. Furthermore, although theauxiliary wiring pattern 120 may have a shape close to a left to right symmetry, the present disclosure is not limited thereto. Furthermore, although inFIG. 2 theauxiliary wiring pattern 120 has an end having a vertical shape forming a rectangular cross-section, the end of theauxiliary wiring pattern 120 may have an inclined shape, and a tapered sectional shape in this case. - The
first electrode 130 is disposed on thesubstrate 110 on which theauxiliary wiring pattern 120 is disposed. Thefirst electrode 130 is connected to afirst electrode pad 130 a as illustrated inFIG. 1 . Thefirst electrode 130 may be formed of a transparent conductive oxide material such as ITO, and may be formed by sputtering process or coating process. - The
auxiliary wiring pattern 120 may include a metal material, and thefirst electrode 130 may include a transparent conductive oxide material. To have light extraction in a downward direction or both of upward and downward directions, thefirst electrode 130 may include a transparent conductive oxide material. As described above, theauxiliary wiring pattern 120 may compensate for the high resistance of a transparent conductive oxide, contributing to application of an overall uniform voltage to thefirst electrode 130. - The
first electrode 130 may be an anode electrode, and thesecond electrode 160 described later may be a cathode electrode. Reversely, while thefirst electrode 130 may be a cathode electrode, thesecond electrode 160 may be an anode electrode. - The
passivation pattern 140 is disposed on thefirst electrode 130. Thepassivation pattern 140 may be disposed in an area where theauxiliary wiring pattern 120 is disposed. Furthermore, thepassivation pattern 140, as illustrated inFIG. 3 , may have a shape surrounding theauxiliary wiring pattern 120 and thefirst electrode 130 in the dummy area DA. - When, in OLED lighting, a short circuit is generated between the
first electrode 130 and thesecond electrode 160 due to moisture intrusion, luminance degradation may occur not only in a shorted portion but also in an entire panel due to current drop. To prevent the above, thepassivation pattern 140 is formed at least in an area where at least theauxiliary wiring pattern 120 is disposed. - The
passivation pattern 140 may be formed of an organic material such as polyimide based material, or an inorganic material such as alumina (Al2O3) or silicon nitride (SiNx). A passivation material may be deposited by an atomic layer deposition (ALD) method or a chemical vapor deposition (CVD) method. - Furthermore, as illustrated in
FIG. 2 , anopening 135 for exposing thesubstrate 110 may be disposed in thefirst electrode 130. Thepassivation pattern 140 is additionally provided in theopening 135. As thepassivation pattern 140 is additionally provided in theopening 135, intrusion of moisture or air into the OLED emission structure may be effectively restricted. - The
OLED emission structure 150 is disposed in the array area AA on thesubstrate 110 where thepassivation pattern 140 is disposed. Referring toFIGS. 2 and 3 , one part of the lower surface of theOLED emission structure 150 contacts thepassivation pattern 140, and the other part thereof contacts thefirst electrode 130. The portion where theOLED emission structure 150 and thepassivation pattern 140 contact each other may be a non-emission area, and a portion where theOLED emission structure 150 and thefirst electrode 130 contact each other may be an emission area. - The
OLED emission structure 150 may include an organic emission layer (EML), a hole injection layer (HIL) and/or a hole transport layer (HTL) for providing holes to the organic emission layer, and an electron transport layer (ETL) and/or an electron injection layer (EIL) for providing electrons to the organic emission layer. - Each layer of the
OLED emission structure 150 may be formed by depositing an organic material, for example, copperphthalocyanine (CuPc), N,N′-Di(naphthalene-1-yl)-N,N′-diphenylbenzidine (NPB), or tris-8-hydroxyquinoline aluminum (Alq3), in a vacuum deposition method. - The
second electrode 160 is disposed on thesubstrate 110 where theOLED emission structure 150 is disposed. Referring toFIGS. 1 and 3 , in the OLED panel for a lighting device according to the present disclosure, thesecond electrode 160 is disposed in the array area AA. Thesecond electrode 160 is connected to each ofsecond electrode pads 160 a, as illustrated inFIG. 1 . Thesecond electrode 160 may be formed of a transparent conductive oxide material such as ITO, or a metal material. - Referring to
FIGS. 2 and 3 , acapping layer 165 may be disposed on thesecond electrode 160. As thecapping layer 165 is disposed on thesecond electrode 160, intrusion of moisture into theOLED emission structure 150 from the above may be effectively prevented. Furthermore, in the case of a double-sided emission type, thecapping layer 165 may contribute to effective extraction of light generated from the OLED emission structure in an upward direction. Thecapping layer 165 may include one or more inorganic materials such as SiO2, SiNx, MgF2, ZnO, TiO2, ZrO2, NiO, or one or more organic materials such as GaN, or acryl, polyimide, polyamide, poly(3,4-ethylenedioxythiophene (PEDOT), or include a mixture of the inorganic material and the organic material. Furthermore, thecapping layer 165 may have a monolayer structure or a multilayer structure of at least two layers. - The
adhesive layer 167 is provided to arrange theencapsulation layer 170, and is disposed on thesubstrate 110 where thesecond electrode 160 is disposed. An upper surface of theadhesive layer 167 may be planarized. - The
encapsulation layer 170 is disposed on theadhesive layer 167 and prevents intrusion of external moisture or air. Theencapsulation layer 170 may be formed of an organic material such as an acrylate based compound or an epoxy based compound, an inorganic material such as ceramic or metal, or an organic/inorganic composite material, and may be in the form of a film having a monolayer structure or a multilayer structure. - A protection film may be disposed on the
encapsulation layer 170 via an additional adhesive layer. The protection film may prevent the intrusion of external moisture or air. The protection film may be a PET substrate or metal foil. - Referring to
FIG. 1 , thefirst electrode pad 130 a is disposed in a pad area PA and connected to thefirst electrode 130. Each of thesecond electrode pads 160 a is connected to thesecond electrode 160. InFIG. 1 , thefirst electrode pad 130 a is disposed in a center portion of the pad area PA, and thesecond electrode pads 160 a are disposed at both sides of thefirst electrode pad 130 a. However, the arrangement, size, or number of the electrode pads may vary as necessary. - The
first electrode pad 130 a may include a lower layer of the same material as theauxiliary wiring pattern 120 and an optional upper layer of the same material as thefirst electrode 130. The lower layer may be simultaneously formed with theauxiliary wiring pattern 120, and may be directly connected to theauxiliary wiring pattern 120. The optional upper layer may be simultaneously formed with thefirst electrode 130. When the lower layer is directly connected to theauxiliary wiring pattern 120, the upper layer does not need to be directly connected to thefirst electrode 130. - Furthermore, the
second electrode pad 160 a may include a lower layer of the same material as theauxiliary wiring pattern 120 and an optional upper layer of the same material as thesecond electrode 160. While the lower layer may be simultaneously formed with theauxiliary wiring pattern 120, the upper layer may be simultaneously formed with thesecond electrode 160. - Referring to
FIG. 3 , it may be seen that, in the dummy area DA, a boundary surface between theadhesive layer 167 and thepassivation pattern 140 may be flat. The intrusion of external moisture into the OLED emission structure is mainly carried out along the boundary surface between theadhesive layer 167 and thepassivation pattern 140. When the moisture intrusion continues, contraction of cells of theOLED emission structure 150 may be generated and thus the life of an OLED panel may be shortened. Accordingly, the moisture intrusion needs to be delayed by increasing a moisture intrusion path to OLED emission structure. - When the boundary surface between the
adhesive layer 167 and thepassivation pattern 140 is flat as illustrated inFIG. 3 , the moisture intrusion may be delayed by increasing the width of the dummy area DA. However, increasing the width of the dummy area DA causes a decrease in the size of the array area AA. As a result, the size of an emission area is decreased. -
FIG. 4 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . - Referring to
FIG. 4 , it may be seen that, in the dummy area DA, thepassivation pattern 140 and theadhesive layer 167 contact each other. In particular, in the dummy area DA, thepassivation pattern 140 and theadhesive layer 167 have an uneven boundary surface corresponding to a three-dimensional (3D) structure. - In the dummy area DA, compared to a moisture intrusion path (arrow a of
FIG. 3 ) when thepassivation pattern 140 and theadhesive layer 167 have a flat boundary surface corresponding to a two-dimensional (2D) structure, a moisture intrusion path (arrow b ofFIG. 4 ) when thepassivation pattern 140 and theadhesive layer 167 have an uneven boundary surface is relatively increased. In the dummy area DA, the external moisture intrusion into theOLED emission structure 150 may be delayed through the uneven boundary surface between thepassivation pattern 140 and theadhesive layer 167. Accordingly, the emission characteristics degradation of theOLED emission structure 150 due to the external moisture intrusion may be prevented. As a result, the life characteristics of the OLED panel for a lighting device may be improved. - In the structure of
FIG. 4 , at least onedummy structure pattern 115 a is disposed in the dummy area DA of thesubstrate 110. Accordingly, a surface of thesubstrate 110 where thedummy structure pattern 115 a is disposed has an uneven structure. Accordingly, thepassivation pattern 140 in the dummy area DA formed by deposition may have an uneven surface corresponding to the surface of thesubstrate 110 where thedummy structure pattern 115 a is disposed. In other words, when thedummy structure pattern 115 a is provided in the dummy area DA of thesubstrate 110, theauxiliary wiring pattern 120, thefirst electrode 130, and thepassivation pattern 140 that are provided thereon by a deposition method may also have uneven surface corresponding to the surface of thesubstrate 110 where thedummy structure pattern 115 a is disposed. Accordingly, in the dummy area DA, the uneven boundary surface between thepassivation pattern 140 and theadhesive layer 167 may be formed. - Referring to
FIG. 4 , in the dummy area DA, thedummy structure pattern 115 a to form the uneven boundary surface between thepassivation pattern 140 and theadhesive layer 167 may be a light extraction pattern including a light extraction material. When thelight extraction pattern 115 is formed in the array area AA by an inkjet coating method to improve the light extraction efficiency, thelight extraction pattern 115 is further formed in the dummy area DA. Thelight extraction pattern 115 formed in the dummy area DA may become thedummy structure pattern 115 a for forming the uneven boundary surface between thepassivation pattern 140 and theadhesive layer 167. -
FIGS. 5 and 6 are schematic plan views illustrating examples of thedummy structure pattern 115 a. Thedummy structure pattern 115 a, as illustrated inFIG. 5 , may be arranged in the form of lines. Furthermore, thedummy structure pattern 115 a, as illustrated inFIG. 6 , may be arranged in the form of dots. -
FIG. 7 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . -
FIG. 7 illustrates adummy structure pattern 120 a in another shape. Thedummy structure pattern 120 a ofFIG. 7 may include the same material as theauxiliary wiring pattern 120, and may be formed simultaneously with theauxiliary wiring pattern 120. In the case of theauxiliary wiring pattern 120, metal is deposited in the entire area of thesubstrate 110, and a part of the pad area such as thesecond electrode pads 160 a and the emission area of the array area AA, is etched and thus theauxiliary wiring pattern 120 may be arranged in the entire area, except the etched areas. Alternatively, theauxiliary wiring pattern 120 may be arranged in the entire area of thesubstrate 110 except the emission area of the array area AA and the pad area by depositing metal in the entire area of thesubstrate 110 except a part of the pad area, and etching the emission area. In this state, when a part of theauxiliary wiring pattern 120 of the dummy area DA is etched, thedummy structure pattern 120 a for forming the uneven boundary surface between thepassivation pattern 140 and theadhesive layer 167 in the dummy area DA may be formed. - A moisture intrusion path (arrow b′ of
FIG. 7 ) illustrated inFIG. 7 may be relatively increased compared to the moisture intrusion path (arrow a ofFIG. 3 ) in which thepassivation pattern 140 and theadhesive layer 167 have a flat boundary surface in the dummy area DA. In addition, the moisture intrusion path (arrow b ofFIG. 4 ) illustrated inFIG. 4 and the moisture intrusion path (arrow b′ ofFIG. 7 ) illustrated inFIG. 7 may be almost similar to each other. The moisture intrusion paths inFIGS. 4 and 7 may be determined according to the number and height of dummy structure patterns. For example, when the number of dummy structure patterns is increased or the height of a dummy structure pattern is increased, the moisture intrusion path between thepassivation pattern 140 and theadhesive layer 167 in the dummy area DA may also be increased. - In
FIGS. 4 and 7 , the moisture intrusion path is increased as thepassivation pattern 140 and theadhesive layer 167 in the dummy area DA have an uneven boundary surface by using the dummy structure patterns (115 a ofFIGS. 4 and 120 a ofFIG. 7 ). -
FIG. 10 is a schematic plan view of an OLED panel for a lighting device according to an embodiment of the present disclosure.FIG. 11 is a cross-sectional view taken along line III-III′ ofFIG. 10 . - Alternatively, as shown in
FIGS. 10 and 11 another embodiment of the present application may increase another possible moisture intrusion path between thepassivation pattern 140 and a pad (such as thepad 160 a) in the pad area PA that have an uneven boundary surface therebetween by using similar dummy structure patterns. - More particularly, in this embodiment, an organic light-emitting diode panel for a lighting device is provided, wherein the organic light-emitting diode panel includes an array area having an emission area and a pad area disposed near the array area and comprises: a substrate; an auxiliary wiring pattern disposed on the substrate; a first electrode disposed on the substrate where the auxiliary wiring pattern is disposed; a passivation pattern disposed on the substrate where the first electrode is disposed; an organic light-emitting diode emission structure disposed on the substrate where the passivation pattern is disposed in the array area; a second electrode disposed on the substrate where the organic light-emitting diode emission structure is disposed; and a pad including the same material as the auxiliary wiring pattern that is disposed on the substrate in the pad area and contacts the passivation pattern; wherein the passivation pattern and the pad have an uneven boundary surface therebetween.
- Optionally, one or more dummy structure patterns are disposed in the pad, and the passivation pattern in the pad area has a surface in an uneven structure corresponding to a surface of the pad where the dummy structure pattern is disposed.
- For example, the dummy structure pattern may comprise a light extraction material. Preferably, a light extraction pattern made of the light extraction material is disposed under the auxiliary wiring pattern.
- Alternatively, the dummy structure pattern may comprise the same material as the auxiliary wiring pattern.
- Optionally, a capping layer is further disposed on the second electrode.
- Optionally, the auxiliary wiring pattern is formed of a material having resistance lower than that of the material of the first electrode.
- Optionally, the passivation pattern is formed at least in a part of the pad area and an area where the auxiliary wiring pattern is disposed.
- Optionally, the organic light-emitting diode panel may further comprise an encapsulation layer disposed on the adhesive layer.
- Optionally, the pad includes a first layer made of the same material as the auxiliary wiring pattern and an optional second layer disposed on the first layer and made of the same material as the first electrode.
-
FIG. 8 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . - As discussed above, in
FIGS. 4 and 7 , the moisture intrusion path is increased as thepassivation pattern 140 and theadhesive layer 167 in the dummy area DA have an uneven boundary surface by using the dummy structure patterns (115 a ofFIGS. 4 and 120 a ofFIG. 7 ). - In contrast, in an example illustrated in
FIG. 8 , agroove 145 penetrating through thepassivation pattern 140 may be provided at least in the dummy area DA, and theadhesive layer 167 is disposed not only above thepassivation pattern 140, but also in thegroove 145. A lower surface of theadhesive layer 167 may have a 3D structure in the dummy area DA due to thegroove 145. In such a structure, the moisture intrusion path may be increased like a moisture intrusion path (arrow c) illustrated in theFIG. 8 . Furthermore, thegroove 145 and thepassivation pattern 140 remaining between thegrooves 145 may act as barriers to the moisture intrusion. - The
groove 145 may additionally penetrate through thefirst electrode 130 disposed under thepassivation pattern 140 in the dummy area DA of thesubstrate 110. As illustrated inFIG. 8 , thegroove 145 may additionally penetrate through thefirst electrode 130 and theauxiliary wiring pattern 120 disposed in the dummy area DA of thesubstrate 110. Thegroove 145 that penetrates through not only thepassivation pattern 140, but also thefirst electrode 130 and theauxiliary wiring pattern 120, may have a depth deeper than the groove that penetrates through only thepassivation pattern 140, thereby further increasing the moisture intrusion path. - The
groove 145 illustrated inFIG. 8 may be formed by sequentially arranging theauxiliary wiring pattern 120, thefirst electrode 130, and thepassivation pattern 140 in the dummy area DA of thesubstrate 110, and then collectively etching the same. -
FIG. 9 is another example of a cross-sectional view taken along line II-II′ ofFIG. 1 . - In an example illustrated in
FIG. 9 , like the example ofFIG. 8 , the lower surface of theadhesive layer 167 has a 3D structure by agroove 145′. - However, while side walls of the
groove 145 ofFIG. 8 have a continuous shape, side walls of thegroove 145′ ofFIG. 9 have a step shape. In the case of thegroove 145′ ofFIG. 9 , after sequentially arranging theauxiliary wiring pattern 120, thefirst electrode 130, and thepassivation pattern 140 in the dummy area DA of thesubstrate 110, thepassivation pattern 140 is first etched, thefirst electrode 130 thereunder is subsequently etched, and then theauxiliary wiring pattern 120 is etched. - A moisture intrusion path (arrow c′) of
FIG. 9 seems to be increased longer than the moisture intrusion path (arrow c) ofFIG. 8 , and thus higher moisture intrusion delay effect may be obtained. - As described above, in the OLED panel for a lighting device according to the present disclosure, as illustrated in
FIGS. 4 and 7 , the dummy structure pattern (115 a ofFIGS. 4 and 120 a ofFIG. 7 ) is formed in the dummy area DA of the substrate, and thus the passivation pattern and the adhesive layer have an uneven boundary surface in the dummy area DA, or as illustrated inFIGS. 8 and 9 , the groove (145 ofFIG. 8 and 145 ′ ofFIG. 9 ) is formed in the dummy area DA of the substrate, and thus the lower surface of the adhesive layer has a 3D structure. Accordingly, the moisture intrusion path may be increased, and consequently the life characteristics of the OLED panel for a lighting device may be improved due to the moisture intrusion delay. - As described above, according to the present disclosure, the OLED panel for a lighting device according to the present disclosure may be easily manufactured to be large and surface emission may be possible. Thus, an expensive sapphire substrate for forming a nitride semiconductor light-emitting diode is not needed, and heat is not much generated compared to the nitride semiconductor light-emitting diode.
- In particular, in the OLED panel for a lighting device according to the present disclosure, since the passivation pattern and the adhesive layer are provided to have an uneven boundary surface therebetween in the dummy area, or the lower surface of the adhesive layer for bonding the encapsulation layer is provided in a 3D structure, the moisture intrusion path may be increased, and a barrier to the moisture intrusion can be provided. Accordingly, the OLED panel for a lighting device according to the present disclosure may prevent degradation of an OLED emission structure due to the external moisture intrusion, and may improve life characteristics.
- The present disclosure described above may be variously substituted, altered, and modified by those skilled in the art to which the present inventive concept pertains without departing from the scope and sprit of the present disclosure. Therefore, the present disclosure is not limited to the above-mentioned exemplary embodiments and the accompanying drawings.
- The various embodiments described above can be combined to provide further embodiments. These and other changes can be made to the embodiments in light of the above-detailed description. In general, in the following claims, the terms used should not be construed to limit the claims to the specific embodiments disclosed in the specification and the claims, but should be construed to include all possible embodiments along with the full scope of equivalents to which such claims are entitled. Accordingly, the claims are not limited by the disclosure.
Claims (17)
1. An organic light-emitting diode panel for a lighting device, the organic light-emitting diode panel comprising:
a substrate including an array area having an emission area, and including a dummy area disposed outside the array area;
an auxiliary wiring pattern disposed on the substrate;
a first electrode disposed on the substrate where the auxiliary wiring pattern is disposed;
a passivation pattern disposed on the substrate where the first electrode is disposed, and surrounding on at least four sides the auxiliary wiring pattern and the first electrode in the dummy area;
an organic light-emitting diode emission structure disposed on the substrate where the passivation pattern is disposed in the array area;
a second electrode disposed on the substrate where the organic light-emitting diode emission structure is disposed; an adhesive layer disposed on the substrate where the second electrode is disposed and contacting the passivation pattern in the dummy area, a lower surface of the adhesive layer having a three-dimensional structure in the dummy area; and
at least one groove that penetrates through the passivation pattern disposed in the dummy area of the substrate,
wherein a part of the adhesive layer is disposed in the at least one groove.
2. The organic light-emitting diode panel for the lighting device of claim 1 , wherein each of the at least one groove further penetrates through the first electrode disposed in the dummy area of the substrate or further penetrates through the first electrode and the auxiliary wiring pattern disposed in the dummy area of the substrate.
3. The organic light-emitting diode panel for the lighting device of claim 2 , wherein a side wall of the at least one groove has a step shape.
4. The organic light-emitting diode panel for the lighting device of claim 1 , wherein a capping layer is on the second electrode.
5. The organic light-emitting diode panel for the lighting device of claim 1 , wherein the auxiliary wiring pattern is a material having resistance lower than a resistance of a material of the first electrode.
6. The organic light-emitting diode panel for the lighting device of claim 1 , wherein the passivation pattern is at least in an area where the auxiliary wiring pattern is disposed.
7. The organic light-emitting diode panel for the lighting device of claim 1 , further comprising an encapsulation layer disposed on the adhesive layer.
8. An organic light-emitting diode panel for a lighting device, the organic light-emitting diode panel comprising:
a substrate including an array area and a pad area disposed near the array area;
an auxiliary wiring pattern disposed on the substrate;
a first electrode disposed on the substrate where the auxiliary wiring pattern is disposed;
a passivation pattern disposed on the substrate where the first electrode is disposed;
an organic light-emitting diode emission structure disposed on the substrate where the passivation pattern is disposed in the array area;
a second electrode disposed on the substrate where the organic light-emitting diode emission structure is disposed; and
a pad including a same material as a material of the auxiliary wiring pattern, the pad disposed on the substrate in the pad area and in contact with the passivation pattern, wherein the passivation pattern and the pad have an uneven boundary surface therebetween.
9. The organic light-emitting diode panel for the lighting device of claim 8 , wherein one or more dummy structure patterns are disposed in the pad, and wherein the passivation pattern in the pad area has a surface with an uneven structure corresponding to a surface of the pad having an uneven structure where the dummy structure pattern is disposed.
10. The organic light-emitting diode panel for the lighting device of claim 9 , wherein the dummy structure pattern comprises a light extraction material.
11. The organic light-emitting diode panel for the lighting device of claim 10 , wherein in the array area of the substrate, a light extraction pattern made of the light extraction material is disposed under the auxiliary wiring pattern.
12. The organic light-emitting diode panel for the lighting device of claim 9 , wherein the dummy structure pattern comprises a same material as a material of the auxiliary wiring pattern.
13. The organic light-emitting diode panel for the lighting device of claim 8 , wherein a capping layer is further disposed on the second electrode.
14. The organic light-emitting diode panel for the lighting device of claim 8 , wherein the auxiliary wiring pattern is a material having resistance that is lower than a resistance of a material of the first electrode.
15. The organic light-emitting diode panel for the lighting device of claim 10 , wherein the passivation pattern is at least in an area where the auxiliary wiring pattern is disposed and a part of the pad area.
16. The organic light-emitting diode panel for the lighting device of claim 8 , further comprising an encapsulation layer disposed on the adhesive layer.
17. The organic light-emitting diode panel for the lighting device of claim 8 , wherein the pad includes a first layer made of a same material as a material of the auxiliary wiring pattern and a second layer disposed on the first layer and made of a same material as a material of the first electrode.