Prior art keywords
coal
charge
mixture
waste
reducing agent
Prior art date
Application number
UAA201305534A
Other languages
Russian (ru)
Ukrainian (uk)
Inventor
Yurii Vasyliovych Filatov
Heorhii Vasyliovych Dolhariev
Serhii Arkadiiovych Mediantsev
Viktor Ivanovych Chalenko
Original Assignee
Do Metallurg Plant Cjs Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Do Metallurg Plant Cjs Co filed Critical Do Metallurg Plant Cjs Co
Priority to UAA201305534A priority Critical patent/UA107862C2/en
Publication of UA107862C2 publication Critical patent/UA107862C2/en

Links

Landscapes

  • Coke Industry (AREA)

Abstract

Винахід належить до коксохімічного виробництва, а саме до термічної переробки вугілля та перезбагачених відходів вуглезбагачення у високореакційний вуглецевий відновник, і може бути використаний у феросплавному виробництві для отримання феросплавів. Спосіб отримання високореакційного вуглецевого відновника включає складання шихти з дрібного газового вугілля і відходів вуглезбагачення, змішування шихти та коксування її у печах. Винахід характеризується тим, що як дрібне газове вугілля беруть малометаморфізоване газове вугілля крупністю менше , в кількості 75-98 % від загальної кількості шихти, а як відходи вуглезбагачення - перезбагачені відходи вуглезбагачення в кількості 2-25 % від загальної кількості шихти, при цьому вміст в шихті Fe+Ca повинен бути не менше 0,8 %, а шихту, після змішування, термічно обробляють інертним теплоносієм до температури 180-220 °С. Винахід забезпечує отримання високоякісного вуглецевого відновника із слабоспікливого вугілля та тонкодисперсних перезбагачених відходів вуглезбагачення, підвищення спікливості, зниження собівартості.The invention relates to coke production, namely, the thermal processing of coal and enriched coal wastes into a highly reactive carbon reducing agent, and can be used in ferroalloy production to produce ferroalloys. A method of producing a highly reactive carbon reducing agent involves assembling a mixture of fine gas coal and coal waste, mixing the mixture and coking it in furnaces. The invention is characterized by the fact that as small gas coal take low-metamorphosed gas coal with a size smaller than 75-98% of the total amount of charge, and as a waste of coal enrichment waste coal enrichment in the amount of 2-25% of the total amount of charge, with the content in the charge of Fe + Ca should be at least 0.8%, and the mixture, after mixing, is thermally treated with an inert coolant to a temperature of 180-220 ° C. EFFECT: invention provides obtaining high-quality carbon reducing agent from low-carbon coal and finely dispersed coal-rich wastes, increasing spiciness, reducing cost.

UAA201305534A 2013-04-29 2013-04-29 Method of obtaining high correction carbon UA107862C2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
UAA201305534A UA107862C2 (en) 2013-04-29 2013-04-29 Method of obtaining high correction carbon

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
UAA201305534A UA107862C2 (en) 2013-04-29 2013-04-29 Method of obtaining high correction carbon

Publications (1)

Publication Number Publication Date
UA107862C2 true UA107862C2 (en) 2015-02-25

Family

ID=52989845

Family Applications (1)

Application Number Title Priority Date Filing Date
UAA201305534A UA107862C2 (en) 2013-04-29 2013-04-29 Method of obtaining high correction carbon

Country Status (1)

Country Link
UA (1) UA107862C2 (en)

Similar Documents

Publication Publication Date Title
RU2013155041A (en) SYSTEM AND METHOD FOR REDUCING IRON OXIDE TO METAL IRON WITH APPLICATION OF COKE GAS AND STEEL-OXYGEN FUEL GAS
MX2016009779A (en) Plasma reactor.
UA100095C2 (en) Method for producing of metalic iron
PH12014501497B1 (en) Cement composition production method
AR092164A1 (en) METHOD FOR REDUCING OXIDE FROM IRON TO METAL IRON WITH THE USE OF COOK OVEN GAS AND GAS OVEN FROM OXYGEN SIDERURGICO
MX2016006560A (en) Method for generating synthesis gas in conjunction with a smelting works.
EA201101157A1 (en) METHOD AND INSTALLATION FOR CHARGE OF COAL IN AN INERT AND NON-INTERACT MEDIUM
IN2015DN02331A (en)
IN2013MU02988A (en)
MX2014005335A (en) Method for operating an arc furnace.
FR2968676B1 (en) PROCESS FOR INTRODUCING NANOCHARGES OF CARBONIC ORIGIN IN A METAL OR ALLOY
MX2016007469A (en) Molten iron manufacturing method and molten iron manufacturing apparatus.
WO2018128682A3 (en) Direct reduction with coal gasification and coke oven gas
UA107862C2 (en) Method of obtaining high correction carbon
RU2011102063A (en) METHOD FOR PREPARING COAL MINING FOR PRODUCING METALLURGICAL COKE
AR089099A1 (en) A SUSTAINABLE PROCESS FOR THE CO-GENERATION OF ARRABIO AND ELECTRICAL ENERGY USING WOOD AS FUEL
WO2016140428A8 (en) Coal briquettes, method and apparatus for manufacturing the same, and method and apparatus for manufacturing molten iron
EA201700186A1 (en) METHOD OF OBTAINING COKE
IN2014KN01261A (en)
MY174695A (en) Method and apparatus for sequestering carbon dioxide from a spent gas
UA116350C2 (en) Method and system for increasing the calorific value of a material flow containing carbon
BR112014019705A8 (en) METHOD, DEVICE AND USE OF DEVICE TO REDUCE RAW MATERIALS CONTAINING IRON OXIDE
UA100025U (en) Thermal conversion method of solid fuel
RU2012128262A (en) METHOD FOR BRIQUETTING IRON-CONTAINING WASTE AS SCALE
Inoue et al. Influence of combined water in coal on pre-reduction of iron oxide with coal carbonization gas in low, middle and high volatile matter coal