TWI450431B - - Google Patents
Info
- Publication number
- TWI450431B TWI450431B TW102114384A TW102114384A TWI450431B TW I450431 B TWI450431 B TW I450431B TW 102114384 A TW102114384 A TW 102114384A TW 102114384 A TW102114384 A TW 102114384A TW I450431 B TWI450431 B TW I450431B
- Authority
- TW
- Taiwan
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| TW102114384A TW201349633A (zh) | 2013-04-23 | 2013-04-23 | 鋰離子電池、其陰極、其陰極材料及該陰極材料之製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| TW102114384A TW201349633A (zh) | 2013-04-23 | 2013-04-23 | 鋰離子電池、其陰極、其陰極材料及該陰極材料之製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| TW201349633A TW201349633A (zh) | 2013-12-01 |
| TWI450431B true TWI450431B (enExample) | 2014-08-21 |
Family
ID=50157577
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| TW102114384A TW201349633A (zh) | 2013-04-23 | 2013-04-23 | 鋰離子電池、其陰極、其陰極材料及該陰極材料之製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| TW (1) | TW201349633A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| TWI499117B (zh) * | 2014-05-06 | 2015-09-01 | Univ Nat Cheng Kung | 適用鋰電池陰極材料之含矽雙相粉末及其製造方法 |
| CN105226265B (zh) * | 2014-06-20 | 2018-01-19 | 吕传盛 | 适用锂电池阴极材料的含硅双相粉末及其制造方法 |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN101569051B (zh) * | 2007-08-09 | 2012-02-01 | 松下电器产业株式会社 | 非水电解质二次电池及其制造方法 |
| TW201246656A (en) * | 2011-03-31 | 2012-11-16 | Daikin Ind Ltd | Lithium ion secondary battery and nonaqueous electrolyte for lithium ion secondary battery |
| TW201308732A (zh) * | 2011-03-30 | 2013-02-16 | Toda Kogyo Corp | 正極活性物質粒子粉末及其製造方法,以及非水電解質蓄電池 |
-
2013
- 2013-04-23 TW TW102114384A patent/TW201349633A/zh not_active IP Right Cessation
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN101569051B (zh) * | 2007-08-09 | 2012-02-01 | 松下电器产业株式会社 | 非水电解质二次电池及其制造方法 |
| TW201308732A (zh) * | 2011-03-30 | 2013-02-16 | Toda Kogyo Corp | 正極活性物質粒子粉末及其製造方法,以及非水電解質蓄電池 |
| TW201246656A (en) * | 2011-03-31 | 2012-11-16 | Daikin Ind Ltd | Lithium ion secondary battery and nonaqueous electrolyte for lithium ion secondary battery |
Also Published As
| Publication number | Publication date |
|---|---|
| TW201349633A (zh) | 2013-12-01 |