TW500602B - Method for integrally producing shoes - Google Patents

Method for integrally producing shoes Download PDF

Info

Publication number
TW500602B
TW500602B TW89119648A TW89119648A TW500602B TW 500602 B TW500602 B TW 500602B TW 89119648 A TW89119648 A TW 89119648A TW 89119648 A TW89119648 A TW 89119648A TW 500602 B TW500602 B TW 500602B
Authority
TW
Taiwan
Prior art keywords
eva
formula
midsole
foamed
mixing
Prior art date
Application number
TW89119648A
Other languages
Chinese (zh)
Inventor
You-Yang Su
Original Assignee
You-Yang Su
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by You-Yang Su filed Critical You-Yang Su
Priority to TW89119648A priority Critical patent/TW500602B/en
Application granted granted Critical
Publication of TW500602B publication Critical patent/TW500602B/en

Abstract

The present invention relates to a method for integrally producing shoes, which comprises: using a blender to blend EVA plastic particle and a pigment to form a mixture for producing an insole formulation material; using a blender to blend EVA plastic particles and a pigment for producing a shoesole formulation material; after putting the insole formulation material on top of the shoesole formulation material, using a hydraulic press and a hydraulic press mold to foam the upper insole material and lower shoesole material of EVA foam plate; using a press mold to press and cool the foamed EVA foam plate for forming. The invented method uses the thermal plastic property of an EVA foam plate, after the foaming by a hydraulic press, using the foaming temperature for direct pressing and cooling for forming, and then forming a product after edge trimming. The present invention has the advantages of conspicuously shortening the production process, reducing the time and cost of process, and having a better outlook and durability.

Description

500602 A7 五、發明說明( 本發明為一種鞋台一體成型之製法,本發明主要係且 有可以明顯縮短製程,以節省加工時間與成本,= 為美觀與耐用的優點。 ^ 按,「鞋台」係為於鞋子上不可或缺的元件之一,而 「鞋台」係具有中底與大底,大底.可與地面或地板接觸, 中底可與人們的腳部接觸,以使鞋台供人們方便於走路或 跑步之用,故鞋台對於人們的日常生活之間係為相當重要 的物品之一。 /以-般傳統式習用的鞋台製法而論(如第五圖中所 示),、,其係以EVA發泡板的中底與EVA發泡板的大底分 別製造,經加工後,再分別予以膠合成型,其各別的製程 如下: (1) · EVA中底製程: 經濟部智慧財產局員工消費合作社印製500602 A7 V. Description of the invention (The present invention is a method for integrally forming a shoe table. The present invention is mainly and has the advantages of significantly shortening the manufacturing process to save processing time and cost, and has the advantages of beauty and durability. ^ Press, "Shoe table "It is one of the indispensable elements on shoes, and" shoe table "has a midsole and an outsole. The outsole can be in contact with the ground or floor, and the midsole can be in contact with people's feet to make shoes The platform is for people to easily walk or run, so the shoe platform is one of the most important items in people's daily life. / Based on the traditional traditional shoe platform manufacturing method (as shown in Figure 5) (Shown) ,,, it is made of the EVA foam board midsole and the EVA foam board outsole separately, after processing, and then plasticized separately, the respective manufacturing process is as follows: (1) · EVA midsole Process: Printed by the Consumer Cooperative of the Intellectual Property Bureau of the Ministry of Economic Affairs

第一步驟為EVA膠料/色料(中底配方藥品)_第 一步驟為係以混煉機混煉成為EVA中底配方料(將eva 膠粒與藥品、色料一起混煉)—第三步驟為以油壓機予以 冷卻(予以加溫發泡為EVA中底發泡板)—第四步驟為 剖皮機將EVA中底發泡板先剖皮後再剖成所需厚度—第 五步驟為裁斷機將剖好厚度的EVA中底發泡體裁成所需 的形體—第六步驟再以加溫箱將裁斷好的EVA中底發泡 體予以加溫軟化—第七步驟再以壓模機將軟化後的EVA 中底予以壓模冷卻成型—第八步驟再以裁斷機將壓模後的 EVA中底予以裁斷沖孔。 ⑵· EVA大底製程:(如第六圖中所示) 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公爱)The first step is EVA compound / colorant (medium bottom formula drug) _The first step is to use a kneader to mix into an EVA midsole formula (mix eva rubber particles with drugs and colorant) —the first The third step is to cool with an oil hydraulic machine (to be heated and foamed into an EVA midsole foamed board)-the fourth step is to use a skinning machine to peel the EVA midsole foamed board to the required thickness-the fifth step Cut the cut EVA midsole foam into the desired shape for the cutting machine—the sixth step is to use a heating box to heat and soften the cut EVA midsole foam—the seventh step is to use a compression mold The softened EVA midsole is die-formed for cooling and molding-in the eighth step, the die-cut EVA midsole is cut and punched by a cutting machine. ⑵ · EVA outsole manufacturing process: (as shown in Figure 6) This paper size applies to China National Standard (CNS) A4 (210 X 297 public love)

五、發明說明(2 ) 經濟部智慧財產局員工消費合作社印製 以EVA大底配方藥品與EVA膠粒/色料依EVA中 底製程的第一步驟至第五步驟裁斷後,大底與壓模裁斷 EVA中底後’再予以膠合成型,習用製程係需要有1 3 個步驟,故有著製程較多且較為繁瑣的缺點。 本發明人有鐘於現有鞋底之製法於設計上未盡精良, 乃積極進行研究改良’經不斷的嚐試與試驗後,終於發展 出確具實用性功效之本發明。 本發明之主要目的在於提供一種鞋台一體成型之製 法’係以EVA膠粒與色料經混煉機混煉成中底配方料, 同時將EVA膠粒與色科經混煉機混煉成大底配方料,將 中底配方料疊置於大底配方料上,再經油壓機及油壓機模 具予以發泡為上層中底料、下層大底料i EVA發泡板, 再經壓模機將發泡完成之EVA發泡板壓模冷卻成型,同 時經裁邊即可成為成品,本發明之製法係利用EVA發泡 板之熱塑性於油壓機發泡後,以發泡溫度直接予以壓模冷 卻成型’本發明具有明顯可以縮短製程且可一體成型,以 節省加工時間與成本,.亦有較為美觀與耐用的優點。 為使 貴審查委員進一步瞭解前述目的及本發 明之製法特徵,茲附以圖式詳細說明如后: (一)圖式部分·· 第一圖:係本發明之流程圖。 第二圖:係本發明之鞋台於油壓機部份的製程 圖。 第三曜:係本發明之鞋台於壓模機部份的製程 (請先閱讀背面之注意事項再填寫本頁) ▼裝 訂ί ! 線_ 泰紙張尺度國國家標準(CNS)A4規格(210 X 297公釐Γ Α7 Β7 五、 發明說明(3V. Description of the invention (2) The EVA outsole formula drug and EVA pellets / colorants are printed by the Consumer Cooperatives of the Intellectual Property Bureau of the Ministry of Economic Affairs according to the first to fifth steps of the EVA midsole process. After the die cuts the EVA midsole, it is then glue-composited. The conventional manufacturing process requires 13 steps, so it has the disadvantages of more and more complicated processes. The present inventor has developed a method for making existing soles, which is not perfect in design, but has actively researched and improved it. 'After continuous trials and tests, the invention has finally been developed with practical utility. The main purpose of the present invention is to provide a method for forming a shoe table in a single piece. The system uses EVA rubber particles and color materials to be mixed into a midsole formula, and at the same time, EVA rubber particles and Color Division are mixed into For the outsole formula, the midsole formula is stacked on the outsole formula, and then foamed by the hydraulic press and the mold of the hydraulic press into the upper middle sole and the lower bottom iEVA foam board. The foamed EVA foam sheet is cooled and formed into a mold, and at the same time, it can be finished by trimming. The manufacturing method of the present invention is to use the thermoplasticity of the EVA foam sheet to foam the oil press, and then directly cool the mold with the foaming temperature. 'The invention has the advantages of significantly shortening the manufacturing process and being integrally formed to save processing time and cost, and also has the advantages of being more beautiful and durable. In order to make your reviewing committee better understand the aforementioned purpose and the characteristics of the manufacturing method of the present invention, detailed drawings are attached as follows: (1) Schematic part ... The first figure: is a flowchart of the present invention. The second figure is a process drawing of the shoe table of the present invention on a hydraulic press. Third 曜: It is the manufacturing process of the shoe table of the present invention on the stamping machine (please read the precautions on the back before filling this page) ▼ Binding!! Thread _ Thai Paper Scale National Standard (CNS) A4 Specification (210 X 297mm Γ Α7 Β7 V. Description of the invention (3

Ms 弟四 第五 第六 圖 圖 圖 ) 0 1 0 2 0 圖。 係以本發明製成之鞋台的立體圖 係習用之中底製法的流程圖。 係習用之大底製法的流程圖。 圖號部分: - )EVA膠粒與色料 )中底配方料 )上層中底料 )EVA膠粒與色料 )大底配方料· )下層大底料 )以壓模機將發泡完成之EVa 广 从,〇傲/尖^ 冷部成型,並同時錄《縣、息如1 于左裁邊即可成為成品 發泡板壓模 <請先閱讀背面之注意事項再填寫本頁) .裝 訂*丨Ms brother 4th 5th 6th photo (photo) 0 1 0 2 0 photo. This is a perspective view of a shoe table made with the present invention. It is a flowchart of a conventional midsole manufacturing method. This is a flowchart of the conventional outsole method. Drawing number part:-) EVA pellets and pigments) Midsole formula) Upper midsole) EVA pellets and pigment) Outsole formula ·) Lower bottom material) The foaming is completed with a compression molding machine EVa Guangcong, 〇 proud / sharp ^ cold section molding, and also recorded "county, interest such as 1 on the left cutting edge can become the finished foam board stamper < please read the precautions on the back before filling this page). Binding * 丨

ϋ n ϋ t— n I 經濟部智慧財產局員工消費合作社印制农 c第-圖所示,本發明係為一種鞋台一 製法,包括有下列各步驟: 卜步驟HEVA膠粒與色料(1〇)(中底配 f樂品)經第二步驟中的混煉機混煉成中底配方料(i ),其係為混煉加溫成為㈣狀態(將—A膠粒藥品 色-料一起混煉); 古从第,步驟:係將EVA膠粒與色料(20)(大底配 樂品四步财的混煉機混煉成大底配方料(2 1) ’其係為混煉加溫成騎融狀態(將eva膠粒 5 DUU0U2ϋ n ϋ t— n I As shown in the first figure of the printed agricultural product of the Consumer Cooperative of the Intellectual Property Bureau of the Ministry of Economic Affairs, the present invention is a method for manufacturing a shoe table, which includes the following steps: Step HEVA rubber particles and pigment ( 1〇) (Midsole with f music) is mixed into the midsole formula (i) by the kneader in the second step, which is kneaded and heated to a simmer state (will be -A rubber particle drug color- The materials are mixed together); Gu Congdi, step: the EVA rubber particles and the coloring material (20) (the four-step mixing machine of the outsole music product) are mixed into the outsole formula (2 1) 'It is Kneading and heating into a molten state (the eva rubber particles 5 DUU0U2

發明說明(4 一起混煉); 將中底配方料(11)叠置於大底配方料(21)上 方(如第一、二圖中所示); 第五步驟係經油壓機及油壓機模具予以加溫發泡為上 層中底料(12)、下層大底料(22)之EVA發泡板 (兩種料刀上層T層-起放入油壓機),其中發泡板於 壓模機壓模冷卻成型所需的時間約需3分鐘,溫度約為i 4 5 C至1 6 5。(:之間,壓力係為丄5 〇Kg/cm2; 本發明之申請重點在於:第六步驟以壓模機將發泡完 成之爾發泡板_冷卻成型(如第―、三圖中所示) 並同時經裁邊後即可成為成品(30)(如第-、四圖中 所示)。 前述之EVA於常溫為固態,熔點約8 5至9 (TC, 因此需於高溫、高麼下予以發泡架橋,屬於直接發泡,JL 發泡尺寸依其發泡倍數與模具尺寸而定。(例如:模具^ :為1 0 0cmx5 〇cmx2cm’而發泡倍數為2倍 板尺寸W〇〇cmX10〇cmX4cm,以此類 故於本發明中的製法係為利用EVA發泡板之敎塑性 於油屢機發泡之後,以其發泡完成時之溫度(約U = 未經冷卻,.直接利用其溫度予以屋 時經裁邊後即可成為鞋台成品,該鞋台係為具有上 ^個ί與下制大底跳發㈣,故於本發明中只需 要6個製程而已,遠比習用者需要13個製程可以明顯^ 氏張尺度適財_家標準(CNS)A4規袼(_£〇 X 297公爱) {請先閱讀背面之注意事項再填寫本頁) * n II ϋ f» n ϋ <Description of the invention (4 Mixing together); Putting the midsole formula (11) on top of the big bottom formula (21) (as shown in the first and second figures); The fifth step is through the hydraulic press and the hydraulic press mold. EVA foamed board with warming and foaming as the middle layer of the upper layer (12) and the bottom layer of the upper layer (22) The time required for cooling molding is about 3 minutes, and the temperature is about i 4 5 C to 1 65. (Between, the pressure is K50 Kg / cm2; the application of the present invention focuses on: the sixth step is to use a compression molding machine to complete the foamed Seoul foam board_cooling molding (as shown in Figures ―3) (Shown) and trimmed at the same time can become the finished product (30) (as shown in Figures-4). The aforementioned EVA is solid at room temperature and has a melting point of about 8 5 to 9 (TC, so it needs to be at high temperature, high temperature The foam bridge is directly foamed. The size of JL foam depends on its foaming factor and mold size. (For example: mold ^: 100 cm x 50 cm x 2 cm 'and foaming factor is 2 times the board size W 〇〇cmX10〇cmX4cm, so the manufacturing method in the present invention is to use the plasticity of EVA foam board after the oil is repeatedly foamed at the temperature at which the foaming is completed (about U = without cooling, .Using its temperature directly to make a finished shoe platform after trimming the house. The shoe platform has upper and lower outsole hair buns, so only 6 processes are needed in the present invention. Far more than 13 processes required by the user can be significantly ^ Zhang Zhang scales suitable financial _ house standard (CNS) A4 regulations (_ £ 〇X 297 公 爱) {Please read first Read the notes on the back and fill out this page) * n II ϋ f »n ϋ <

If — . -I I ί - 500602 A7 B7 五、發明說明(女) 予以縮短,故本發明具有可以一體成型以明顯縮短製程, 以節省加工時間與成本,並具有較為美觀與耐用的優點, 同時對於不同密度與不同顏色的中底、大底皆可適用。 因此,經由以上之說明可知,本發明以優異之結構配 置下,至少具有如后的優點: . 可縮短製程:於本發明中所需的製程僅需要6個步驟 而已1雨習用者卻需要13個步驟的製程,故本發明與習 用者相較,本發明具有可明顯縮短製程,並有著可節省加 工時間與成本的優點0 綜上所述,當知本發明具有實用性與創作性,且本 明於申請前並未有已見於任何刊物及公開使用之情事,二 符合專利法第十九條及第二十條之規定1依法具文提: 申請0If —. -II ί-500602 A7 B7 5. The description of the invention (female) is shortened, so the invention can be integrally molded to significantly shorten the manufacturing process, to save processing time and cost, and has the advantages of beautiful appearance and durability. Different densities and different colors of midsole and outsole are applicable. Therefore, from the above description, it can be known that the present invention has at least the following advantages under the excellent structural configuration:. The process can be shortened: The process required in the present invention only needs 6 steps, but the user needs 13 Compared with the user, the invention has the advantages of significantly shortening the manufacturing process, and has the advantages of saving processing time and cost. In summary, when the invention is practical and creative, and Before the application, this application has not been seen in any publications and public use. Secondly, it complies with the provisions of Articles 19 and 20 of the Patent Law.

III ^ -·裝·丨 (請先閱讀背面之注意事項再填寫本頁) n / n n K j 訂ί I 經濟部智慧財產局員Η消費合作社印製III ^-· 装 · 丨 (Please read the notes on the back before filling out this page) n / n n K j Order I Printed by the Intellectual Property Bureau of the Ministry of Economic Affairs and printed by Consumer Cooperatives

本紙張尺度適用中國國家標準(CNS)A4規格(21〇 x 297公釐) 奏This paper size applies to China National Standard (CNS) A4 (21 × 297 mm)

Claims (1)

i 500602 _ SI I————W———________________________________________________________________________________________________丨..丨丨丨丨 六、申請專利範圍 ^ · 一種鞋台一體成型之製法,包括有下列各步驟: 第一步驟:係以EVA膠粒與色料(中底配方藥品);第 二步驟:經混煉機混煉成中底配方料(將EVA膠粒藥品 色枓一起混煉);第三步驟··將EVA膠粒與色料(大底 配方藥品);第四步驟:經混煉機混煉成大底配方料(將 EVA膠粒藥品色料一起混煉);第五步驟:將中底配方 料唛置於大底配方料上,再經油履機及油壓機模具予以發 泡為上層中底料、下層大底料之EVA發泡板;其特徵在 於: 第六步驟:經壓模機將發泡完成之EVA發泡板壓模 冷卻成型並同時經裁邊即可成為成品。 2·如申請專利範圍第1項所述鞋台一體成型之製 法,其中發泡板於壓模機壓模冷卻成型所需的時間约3分 4里,溫度約為1 4 5 °C至1 6 5。(:之間,壓力為1 5 0 Kg/cm2 ° (請先閱讀背面之注意事項再填寫本頁) II ϋ n 如-eJ* cl ϋ n n >i € 經濟部智慧財產局員Η消費合作社印製 8 本紙張尺度適用中國國家標準(CNS)A4規袼(210 X 297公釐)i 500602 _ SI I ———— W ————________________________________________________________________________________________________ 丨 .. 丨 丨 丨 丨 Ⅵ. Patent application scope ^ · A manufacturing method of shoe table integrated molding, including the following steps: First step: EVA Rubber granules and pigments (medium bottom formula drugs); the second step: mixing with a kneader into a midsole formula (mixing the EVA rubber granules and drug colors together); the third step ·· the EVA rubber granules and Coloring material (outsole formula drug); The fourth step: mixing into a large-bottom formula through a kneader (mixing the EVA rubber granule drug color material together); the fifth step: placing the midsole formula in a large On the bottom formula, it is then foamed into the upper middle bottom material and the lower big bottom material by the oil track machine and hydraulic press mold. The EVA foam board is characterized by: The sixth step: the foamed EVA is passed through the compression molding machine. The foamed board compression mold can be cooled to form a finished product and can be trimmed at the same time. 2. According to the manufacturing method of integrated shoe table as described in item 1 of the scope of patent application, wherein the time required for the foam board to cool and form on the compression mold is about 3 minutes and 4 miles, and the temperature is about 1 4 5 ° C to 1 6 5. (: In between, the pressure is 150 Kg / cm2 ° (Please read the precautions on the back before filling this page) II ϋ n If -eJ * cl ϋ nn > i € Printed by a member of the Intellectual Property Bureau of the Ministry of Economic Affairs Η Consumer Cooperative 8 This paper size applies to China National Standard (CNS) A4 (210 X 297 mm)
TW89119648A 2000-09-22 2000-09-22 Method for integrally producing shoes TW500602B (en)