TW305908B - Manufacturing method for stainless trowel - Google Patents

Manufacturing method for stainless trowel Download PDF

Info

Publication number
TW305908B
TW305908B TW85110825A TW85110825A TW305908B TW 305908 B TW305908 B TW 305908B TW 85110825 A TW85110825 A TW 85110825A TW 85110825 A TW85110825 A TW 85110825A TW 305908 B TW305908 B TW 305908B
Authority
TW
Taiwan
Prior art keywords
polishing
trapezoidal plate
procedure
plate body
make
Prior art date
Application number
TW85110825A
Other languages
Chinese (zh)
Inventor
Jau-Jiunn Sheu
Original Assignee
Jau-Jiunn Sheu
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jau-Jiunn Sheu filed Critical Jau-Jiunn Sheu
Priority to TW85110825A priority Critical patent/TW305908B/en
Application granted granted Critical
Publication of TW305908B publication Critical patent/TW305908B/en

Abstract

A manufacturing method for stainless trowel using white iron with stainless as material having the following steps: cutting the material into a trapezoid plate with front end an arch shape, punching the rear bottom side to make the hole protrude through the top side and punching several triangle outlets with appropriate slope at the hole rim of the bottom side; striking the protruding part from the top side to make it protrude through the bottom side, heating at 58 to 60 Centigrade degrees to form wave shape, water polishing the top side and the bottom side of the trapezoid plate,2nd polishing the top side using black jack, 3rd and 4th polishing the top side, inserting a connection rod into the hole and riveting it, thus making a little bit grinding effect to the protruding part on the top side, heating it at 800 Centigrade degree, striking the riveting part to make it flat and smooth, setting a wood handle on the connection rod, 2nd polishing the bottom side using black jack, 3rd and 4th polishing the bottom side and thus obtain the desired trowel.

Description

經濟部中央揲率局工消费合作社印装 305908 A7 B7 五、發明説明(1 ) 一種不銹鋼抹刀之製造方法,主要包’含下列之程序: 裁切程序、打孔程序、熱處理程序、研磨程序、頂面二次 研磨程序、頂面拋光程序、鉚結連接桿並加木柄程序、底 面二次研磨程序、底面拋光程序,尤指藉由上述方法製造 之抹刀,具高跗磨性且不易生銹,另使用較為滑順,俥達 使用壽命延長及使用效率提高者。 〈產業上利用範圍&gt; 本發明係主要以一加工製造方法,製造出高耐磨性且 不易生銹之不銹鋼抹刀,而得以延長其使用壽命,另可於 使用抹平水泥時較為滑順,以得到較佳之使用效率者。 &lt;發明背景&gt; 按目前一般抹刀之製造方法(_參閲第-圖習用方法 之方塊流程圖),像以綑料之S K - 5鋼板為材料(因其含硪 成分低,故其密度較稀疏硬度較薄弱,恰可供習甩方法製 造之),其主要包含下列之程序: 裁切程序:先裁切成適當大小之提方狀板體,再將長 方狀板體之前端裁切成弧尖狀; 研磨程序:於良方狀板體之頂面及反ig進行水磨加工 打孔程序:於艮方狀板體頂面後段適當位置上打孔, 使孔緣往底面凸出,並於頂面孔緣打出適當斜度及打出複 數之三角狀缺口; 頂面二次研磨程序:於畏方狀板體頂面以黑石進行二 次研磨; 本纸張尺度逋用中國家樣率(CNS &gt; A4规格(210 X 297公釐) 83. 3.10,000 3 ---------^ II - (請先閱讀背面之注fvf袄寫本頁) 訂 線 2 /V 明説 明發Printed and printed by 305908 A7 B7 of the Industrial and Consumer Cooperative of the Central Bureau of Economic Affairs of the Ministry of Economic Affairs 5. Description of invention (1) A manufacturing method of stainless steel spatula, mainly including the following procedures: cutting procedures, punching procedures, heat treatment procedures, grinding procedures , Top surface secondary grinding procedure, top surface polishing procedure, riveting connecting rod with wooden handle, bottom surface secondary grinding procedure, bottom surface polishing procedure, especially the spatula manufactured by the above method, which has high tarnishing ability and It is not easy to rust, and it is more smooth to use, and the life of the Lida is extended and the efficiency of use is improved. <Industrial application range> The present invention mainly uses a manufacturing method to produce a stainless steel spatula with high wear resistance and not easy to rust, which can extend its service life and can be smoother when using flat cement , In order to get better use efficiency. &lt; Background of the invention &gt; According to the current general spatula manufacturing method (_refer to the block flow chart of the conventional method of drawing), like using SK-5 steel plate as a material (because of its low content of squeegee, its The density is relatively sparse and the hardness is relatively weak, which can be manufactured by the conventional method), which mainly includes the following procedures: Cutting procedure: first cut into a rectangular plate body of appropriate size, and then the front end of the rectangular plate body Cut into arc-shaped points; Grinding procedure: water milling on the top surface and anti-ig of the rectangular plate. Punching procedure: drill holes in the proper position on the rear section of the top surface of the rectangular plate, so that the edge of the hole protrudes toward the bottom Out, and make a proper slope and a plurality of triangle-shaped notches on the edge of the top surface; Top surface secondary grinding procedure: secondary grinding with black stone on the top surface of the square plate; this paper scale uses Chinese national samples Rate (CNS &gt; A4 specification (210 X 297 mm) 83. 3.10,000 3 --------- ^ II-(Please read the note fvf on the back to write this page) Thread 2 / V Clearly stated

7 7 A B ;板 理狀 處方 光長 拋入 行插 進桿 面接 頂連 之 一 體以 板: 狀序 方程 長柄 於木 : 加 序並 程桿 光接 扰遶 面結 頂鉚 處 結 鉚 ^*&gt; 板合 狀嵌 方内 長槽 與缺 捍之 接柄 連木 該 一 將入 再套 而端 , 上 結桿 鉚接 内連 孔於 之並 段 , 後平 體敲' bla 進 石 黑 以 面 底 體 板 狀 方 長 於 序 程 磨 研 次 二 面 ., 底磨 研 次 理 處 光 拋 行 進 面 底 之 捿 板 狀 方 長 〇 於者 : 品 序成 程整 光完 拋一 面成 ;®造 •,製 即 失易 缺且 點低 二性 列磨 ·-、 JMJ T 而 有故 具, ,鋼 刀銹 抹不 之為 出非 造且 製弱 所薄 法較 方度 造硬 製其 之因 述5 上 1 氧故 成 , 造疏 中稀 氣較 空度 之密 氣其 含因 在且 放丨 置 2 後ί 之 ; 用命 使壽 者用 用使 使其 於短 往縮 往而 ,因 銹, 生化 者 率 效 用 使 其 低 降 而 因 順 滑 不 較 時 泥 &gt; 水理 平原 抹用 用作 使 &lt; ,計 刀設 抹方 之多 出經 造 , 製念 所意 法作 方創 造明 製發 刀及 抹思 統乃 傳 &gt; 於失 鑑缺 有多 人諸 明之 發上 本用 使 其 明高 發分 本成 出硪 推含 乃其 良理 改處 正經 修未 次尚 多 C 及鐵 , 白 驗之 試綱 品含 樣將 作先 試係 並其 討 探 ---------裝-- .' (請先聞讀背面之注{:壤寫本頁) 訂 線 經濟部中央橾準扃貝工消费合作社印«. 板體 ‘狀板 梯狀 成梯 切該 裁於 }而 高 ’ 愈狀 度尖 硬弧 、成 高製 愈裁 度端 密前 則之 '體 高板 愈狀 分梯 成將 硪再 含 , 而體 面狀 底梯 於將 並再 ,而 出, 凸 口 面缺 頂狀 往角 緣三 孔之 其數 使禊 ’出 孔打 打及 置度 位斜 當當 適適 段出 後打 面緣 底孔 出 5 凸以 緣再 孔另 面, 頂出 體凸 板面 部 底稍 體而 板, 狀理 梯處 往熱 其行 使進 ,度 打溫 敲之 向 P 方 ο 反 6 往 ~ 份p 本紙張尺度迷用中__家輾率(&lt;:糊以4«冰(2丨0&gt;&lt;297公釐)4 83. 3.10,000 305908 A7 A 7 B7 五、發明説明(3 ) ,研又 8 體,後成 工次,以板合磨造 加二理後狀嵌研製 磨,處結梯内次即 水磨光鉚與槽二 , 行研拋,桿缺,理 進次次結接之磨處 二再鉚連柄研光 後行及内將木次拋 狀進理孔再一二次 板面處之後入行再 平頂光段銷套進及 為體拋後退端石理 成板行體溫上黑處 而狀進板加桿以光 平梯面狀,接面拋 壓於頂梯鋦連底行 經石之入退將之進 再黑體插溫並體面 。 ,以板桿加,板底者 &gt; 狀後狀接行平狀板品的 浪工梯連進敲梯狀成目 波加於 I P 處於梯.霉明 成磨後以 ο 結再於完發 形水磨再'ο 鉚而再 一 &lt; 造俾 製, 之刀 刀抹 抹鋼 鏑銹 銹不 不之 ii 種鋇 1 生 供易 提不 在且 乃性。 , 磨者 的耐命 目高漭 要出用 主造使 之製之 明可刀 發其抹 本,長 ,法延 方逹 造率 製效 之用 刀使 抹之 綱佳 鈣較 不達 種俾 供順 提滑 在為 乃較 ,時 的泥 目水 平 次抹 之用 作使 創其 本, 法。 方者 發 本 明 説 細 詳 例 施 實 體 具 | 舉·* 列后 式如 圖節 合細 &gt; 配及 例M容 施,内 實下序 體餘程 具 之 &lt; 明 (請先聞讀背面之注意事填寫本頁 裝· 订 線 經濟部中央梂準局貞工消费合作社印家 綱,序 含高程 以愈之 係分列 其成下 , 硪含 圄含包 程而要 流,主 塊高其 方分, 之成料 明硪材 發含為 本其} 為,高 像理愈 示處度 所經硬 圖未 、 二尚高 第丨愈 如鏃度 白密 之則 前 之 體 板 狀 梯 將 並 體 板 狀 梯 成 切 裁 先 序 程 切 裁 本紙張尺度適用中國_家褊奉(CNS &gt; Α4ϋ格(210X297公釐&gt; 5 83. 3.10,000 A7 B7 五、發明説明(4 ) 端裁製成弧尖狀; 2 .打孔程序:於梯狀板體底面後段適當位置打孔(長 方狀),使其孔緣往頂面凸出,並於底面孔緣打出適當斜 度及打出禊數之三角狀缺口 ,再將梯狀板髓頂面孔綵凸出 部份往反方向敲打,使其往梯狀板體底面凸出; 3. 熱處理程序:以5 8 10〜6 OC之溫度進行熱處理 ,使其稍形成波浪狀; 4. 研磨程序:先經壓平而成為平板狀後,於梯狀板體 之頂面及底面進行水磨加工; 5. 頂面二次研磨程序:以黑石於梯狀板體之頂面進行 二次研磨; 6. 頂面拋光程序:於梯狀板髓之頂面進行抛光處理及 再次.抛光處理; 鉚結連接桿處理程序··以一逋接桿插入梯狀板體後 段之孔内鉚結,鉚結之同時亦會使原先打孔程序中往梯狀 板體底面凸出之部份有輪平之效果,但邇是稍微凸出一小 部份; 8 ·加溫退銅程序:鉚結後以8 0 0 C進行加溫退銷, 加溫退鏑後再將連接桿與梯狀板體鉚結處敲平,並將連接 桿上端套入一木抦之缺槽内嵌合; 9. 底面二次研磨程序:以黑石於梯狀板醴之底面進行 二次研磨; 10. 底面拋光程序:於掸狀板鱷之底面進行拋光處理 及再次拋光處理,卽製造成一完整成品者。 本紙張尺度適用中國國家標率(CNS &gt; A4规格(210X297公釐) 6 五、發明説明(5 A7 B7 而值申 ,價利 法用專 方利明 之之發 用上出 習業提 破產法。 。 突有依播 圖。 有具爰為 程匾 具又 &gt; 利 流程 經時定専 塊流 己同規准 方塊 實,條惠 之方 確容九員 法之 明内十委 方明 發法第查 用發 本方法審 &gt; 習本 ,之利局明係係 陳作專鈞説:: 所創合 單圖臛 上度符謓簡一 二 綜高能懇式第第 有當,圄 具,讅&lt; ----------^------ir------i (請先 W 讀.背面之·&gt;±*fqix、^4Jr) 一 經濟部中央搮準局貝工消费合作社印製 本紙張尺度逋用中國II家樣窣(CNS ) A4规格&lt; 210X297公漦&gt;7 7 AB; The plate-like prescription light length is thrown into the face and the top is connected to one body to the plate: the state-order equation long handle is to the wood: the addition of the parallel rod light interference around the surface knot rivet knot ^ * &gt; The long groove in the plate-like embedded square and the lack of the handle and the wood should be put into the end, the upper knot rod is riveted to the inner connecting hole, and the flat body knocks' bla into the stone black to face the bottom body The plate-shaped square is longer than the sequence grinding and grinding two sides., The bottom grinding and polishing treatment is to polish the surface of the polishing surface. The plate-shaped square is longer than: That is, it is indispensable and the point of low-impermanence column grinding ---, JMJ T has a reason, and the steel knife can't be wiped out for non-manufacturing and the weakening method is thinner than the square manufacturing method. 1 Oxygen is formed, and the dense gas with less air in the sparseness is contained in and placed after 2; it is used by the life-saver to shrink it in the short term, due to rust, biochemical The rate utility makes it lower and the sludge is smoother and smoother Acting &lt; Counting knives to set up a lot of ways to create more than the creation, the method of thinking to create a method to create a hair-cutting knife and the way of thinking is to pass &gt; Ming Gaofa splits the book into a book and pushes it out. It ’s a good reason to change it. It ’s still a lot of C and iron. The sample content of the white test will be used as the first test and discussed -------- -Install--. '(Please read the note on the back {: Yang writes this page). Printed by the Ministry of Economic Affairs, Central Ministry of Industry and Fisheries Cooperative Printing Co., Ltd. «. The plate body is shaped like a ladder and cut into ladders. And the higher the sharper the harder the arc, the higher the degree of cutting and the denser the front is, the higher the body plate is, the more the ladder is divided into the re-contained, and the decent-shaped bottom ladder is merged again and out, the protruding mouth The number of holes on the corner is three holes at the corner edge, so that the holes are punched out and the position is skewed. When the proper section is out, the bottom hole of the face edge is punched out and 5 holes are raised. The bottom of the face is slightly flat, and the ladder is heated towards the front of the ladder, and the temperature is knocked toward the side P ο The counter 6 toward ~ copies p This paper size is used_ _Home roll rate (&lt;: paste with 4 «ice (2 丨 0> &lt; 297mm) 4 83. 3.10,000 305908 A7 A 7 B7 V. Description of the invention (3), research and 8 body, later The number of times is to use the plywood grinding and secondary grinding to embed and develop the grinding. The internal ladder is the second time, which is water grinding and riveting, and the groove is two. After polishing the stem, the wood will be thrown into the hole and then into the hole again and again, then the flat-top light section pin will be inserted and the body will be thrown back to the stone to form the board and the body temperature will be darkened and the board will be added. The pole is in the shape of a smooth flat ladder, and the junction is pressed against the top ladder and the bottom passes through the stone, and then it is inserted into the black body and inserted into the temperature and decent. , Add with poles, bottom of the plate> the wave-shaped ladder that connects the flat-shaped plate products after the shape is connected into the shape of the knocking ladder, and the wave is added to the IP. It is on the ladder. After the mold is ground, it will be knotted and then finished. Water milling again 'ο riveting and making again &lt; made by the system, the knife knife wipes the steel dysprosium rust rust is not only ii kind of barium 1 raw material is easy to mention and is not. , The grinder ’s perseverance is high, and he must use the master to make it clear, and use the knife to make it. The smoothness of the slippery slope is the second time, and the level of muddy eyes is used as a method to create its original value. Fang Zhe issued a detailed explanation of the specific examples of the physical implements | Example · * The following formula is as shown in the section &gt; Matching and example M Rong Shi, the actual sequence of the remaining parts of the program &lt; Ming (please read the back first Please pay attention to this page and fill out this page. · The Order of the Ministry of Economic Affairs, Central Bureau of Economic Affairs, Jeonggong Consumer Cooperative, Yinjiagang. The sequence contains the elevation and is divided into more and more. The main block is higher than the main block. Fangfen, the composition of the material is based on the original material. The higher the image, the more the image shows, the harder the picture is, the second is still higher, and the front is more like a white plate. The parallel plate-shaped ladder is cut into the cutting process. The paper size is suitable for China_ 家 褊 奉 (CNS &gt; Α4ϋ grid (210X297mm &gt; 5 83. 3.10,000 A7 B7 V. Invention description (4) Cut into an arc-shaped shape; 2. Punching procedure: punch holes (rectangular shape) at the appropriate position in the rear section of the bottom surface of the trapezoidal plate body to make the hole edge protrude toward the top surface, and punch the appropriate slope and edge on the bottom edge Make a triangle-shaped notch, and then tap the protruding part of the top surface of the ladder-shaped plate pulp in the opposite direction to make it go to the ladder The bottom surface of the plate-shaped body is protruding; 3. Heat treatment process: heat treatment at a temperature of 5 8 10 ~ 6 OC to make it slightly wavy; 4. Grinding process: flattened to a flat shape first, and then on a ladder-shaped plate The top surface and bottom surface of the body are water-milled; 5. The second surface grinding process of the top surface: using black stone to perform the second grinding on the top surface of the trapezoidal plate body; 6. The top surface polishing procedure: performing on the top surface of the trapezoidal plate pith Polishing treatment and again. Polishing treatment; Riveting connecting rod processing procedure · · Riveting a rod into the hole in the rear section of the trapezoidal plate body, riveting at the same time will also cause the original punching process to the trapezoidal plate body The protruding part of the bottom surface has the effect of wheel flatness, but it is slightly protruding a small part; 8 · Heating and copper removal procedure: after riveting, heating and reversing are carried out at 800 C, after heating and dysprosium Knock the connecting rod and the trapezoidal plate body flat, and fit the upper end of the connecting rod into the missing groove of a wooden shaft; 9. Secondary grinding process of the bottom surface: use black stone on the bottom surface of the ladder plate Secondary grinding; 10. Bottom surface polishing procedure: perform polishing treatment and re-polishing treatment on the bottom surface of the alligator , 卽 Manufactured into a complete finished product. This paper scale is applicable to China's national standard rate (CNS> A4 specification (210X297 mm) 6 V. Description of invention (5 A7 B7 Value application Use the bankruptcy law to apply the practice.. Suddenly according to the broadcast map. You have to be Cheng Chengjue &gt; the profit process is fixed over time, and the block flow is the same as the standard. The tenth committee of the Ming dynasty Fang Mingfa issued a legal review method for reviewing the textbooks.> This book, the Department of the Ming Dynasty ’s Ming Dynasty Department, Chen Zuozhuanjun said: The first is the right thing, the joke, the omission &lt; ---------- ^ ------ ir ------ i (please read the W first. Back of it &gt; ± * fqix, ^ 4Jr) A copy of the paper size printed by the Beigong Consumer Cooperative of the Central Bureau of Economics and Trade of the Ministry of Economic Affairs, using the Chinese II model (CNS) A4 specification &lt; 210X297 Gongluo &gt;

Claims (1)

經濟部中央揉準局負工消费合作社印製 305908 H C8 D8六、申請專利範圍 一種不銹鏑@刀之製造方法,其像以含鋼之白鐵為材 料,其程序包含: 裁切程序:先裁切成梯狀板體,並將梯狀板體之前端 裁製成弧尖狀; 打孔程序:於梯狀板體底面後段適當位置打孔,使其 孔緣往頂面凸出,並於底面孔絲打出適當斜度及打出複數 之三角狀缺口 ,再將涕狀板體頂面孔綠凸出部份往反方向 敲打,使其往悌狀板體底面凸出; 熱處理程序:以5 8 t)〜6 ◦ 之溫度進行熱處理, 使其稍形成波浪狀; 研磨程序:先經壓平而成為平板狀後,於梯狀板體之 頂面及底面進行水磨加工; 頂面二次研磨程序:以黑石於梯狀板體之頂面進行二 次研磨; 頂面拋光程序:於梯狀板體之頂面進行抛光處理及再 次拋光處理; 鉚結連接桿處理程序:以一連接桿插入梯狀板體後段 之孔内鉚結,鉚結之同時亦會使原先打孔程序中往梯狀板 體底面凸出之部份有輪平之效果,但還是稍微凸出一小部 份; 加溫退鋼程序,鉚結後以8 Ο Ο T:進行加溫退鋼,加 溫退鋼後再將連接桿與梯狀板體鉚結處敲平,並將連接桿 上端套入一木柄之缺槽内嵌合; 底面二次研磨程序:以黑石於梯狀板體之底面進行二 (請先閲讀背面之注意為填寫本頁) •裝. 訂 線. 本紙張尺度逋用中國困家摞率(CNS &gt; A4规格(210X297公釐) 8 申請專利範圍 A8 B8 C8 D8 再 及 理 處 光 拋 -了 //Ί 進 面 底 之 體 板 狀 梯 於 序 程 光 拋 ; 面 磨底 研 次 月 使 另 生 易 不 且 性 磨 耐 高 具 成 造。 製者 即刀 ,抹 理之 處順 光滑 抛為 次較· ------:---裝-- (請先聞讀背面之注意事ί-?»填寫本頁) 訂 經濟部中央標準局®C工消费合作杜印製 I Ns6 /1% 率 鏢 家 國 國 中 用 適 ¥ 97n 2 XPrinted 305908 H C8 D8 by the Negative Workers' Consumer Cooperative of the Ministry of Economic Affairs of the Ministry of Economic Affairs. 6. Patent application. A manufacturing method of stainless dysprosium @ 刀, which is made of white iron containing steel. Its procedures include: Cutting procedure: first Cut into a trapezoidal plate body, and cut the front end of the trapezoidal plate body into an arc-shaped shape; Punching procedure: punch holes at an appropriate position on the bottom section of the bottom surface of the trapezoidal plate body so that the edge of the hole protrudes toward the top surface, and Make a proper slope and a plurality of triangular notches on the bottom surface, and then tap the green protruding part of the top surface of the slab-shaped body in the opposite direction to make it protrude toward the bottom of the slab-shaped body; Heat treatment procedure: 5 8 t) ~ 6 ◦Temperature heat treatment to make it slightly wavy; Grinding procedure: after flattening into a flat shape, water grinding on the top and bottom surfaces of the trapezoidal plate body; secondary grinding of the top surface Procedure: Black stone is used for secondary grinding on the top surface of the trapezoidal plate; Top surface polishing procedure: Polishing and re-polishing treatment on the top surface of the trapezoidal plate; Rigid connecting rod processing procedure: Inserting with a connecting rod Riveting of holes in the rear section of the trapezoidal plate body At the same time, the riveting will also make the part protruding toward the bottom of the trapezoidal plate body in the original punching program have a wheel flat effect, but it still slightly protrudes a small part; 8 Ο Ο T: Heating and stripping steel, after heating and stripping steel, knock the connecting rod and the trapezoidal plate body riveting flat, and insert the upper end of the connecting rod into a groove with a wooden handle to fit; bottom surface two Sub-grinding procedure: Use black stone on the bottom surface of the trapezoidal plate body (please read the note on the back to fill out this page) • Binding. Threading. The paper size is based on China ’s sleepy stacking rate (CNS &gt; A4 specification ( 210X297mm) 8 Patent scope A8 B8 C8 D8 and then deal with light polishing-// Ί Enter the bottom of the body plate-shaped ladder in the sequence of light polishing; surface grinding bottom research the next month to make the other easy to wear It ’s a masterpiece. The maker is the knife, and the smoothing is smooth and the second is better. ------: --- install-- (please read the notes on the back first-? »Fill in this page ) Ordered by the Central Bureau of Standards of the Ministry of Economic Affairs ®C Industrial and Consumer Cooperation Du Printed I Ns6 / 1% rate dart home country junior high school ¥ 97n 2 X
TW85110825A 1996-09-05 1996-09-05 Manufacturing method for stainless trowel TW305908B (en)