Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiann-Ren LinfiledCriticalJiann-Ren Lin
Priority to TW83102879ApriorityCriticalpatent/TW246659B/en
Application grantedgrantedCritical
Publication of TW246659BpublicationCriticalpatent/TW246659B/en
A process of EVA surface printing, in which the medium dry diluent mainlycomprises cyclohexanone, the slow dry diluent mainly comprises isophorone, the auxiliary binder comprises diluent resin, and the ink comprises lead, antimony, arsenic, barium, cadmium, chromium, mercury, selenium; which comprise sadding rubber treatment agent with about 0.5% of auxiliary binder and mixing the mixture to be used as treatment of silicone delamination agent on EVA surface, mixing the auxiliary binder with ink as the printing ingredient, placing the EVA formed material into the printing machine to be printed by the printing ingredient, heating the printed material, cooling the printed material to obtain the product.
TW83102879A1994-04-011994-04-01Process of EVA surface printing
TW246659B
(en)