TW200927492A - Method of making mouse pad - Google Patents

Method of making mouse pad Download PDF

Info

Publication number
TW200927492A
TW200927492A TW96150702A TW96150702A TW200927492A TW 200927492 A TW200927492 A TW 200927492A TW 96150702 A TW96150702 A TW 96150702A TW 96150702 A TW96150702 A TW 96150702A TW 200927492 A TW200927492 A TW 200927492A
Authority
TW
Taiwan
Prior art keywords
fiber cloth
mouse pad
heating
heated
fiber
Prior art date
Application number
TW96150702A
Other languages
Chinese (zh)
Other versions
TWI426023B (en
Inventor
Jen-Yi Gau
Original Assignee
See Green Ind Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by See Green Ind Co Ltd filed Critical See Green Ind Co Ltd
Priority to TW96150702A priority Critical patent/TW200927492A/en
Publication of TW200927492A publication Critical patent/TW200927492A/en
Application granted granted Critical
Publication of TWI426023B publication Critical patent/TWI426023B/zh

Abstract

This invention provides a method of making a mouse pad, which mainly heats and imposes pressure on a fiber cloth on the surface of a mouse pad so as to transform the fiber cloth into a flat layer and a fiber layer. A pattern is then printed on the flat layer of the fiber cloth so as to produce a mouse pad with a clear pattern.

Description

200927492 九、發明說明: 【發明所屬之技術領域】 本發明係與滑鼠墊有關,更詳而言之是指一種可 一製成具清晰圖案之-滑鼠墊之氣法者。 _ 【先前技術】 按,習知滑鼠墊大體上有硬式滑鼠墊與軟式滑鼠 ❹ 塾一大類’硬式滑鼠塾係由一塑料層(如PP、PVC及 PE等材質)與一防滑層(如NR、EVA及pu等材質) 所構成’而軟式滑鼠塾係由一纖維布料層(如 POLYESTER、COTTON等材質)與一防滑層(如NR、 EVA及PU等材質)所構成。其次,為增進外觀之美 感,不論硬式滑鼠墊或軟式滑鼠墊其塑料層或纖維布 料層表面皆印刷有圖案或文字。 由於硬式滑鼠墊之塑料層表面較平坦細緻,因 此’塑料層表面所印刷之圖案可甚為清晰,同時,表 面之污物亦容易清除’惟,其整體材質較硬,不易折 收攜帶、攜帶較為不便。而軟式滑鼠墊整體材質較柔 軟、易於捲收攜帶’緩衝性亦佳,不過,其織維布料 層易污損’纖維布料層表面所印刷之圖案通常不夠清 晰,且’其邊緣易產生毛邊、較不美觀。換言之,習 知之硬式滑鼠墊或軟式滑鼠墊皆有其優缺點’仍有可 改善之處。 200927492 【發明内容】 之二明:主要目的即在提供一種可解決前揭缺失 之滑鼠墊之製法,其不僅整黯質錄、易於捲收播 帶,緩衝性佳,且,其表面所印刷《圖案可甚為清晰, 表,之污物亦容易清除,俾可兼具習知 墊之優點而改善二者之缺點者。 '滑鼠 緣是,為達成前述之目的,本創作係提供一種滑 ❹1墊之製法’其主要步驟係包含有:備取原料:取一 纖維布料;加熱加壓:對該纖維布料一側加熱並施加 壓力,使該纖維布料形成一平坦層與一纖維層;印刷: 於該纖維布料之平坦層上印刷圖案;結合彈性墊:將 該纖維布料之纖維層一側貼置於一彈性墊上,俾製成 一滑鼠塾。200927492 IX. Description of the Invention: [Technical Field of the Invention] The present invention relates to a mouse pad, and more particularly to a gas-method that can be made into a clear pattern-mouse pad. _ [Prior Art] According to the conventional mouse pad, there are basically a hard mouse pad and a soft mouse ❹ 塾 A large type of 'hard mouse 塾 is made of a plastic layer (such as PP, PVC and PE) and a non-slip Layers (such as NR, EVA, and pu) are composed of 'soft rat's made of a fiber cloth layer (such as POLYESTER, COTTON, etc.) and a non-slip layer (such as NR, EVA, and PU). Secondly, in order to enhance the aesthetic appearance, the surface of the plastic layer or the fiber cloth layer of the hard mouse pad or the soft mouse pad is printed with a pattern or a letter. Since the surface of the plastic layer of the hard mouse pad is relatively flat and fine, the pattern printed on the surface of the plastic layer can be very clear, and the dirt on the surface can be easily removed. However, the overall material is hard and difficult to carry and carry. It is inconvenient to carry. The soft mouse pad is soft and easy to roll and carry. 'The cushioning property is also good. However, the weaving fabric layer is easily stained. The printed pattern on the surface of the fiber cloth layer is usually not clear enough, and the edge is easy to produce burrs. Less beautiful. In other words, the conventional hard mouse pad or soft mouse pad has its advantages and disadvantages. There is still room for improvement. 200927492 [Description of the Invention] The second objective: the main purpose is to provide a method for solving the missing mouse pad, which is not only tidy, easy to roll, and has good cushioning, and the surface is printed. "The pattern can be very clear, the table, the dirt can be easily removed, and the advantages of the conventional pad can be improved to improve the shortcomings of both. 'The mouse edge is, in order to achieve the above purpose, the present invention provides a method for the production of a sliding mat 1'. The main steps include: preparing raw materials: taking a fiber cloth; heating and pressurizing: heating one side of the fiber cloth And applying pressure to form the fiber cloth to form a flat layer and a fiber layer; printing: printing a pattern on the flat layer of the fiber cloth; and combining the elastic pad: the fiber layer side of the fiber cloth is placed on an elastic mat,俾 Make a mouse 塾.

此外,本發明更提供一種滑鼠墊之製法,其主要 步驟係包含有:備取原料:取未印刷圖案之一滑鼠墊 胚料,該滑鼠墊胚料包含一彈性體及貼置於彈性體表 面之一纖維布料;加熱加壓:對該纖維布料表面加熱 並施加壓力,使該纖維布料形成一平坦層與一纖維 層;印刷:於該纖維布料之平坦層上印刷圖案,俾製 成表面具清晰印刷圖案之一滑鼠塾。 【實施方式】 以下,茲舉本發明作若干較佳實施例,並配合圖 200927492 式做進一步之詳細說明如後: •請參閱圖-至圖四所示,本發明一較佳實施例之 /月鼠墊ίο之製法,其第一步驟係備取原料ιι〇 :係取 .一纖維布料12’該纖維布料_12係具纖维結構之 如 POLYESTER、COTTON 等材質。 本發明之第二步驟係加熱加壓12〇:係利用一習 知滾軋裝置20對該纖維布料12同時加熱加壓,該滾 G車L裝置20係包含相對之一加熱滾輪201與-常溫滾輪 〇2該加熱滾輪201係具備等於或大於該纖維布料 12熔點之溫度,俾該纖維布料12經由加熱滾輪 與常溫滾輪202之間受熱、受滾軋後,該纖維布料12 表面部分之纖維可熔化、受壓而形成厚度甚薄之一平 坦層22與一纖維層24。該平坦層22係呈光滑塑膠面 狀。 本發明之第三步驟係印刷13〇:於該平坦層22上 ◎ 印刷圖案。 本發明之第四步驟係結合彈性體140 ··將該纖維 布料12之纖維層24 一側貼置於一彈性體14上俾可 製成表面具清晰印刷圖案之一滑鼠墊20。該彈性體14 係橡膠材料製成之彈性體,而該纖維布料12貼置於彈 性體14上之方式,可利用黏著劑將二者貼合,亦可將 該纖維布料12置於尚未發泡成型之橡膠片(内含發泡 劑等原料)上一體發泡成型而結合,俾毋須利用黏著 200927492 劑將二者貼合者。 藉此,本發明所提供滑鼠塾之製法,其藉由將組 成該滑鼠墊20之纖維布料12加熱並施加壓力之方 式,使該纖维布料12可形成一平坦層22與一纖維層 24,由於好坦層22之結構已成為缝塑膠面故, 於該平坦層22表面所印刷之圖案甚為清晰,表面之污 物亦容易清除,且,該平坦層22邊緣更不會產 Ο 而影響美觀,再者’該平坦層22之厚度甚薄,俾使該 滑鼠塾2G甚為柔軟而易於捲收攜帶,該彈性體^亦 可使滑鼠塾20具甚佳之緩衝性。基此,該滑鼠塾加 可兼具習知硬、軟式滑鼠塾之優點而改善二者之 者。 、” 此外,如圖五所示,本發明之加熱加壓步驟中, 亦可先利用一習知烤箱30對該纖維布料12加熱後, 再利用一滾軋裝置32對該纖維布料12加壓,此時, 該滚軋裝置32係由二常溫滾輪34所組成。 更者,本發明之加熱加壓步驟中,亦可利用一習 知之熱壓裝置(圖中未示)對該纖維布料同時加熱加 壓,該熱壓裝置係包含一承座與可移動之一熱壓板, 該纖維布料係置於承座上而受熱壓板加熱施壓' :, 其次,如圖六及圖七所示,本發明備取原料之步 驟中,亦可先取未印刷圖案之滑鼠墊胚料4〇,該滑鼠 墊胚料40包含已黏貼完成之彈性體42及纖維布料 200927492 44,再利用前揭包含加熱滾輪之滾軋裝置或烤箱、滚 軋裝置搭配之二種不同方式實施加熱加歷步驟,使該 纖維布料44形成平坦層46與纖維層48,俾可於該平 坦層46上印刷圖案:藉此,亦可製成表面具清晰印刷 圖案之滑鼠墊,而產生如前所述之功效者。 值得一提的是,本發明之加熱加壓步驟中所採用 之滾乾裝置,其加熱滾輪上亦可設有凹凸紋路狀之壓 ❷ 印部位,俾可使該滑鼠墊表面除了具有清晰印刷圖案 外’更可具有紋路之造型而增進外觀之美感。 綜上所陳,本發明所提供滑鼠墊之製法,其不僅 整體材質柔軟、易於捲收攜帶、緩衝性佳,且,其表 面所印刷之圖案可甚為清晰,表面之污物亦容易清 除,俾可兼具習知硬、軟式滑鼠墊之優點而改善二者 之缺點;緣是,本發明確實符合發明專利之規定,爰 依法提出申請。 〇 【圖式簡單說明】 圖一係本發明一較佳實施例之流程圖。 圖二係本發明一較佳實施例所製成滑鼠墊之外觀 圖。 圖三係本發明一較佳實施例所製成滑鼠墊之側視 圖。 圖四係本發明一較佳實施例中加熱加壓步驟之示 9 200927492 意圖。 圖五係本發明另一較佳實施例中加熱加壓步驟之 示意圖。 _圖六係本弩明再一較佳實施例中加熱加壓步驟之 示意圖。 圖七係本發明又一較佳實施例中加熱加壓步驟之 不意圖。 ΟIn addition, the present invention further provides a method for preparing a mouse pad, the main steps of which are: preparing a raw material: taking a mouse pad blank of an unprinted pattern, the mouse pad blank comprising an elastic body and a sticker a fiber cloth on the surface of the elastomer; heating and pressurizing: heating and applying pressure on the surface of the fiber cloth to form a flat layer and a fiber layer; printing: printing a pattern on the flat layer of the fiber cloth, tanning One of the surface has a clear printed pattern of mouse 塾. [Embodiment] Hereinafter, the present invention will be described as a few preferred embodiments, and further detailed description will be made in conjunction with FIG. 200927492: • Please refer to FIG. 4 to FIG. 4, a preferred embodiment of the present invention/ The method of making the mouse pad ίο, the first step is to prepare the raw material ιι〇: to take a fiber cloth 12' the fiber cloth _12 with a fiber structure such as POLYESTER, COTTON and other materials. The second step of the present invention is heating and pressurizing 12: the fiber cloth 12 is simultaneously heated and pressurized by a conventional rolling device 20, which comprises a heating roller 201 and a normal temperature. The heating roller 201 has a temperature equal to or greater than the melting point of the fiber cloth 12, and after the fiber cloth 12 is heated and rolled by the heating roller and the normal temperature roller 202, the fiber of the surface portion of the fiber cloth 12 can be It is melted and pressed to form a flat layer 22 and a fibrous layer 24 which are very thin. The flat layer 22 is in the form of a smooth plastic surface. The third step of the present invention is to print 13: on the flat layer 22 ◎ print the pattern. The fourth step of the present invention is to bond the elastic body 140 to the side of the fibrous layer 24 of the fibrous cloth 12, and to form a mouse pad 20 having a clear printed pattern on the surface. The elastic body 14 is an elastic body made of a rubber material, and the fiber cloth 12 is attached to the elastic body 14 in such a manner that the two can be adhered by an adhesive, and the fiber cloth 12 can be placed not yet foamed. The molded rubber sheet (the raw material containing a foaming agent) is integrally molded by foam molding, and it is not necessary to adhere the two by using the adhesive 200927492. Accordingly, the present invention provides a method for manufacturing a mouse squeegee, which can form a flat layer 22 and a fibrous layer by heating and applying pressure to the fiber cloth 12 constituting the mouse pad 20. 24, since the structure of the good layer 22 has become a plastic surface, the pattern printed on the surface of the flat layer 22 is very clear, the dirt on the surface is easily removed, and the edge of the flat layer 22 is less likely to be produced. The effect is beautiful, and the thickness of the flat layer 22 is very thin, so that the mouse 塾 2G is very soft and easy to carry and carry, and the elastic body can also make the mouse 塾 20 have a very good cushioning property. Based on this, the mouse can be improved by combining the advantages of the conventional hard and soft mouse. In addition, as shown in FIG. 5, in the heating and pressurizing step of the present invention, the fiber cloth 12 may be heated by a conventional oven 30, and then the fiber cloth 12 is pressurized by a rolling device 32. In this case, the rolling device 32 is composed of two normal temperature rollers 34. Further, in the heating and pressurizing step of the present invention, the fiber cloth can be simultaneously used by a conventional hot pressing device (not shown). Heating and pressurizing, the hot pressing device comprises a socket and a movable heat pressing plate, the fiber cloth is placed on the bearing seat and heated and pressed by the hot pressing plate ':, secondly, as shown in FIG. 6 and FIG. As shown in the present invention, in the step of preparing the raw material, the unloaded pattern of the mouse pad blank 4 may be taken first, and the mouse pad blank 40 includes the adhered elastic body 42 and the fiber cloth 200927492 44, and reused. The heating and calendering step is carried out in two different ways, including the rolling device comprising the heating roller or the oven and the rolling device, so that the fiber cloth 44 forms the flat layer 46 and the fiber layer 48, and the crucible can be printed on the flat layer 46. Pattern: This can also be used to make the surface clear The pattern of the mouse pad, which produces the effect as described above. It is worth mentioning that the drying device used in the heating and pressurizing step of the present invention may also be provided with a concave-grained pressure on the heating roller. In addition to the printed portion, the surface of the mouse pad can have a grainy shape to enhance the aesthetic appearance. In summary, the method for manufacturing the mouse pad of the present invention is not only the overall material. It is soft, easy to carry, and has good cushioning properties. The printed pattern on the surface can be very clear, and the dirt on the surface can be easily removed. The advantages of the conventional hard and soft mouse pad can be improved. The reason for this is that the present invention does meet the requirements of the invention patent, and the application is made according to the law. 〇 [Simplified description of the drawings] Figure 1 is a flow chart of a preferred embodiment of the present invention. Figure 2 is a preferred embodiment of the present invention. Figure 3 is a side view of a mouse pad made in accordance with a preferred embodiment of the present invention. Figure 4 is a representation of a heating and pressurizing step in a preferred embodiment of the present invention 9 200927492 intention. Figure 5 is a schematic view showing a heating and pressurizing step in another preferred embodiment of the present invention. Fig. 6 is a schematic view showing a heating and pressurizing step in still another preferred embodiment of the present invention. Fig. 7 is still another preferred embodiment of the present invention. In the example, the heating and pressurizing step is not intended.

【主要元件符號說明】 10 :滑鼠墊 14 :彈性體 2 01 :加熱滾輪 22 :平坦層 30 :烤箱 34常溫滾輪 42 :彈性體 46 :平坦層 110 :備取原料 130 ··印刷 12 :纖維布料 2〇 :滾軋裝置 202 :常溫滾輪 24 :纖維層 32 :滾軋裝置 40 :滑鼠墊胚料 44 :纖維布料 48 :纖維層 120 :加熱加壓 140 :結合彈性體[Description of main component symbols] 10: Mouse pad 14: Elastomer 2 01: Heating roller 22: Flat layer 30: Oven 34 Normal temperature roller 42: Elastomer 46: Flat layer 110: Raw material 130 • Print 12: Fiber Cloth 2: Rolling device 202: Normal temperature roller 24: Fiber layer 32: Rolling device 40: Mouse pad blank 44: Fiber cloth 48: Fiber layer 120: Heat and pressure 140: Bonding elastomer

Claims (1)

200927492 十、申請專利範固: L一種滑鼠墊之製法,其主要步驟係包含有: 備取原料:取1”料; 加,’、、加壓·對該纖維布料一侧加熱並施加壓力, 使該纖維布料形成,平坦層與一纖維層; 印刷·於該纖維布料之平坦層上印刷圖案;及 Ί σ彈性塑*:將該纖維布料之纖維層一側貼置於 ❹一彈性體上’俾製成-滑鼠墊。 2. 依據申請專利範圍第1項所述滑鼠墊之製法, 其中,加熱加壓之步驟中,係以等於或大於該纖維布 料熔點之溫度加熱纖維布料,用以使該纖維布料表面 之纖維溶化而受壓成平坦層。 3. 依據申請專利範圍第1項所述滑鼠墊之製法, 其中,加熱加壓之步驟中,係利用一滚軋裝置對該纖 維布料同時加熱加廢。 4·依據申請專利範圍第3項所述滑鼠墊之製法, 其中,該滾軋裝置係包含相對之一加熱滾輪與一常溫 滾輪’該纖維布料係經由加熱滾輪與常溫滾輪之間受 熱及受滾軋。 ^ 5. 依據申請專利範圍第1項所述滑鼠墊之製法, 其中,加熱加壓之步驟中,係先將該纖維布料表面加 熱後再施壓而形成平坦層。 6. 依據申請專利範圍第5項所述滑鼠墊之製法, 11 200927492 其中,加熱加壓之步驟中’係先利用一烤箱對該纖維 布料加熱,再利用一滾軋裝置對該纖維布料加壓。 7·依據申請專利範圍第6項所述滑鼠塾之製法, -其中,該滾〜軋裝置係包含相對之二常溫滾輪,該纖維 布料係經电二常溫滾輪之間受滾軋。 8. 依據申請專利範圍第1項所述滑鼠塾之製法, 其中,加熱加壓之步驟中,係利用一熱壓裝置對該纖 I 維布料同時加熱加麼。 "" 9. 依據申請專利範圍第8項所述滑鼠墊之製法, 其中,該熱壓裝置係包含一承座與可移動之一熱壓 板,該纖維布料係置於承座上受熱壓板加熱施壓。 1〇·依據申請專利範圍第1項所述滑鼠墊之製法, 其中,該彈性體係橡膠材料製成之彈性體。 11. 一種滑鼠墊之製法’其主要步驟係包含有· 備取原料:取未印刷圖案之-滑鼠墊胚料,該滑 =塾胚料包含-彈性體及貼置於彈性體表面之 布料; 熱加壓.對該纖維布料表面加熱並施加廢力, 使該纖維布料形成一平坦層與一纖維層;及 I7刷·於該纖維布料之平坦層上印刷圖案,俾製 成表面具清晰印刷圖案之一滑鼠墊。 ,=·依據申請專利範圍第u項所述滑鼠塾之製 、加熱加墨之步驟中,係以等於或大於該纖 12 200927492 ==Γ織維布料“加熱,用以使該 纖維布料表面之纖維熔化而受壓成平括層 13.依據申請專利範圍第丨 — ..^ ^ ,罘11項所述滑鼠墊之製 法,-其中’加綠加麼之步驟中,係利用一滾 該滑鼠墊胚料同時加熱加壓。 赛 、Λ依據申請專利範圍第13項所述滑鼠藝之製 該滾軋裝置係包含相對之-加熱滾輪與- ❹ 該滑鼠墊胚料係以纖維布料對應加熱滾輪 之方式經由加熱滾輪與常溫滾輪之間受熱及受滚軋。 15·依據申請專利範圍帛U項所述滑鼠塾之製 法’其中’加熱加壓之步驟中,係先將該纖維布料表 面加熱後再施壓而形成平坦層。 16. 依據申請專利範圍第15項所述滑鼠墊之製 法,其中,加熱加壓之步驟中,係先利用一烤箱對該 ο 滑鼠塾胚料之纖維布料加熱,再利用-滾軋褒置對該 滑鼠墊胚料加壓。 17. 依據申請專利範圍第16項所述滑鼠墊之製 法’其中’該滾軋裝置係包含相對之二常溫滾輪,該 滑鼠墊胚料係經由二常溫滾輪之間受滾軋。 18. 依據申請專利範圍第u項所述滑鼠墊之製 法,其中,加熱加壓之步驟中,係利用一熱壓裝置對 該滑鼠墊胚料同時加熱加壓。 19. 依據申請專利範圍第18項所述滑鼠墊之製 13 200927492 法,其中,該熱壓裝置係包含一承座與可移動之一熱 壓板,該滑鼠墊胚料係置於承座上而使纖維布料受熱 壓板加熱施壓。 p 20.依據申請專利範-圍·第10項所述滑鼠墊之製 法Λ其中,該彈性體係橡膠材料製成之彈性體。200927492 X. Patent application: The method of making a mouse pad, the main steps of which include: Preparing raw materials: taking 1" material; adding, ',, pressing · heating and applying pressure to one side of the fiber cloth Forming the fiber cloth, a flat layer and a fiber layer; printing and printing a pattern on the flat layer of the fiber cloth; and Ί σ elastic plastic*: attaching the fiber layer side of the fiber cloth to the elastic body 2. The method of manufacturing a mouse pad according to the scope of claim 1, wherein in the step of heating and pressurizing, the fiber cloth is heated at a temperature equal to or greater than the melting point of the fiber cloth. In order to melt the fibers on the surface of the fiber cloth and press it into a flat layer. 3. The method for manufacturing a mouse pad according to claim 1, wherein in the step of heating and pressurizing, a rolling device is used. The fiber cloth is heated and added at the same time. 4. The method for manufacturing a mouse pad according to claim 3, wherein the rolling device comprises a heating roller and a normal temperature roller. The hot roller and the normal temperature roller are heated and rolled. ^ 5. According to the method for preparing the mouse pad according to claim 1, wherein in the step of heating and pressurizing, the surface of the fiber cloth is heated first. Pressing to form a flat layer. 6. According to the method for preparing the mouse pad according to the scope of claim 5, 11 200927492 wherein, in the step of heating and pressurizing, the fiber cloth is first heated by an oven, and then a roll is used. The rolling device pressurizes the fiber cloth. 7. The method according to claim 6, wherein the rolling device comprises a relatively normal temperature roller, and the fiber cloth is subjected to electricity and normal temperature. The roller is rolled between the rollers. 8. The method according to claim 1, wherein in the step of heating and pressurizing, the fiber is heated simultaneously by a hot pressing device. "" 9. The method of manufacturing a mouse pad according to claim 8 wherein the hot pressing device comprises a socket and a movable heat pressing plate, the fiber cloth is placed on the socket Heated plate heating According to the method for manufacturing a mouse pad according to claim 1, wherein the elastic system is made of a rubber material. 11. A method for preparing a mouse pad, the main steps of which include Take raw material: take unprinted pattern - mouse pad blank, the slip = 塾 blank contains - elastomer and cloth attached to the surface of the elastomer; heat pressurization. The surface of the fiber cloth is heated and applied with waste force, The fiber cloth is formed into a flat layer and a fiber layer; and the I7 brush prints a pattern on the flat layer of the fiber cloth, and is formed into a mouse pad having a clear printed pattern on the surface. In the step of the method of heating and refilling the mouse, the method of heating or adding ink is equal to or larger than the fiber 12 200927492 == Γ woven fabric "heating, so that the fiber on the surface of the fiber cloth is melted and pressed into a flat Layer 13. According to the scope of the patent application 丨 - .. ^ ^, 罘 11 items of the mouse pad method, - in the step of adding green plus, the use of a roll of the mouse pad while heating Pressure. The rolling device according to the claim 1 of the patent application scope includes the heating roller and the 加热. The mouse pad is made of a fiber cloth corresponding to the heating roller via the heating roller. The rollers at normal temperature are heated and rolled. 15. According to the method of patent application 帛U, the method of heating and pressing, in the step of heating and pressurizing, the surface of the fiber cloth is heated and then pressed to form a flat layer. 16. The method according to claim 15, wherein in the step of heating and pressurizing, the fiber cloth of the mouse squeegee material is first heated by an oven, and then rolled-rolled. The mouse pad blank is pressurized. 17. The method according to claim 16, wherein the rolling device comprises a second normal temperature roller, the mouse pad being rolled between two normal temperature rollers. 18. The method according to claim 5, wherein in the step of heating and pressurizing, the mouse pad blank is simultaneously heated and pressurized by a hot pressing device. 19. The method according to claim 18, wherein the hot pressing device comprises a socket and a movable heat pressing plate, and the mouse pad is placed on the bearing. The fiber cloth is heated and pressed by the hot platen. p 20. The method of applying the mouse pad according to the application of the patent, which is an elastic body made of a rubber material of the elastic system.
TW96150702A 2007-12-28 2007-12-28 Method of making mouse pad TW200927492A (en)