SU92973A1 - The method of hardening a joint welded by butt electrocontact welding - Google Patents

The method of hardening a joint welded by butt electrocontact welding

Info

Publication number
SU92973A1
SU92973A1 SU432711A SU432711A SU92973A1 SU 92973 A1 SU92973 A1 SU 92973A1 SU 432711 A SU432711 A SU 432711A SU 432711 A SU432711 A SU 432711A SU 92973 A1 SU92973 A1 SU 92973A1
Authority
SU
USSR - Soviet Union
Prior art keywords
welding
hardening
butt
joint
welded
Prior art date
Application number
SU432711A
Other languages
Russian (ru)
Inventor
А.В. Обухов
В.Б. Шляпин
пин В.Б. Шл
Original Assignee
А.В. Обухов
В.Б. Шляпин
пин В.Б. Шл
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.В. Обухов, В.Б. Шляпин, пин В.Б. Шл filed Critical А.В. Обухов
Priority to SU432711A priority Critical patent/SU92973A1/en
Application granted granted Critical
Publication of SU92973A1 publication Critical patent/SU92973A1/en

Description

Предлагаетс  способ упрочнени  соедине ;11Я, сваренного стыковой электроконтактной сваркой с повторным нагревол после сварки.A method is proposed for hardening a joint; 11I welded by butt electric contact welding with repeated heating after welding.

Известные способы электрокоитактной ссарки деталей ас обеснечнвают сварным соединени м механнческой прочности, разной прочности ocFiOBiioro металла.Known methods of electro-contact locking of parts of ac impure weld metal joints with mechanical strength and different metal ocFiOBiioro strengths.

При сварке особен ю резко понижаютс  предел усталости, ударна  в зкость li преде; прочности сварного шва.When welding, the fatigue limit is sharply reduced, the impact strength li is exceeded; strength of the weld.

Предлагаемый способ существенно повышает прочность п предел усталости сварного соединени  благодар  то.му, что соединение нагревают до 900-1100° п при этой температуре сварной стык онрессовывают с применением давлени  1,5-2 кг/лш1The proposed method significantly increases the strength n. The fatigue limit of the welded joint due to the fact that the joint is heated to 900-1100 ° n at this temperature, the welded joint is pressed using a pressure of 1.5-2 kg / lsh1.

После этого сварное соединение, в зависимости от требований дальнейше; эксплуатации, может быть подвергнуто термической илн ме.ханнческой обработке.After that, the welded joint, depending on the requirements further; operation, may be subjected to thermal or mechanical processing.

Термомехаиический способ упрочнени  сварного электроконтактного стыка может производитьс  как непосредственно в зажимах контактно-сварочных машин, так и вне машины, на которой производилась сварка.The thermomechanical method of hardening a welded electric contact joint can be carried out both directly in the terminals of resistance welding machines and outside the machine where the welding was performed.

Кроме повышени  прочности, нагрев с вторичным опрессованием унлотн ет сварной шов, ликвидиру  при этом пеплотность околошовной зоны, неизбежную при сварке обычным электроконтактным методом , устран   тем самым возможность развити  микротрешин в услови х в эксплуатации.In addition to increasing strength, heating with secondary crimping of the weld seam, while eliminating the heat density of the heat-affected zone, which is unavoidable during welding by the usual electrocontact method, thereby eliminating the possibility of microcrack development under operating conditions.

Предмет изо бретени Subject matter

Способ упрочнени  соединени , сваренного стыковой электроконтактной сваркой с повторным нагревам после сварки, отличаю№ 92973- 2 - щийс  тем, что соединение нагревают до 900- ператзфе сварной стык о рессовьпвают с ни  1,5-2 кг/мл1-. 1100 и лри этой темприменением давлеThe method of strengthening the joint welded by butt electric contact welding with reheating after welding, characterized in No. 92973-2, is that the joint is heated to 900 degrees and the weld joint is replaced with not 1.5-2 kg / ml1-. 1100 and with this pressure

Ш-.  Sh-.

SU432711A 1950-08-04 1950-08-04 The method of hardening a joint welded by butt electrocontact welding SU92973A1 (en)