SU83665A1 - A method of making electrical resistances with a negative temperature coefficient - Google Patents

A method of making electrical resistances with a negative temperature coefficient

Info

Publication number
SU83665A1
SU83665A1 SU342590A SU342590A SU83665A1 SU 83665 A1 SU83665 A1 SU 83665A1 SU 342590 A SU342590 A SU 342590A SU 342590 A SU342590 A SU 342590A SU 83665 A1 SU83665 A1 SU 83665A1
Authority
SU
USSR - Soviet Union
Prior art keywords
temperature coefficient
negative temperature
making electrical
electrical resistances
negative
Prior art date
Application number
SU342590A
Other languages
Russian (ru)
Inventor
А.А. Княжев
жев А.А. Кн
Original Assignee
А.А. Княжев
жев А.А. Кн
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.А. Княжев, жев А.А. Кн filed Critical А.А. Княжев
Priority to SU342590A priority Critical patent/SU83665A1/en
Application granted granted Critical
Publication of SU83665A1 publication Critical patent/SU83665A1/en

Description

Известные способы изготовлени  сопротивланпп с отрицательным температурным коэфф.ициентом обычно свод тс  -к опрессойке пцд давлением смеси ИЗОЛЯЦИОННОГО м нрювод щего материала, однако они не .обеспечивают получени  необходимого, достаточна большого отрлцательного температурного коэффициента.The known methods of making resistance with a negative temperature coefficient of the patient are usually reduced to pressure testing of the PSD with a mixture of INSULATING vibration material, but they do not provide the necessary, sufficiently large relative temperature coefficient.

Согласно предлагаемому спооэбу отпип,ательп1, телпер .ту- ibifi коэффициент сопроти1влеНИЙ, изгoтaвливлe ;ыx lio описыр/аемому способу , дохс1Д ит дю величины 2-3% на 1°.According to the proposed method, an otpip, aperp1, telper. Tut- ibifi coefficient conformed, manufactured, yo, lio to the descriptive / method, dahs1d and du of 2-3% by 1 °

Дл  изготовлени  со противланий ;в качестве основного rc o:bi-;iOio материала используетс  98-99% ма11 ет(итовой руды (гезО) и в чачестве св зующего (впослсйстви,и выгорающего) -.--2. речолытой ол(ты.For the manufacture of counterbalances; 98-99% of mantle (total ore (GeO) and as a binder (after burning)) are used as the main rc o: bi-; iOio material (and burnable) .

Указанна  смесь прессуетс  под да влением от ).2 до ( //гл;- ;; затем подвергаетс  термической обработке ,до спека:ни5 в вакуумных ил)1 газовых срсаах при 150-250°.This mixture is pressed under the pressure from) .2 to (// ch; - ;; then subjected to heat treatment, before sintering: under 5 in vacuum or) 1 gas srs at 150-250 °.

В определенном интервале температур со; ро7ив.-1ени  могут и-меть температурный коэффициент, по абсолютной величиж превосхоапщип температурные коэффициенты известных проводников ц полупроводников , и имеют удельное со1прютивлен|и.е при 16 в пределах ; 400 дo5.10 oлг/«fIn a certain temperature range co; Po.iv.-1eni may have a temperature coefficient, in absolute magnitude it exceeds the temperature coefficients of the known conductors of semiconductors and semiconductors, and they have a specific correlation | ie at 16 within; 400 to 5.10 Olga / "f

Г1 р с .1 л С Т И 3 О О ; г ; п /1Г1 р с .1 л С Т И 3 О О; g; p / 1

Способ изгоБОВленм  электр:ических сопротивлений с отрицатель-и-лм температурным коэффициентом на базе использовани  магнетитстоу руды, от л и ч а ю щи и с,  тем, что, с целью почыпкчнч  температурного коэффициента ,до величины 2-3% на 1°, смесь из магнет.нтовой руаы в количестве 98-99% и органической св зи в количестве --2% прессуют под давлен|ием 0,2-10 т/см- и спекают в вакуумной :и.;1и газовой среде при температуре, достаточной дл  выгорани  органической св зки.Electromagnetic resistance method with negative-and-lm temperature coefficient based on the use of magnetite ore, from l and h, and with the fact that, in order to obtain a temperature coefficient, to a value of 2-3% by 1 °, a mixture of magnet.nova rua in the amount of 98-99% and organic bond in the amount of -2% is pressed under pressure of 0.2-10 t / cm and is sintered in a vacuum: i.; 1 and gaseous medium at a temperature sufficient to burn organic binder.

SU342590A 1938-11-23 1938-11-23 A method of making electrical resistances with a negative temperature coefficient SU83665A1 (en)