SU654587A1 - Method of manufacturing concrete articles - Google Patents
Method of manufacturing concrete articlesInfo
- Publication number
- SU654587A1 SU654587A1 SU772546285A SU2546285A SU654587A1 SU 654587 A1 SU654587 A1 SU 654587A1 SU 772546285 A SU772546285 A SU 772546285A SU 2546285 A SU2546285 A SU 2546285A SU 654587 A1 SU654587 A1 SU 654587A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- manufacturing concrete
- concrete articles
- articles
- concrete
- manufacturing
- Prior art date
Description
ние 15 ати и поддерживают его 20 мин, затем давление снижают до нормального в течение 2 мин.15 API and maintain it for 20 minutes, then reduce the pressure to normal for 2 minutes.
Результаты испытаний образцов следующие:The test results of the samples are as follows:
Объемна масса бетона , кг/мVolume of concrete mass, kg / m
после пропаривани 2200-2330 через 28 суток (с пропиткой )2320-2350 Прочность при сжатии , кгс/смafter steaming 2200-2330 after 28 days (impregnated) 2320-2350 Compressive strength, kgf / cm
после пропаривани 98-180after steaming 98-180
через 28 суток (с пропиткой )250-305 Водонепроницаемость,after 28 days (with impregnation) 250-305 Waterproof,
кгс/см 3-15kgf / cm 3-15
Пропитка под давлением цементной суспензией позвол ет повысить прочность при сжатии через 28 суток на 20% при расходе цемента 240-300 кг/см и на 50-60% при расходе цемента 193 кг/м бетона. Эффективность пропитки тем больше, чем меньшеImpregnation of cement slurry under pressure makes it possible to increase compressive strength after 28 days by 20% with cement consumption of 240-300 kg / cm and by 50-60% with cement consumption of 193 kg / m concrete. The effectiveness of the impregnation is greater than less
расход цемента на 1 м бетона. Водонепроницаемость бетона повышаетс в 3-6 раз.cement consumption per 1 m of concrete. The water resistance of concrete is increased by 3-6 times.
Claims (2)