SU61837A1 - The method of obtaining soluble varnish resin - Google Patents

The method of obtaining soluble varnish resin

Info

Publication number
SU61837A1
SU61837A1 SU29787K SU29787K SU61837A1 SU 61837 A1 SU61837 A1 SU 61837A1 SU 29787 K SU29787 K SU 29787K SU 29787 K SU29787 K SU 29787K SU 61837 A1 SU61837 A1 SU 61837A1
Authority
SU
USSR - Soviet Union
Prior art keywords
varnish resin
obtaining soluble
soluble varnish
resin
maleic anhydride
Prior art date
Application number
SU29787K
Other languages
Russian (ru)
Inventor
А.М. Брусиловский
Original Assignee
А.М. Брусиловский
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from SU29787A external-priority patent/SU61084A1/en
Application filed by А.М. Брусиловский filed Critical А.М. Брусиловский
Application granted granted Critical
Publication of SU61837A1 publication Critical patent/SU61837A1/en

Description

Высока  склонность терпенов к изомеризации под действием нагрева , окислителей и других факторов позвол ет рассчитывать на соединение с малеиновым ангидридом не только тех терпенов, которые заведомо имеют сопр женные двойные св зи, но и тех, которые в обычном своем виде таких св зей не имеют.The high tendency of terpenes to isomerize under the action of heat, oxidizing agents and other factors makes it possible to rely on the connection with maleic anhydride not only to those terpenes that obviously have conjugated double bonds, but also to those that do not normally have such bonds.

Согласно изобретению, предлагаетс  использовать это свойство терпенов дл  получени  спирторастворимых смол путем соединени  живицы или скипидара или пинена, терпинена, мирцена с малеиновым ангидридом с последующим введением в соединение мочевины. Получаема  при этом красновата  тверда  хрупка  смола отлично раствор етс  в спиртах, дава  при высыхании прочные, светлые, эластичные и блест щие пленки.According to the invention, it is proposed to use this property of terpenes to obtain alcohol-soluble resins by combining sap or turpentine or pinene, terpinene, myrcene with maleic anhydride, followed by the introduction of urea into the compound. The resulting reddish, hard, brittle resin is highly soluble in alcohols, giving strong, light, elastic and glossy films upon drying.

Пример. 50 г. пинена нагревают в течение 2 час при температуре 160-170° с 36 3 малеинового ангидрида, после чего добавл ют к сплаву 22 г мочевины, продолжа  далее варку еще 3-5 час. Полученную смолу раствор ют в спирте, получа  готовый спиртовой лак.Example. 50 g of pinene is heated for 2 hours at a temperature of 160-170 ° C with 36 3 maleic anhydride, after which 22 g of urea is added to the alloy, continuing further cooking for another 3-5 hours. The resulting resin is dissolved in alcohol to form a finished alcohol varnish.

Предмет изобретени Subject invention

Способ получени  лаковых смол на основе продуктов взаимодействи  терпеновых углеводородов с малеиновым ангидридом, отличающийс  тем, что, в цел х получени  спирторастворенной смолы, к сплаву живицы, скипидара, пинена, терпигена или мирцена с малеиновым ангидридом добавл ют мочевину и сплав подвергают дальнейщему нагреванию .A method of producing lacquer resins based on the reaction products of terpene hydrocarbons with maleic anhydride, characterized in that, in order to obtain an alcohol-soluble resin, urea is added to the resin resin, turpentine, pinene, terpigena or mycene with maleic anhydride and the alloy is further heated.

Редактор В. Е. Гридчин Техред А. А. Камышникова Корректор С. Ю. ЦверннаEditor V. E. Gridchin Tehred A. A. Kamyshnikov Proofreader S. Yu. Tzvernn

Подп. к печ. Ю/ХП-61 г. . Формат бум. 70 X ЮЭ/ш.Объем 0,09 изд. л.Sub. to pec. U / HP-61 g. Format boom. 70 X JE / w. Volume 0.09 ed. l

Зак. 314.3/13.Тираж 220.Цена 2 коп.Zak 314.3 / 13. Circulation 220. Price 2 cop.

ЦБТИ при Комитете по делам изобретений и открытийTsBTI under the Committee on Inventions and Discoveries

при Совете Министров СССР Москва, Центр, М.-Черкасский пер., д. 2/6.Under the Council of Ministers of the USSR, Moscow, Center, M.-Cherkassky Lane, 2/6.

Типографи , пр. Сапунова, 2.Printing house, Sapunova Ave., 2.

SU29787K 1940-02-13 1940-02-13 The method of obtaining soluble varnish resin SU61837A1 (en)