SU55719A1 - Method of briquetting raimki - Google Patents

Method of briquetting raimki

Info

Publication number
SU55719A1
SU55719A1 SU18649A SU18649A SU55719A1 SU 55719 A1 SU55719 A1 SU 55719A1 SU 18649 A SU18649 A SU 18649A SU 18649 A SU18649 A SU 18649A SU 55719 A1 SU55719 A1 SU 55719A1
Authority
SU
USSR - Soviet Union
Prior art keywords
briquetting
briquettes
raimki
presses
current
Prior art date
Application number
SU18649A
Other languages
Russian (ru)
Inventor
Н.С. Загребельный
Original Assignee
Н.С. Загребельный
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Н.С. Загребельный filed Critical Н.С. Загребельный
Priority to SU18649A priority Critical patent/SU55719A1/en
Application granted granted Critical
Publication of SU55719A1 publication Critical patent/SU55719A1/en

Description

Предлагаемый способ брикетирозани  раймовки цинкодестилл ционных .заводов состоит в том, что отвальна  раймовка смешиваетс  с текущей и предварительно подвергаетс  грохочению, с целью отделени  кирпичных выломок, кусков глины, которые посто нно наход тс  в раймовке в незначительном количестве .The proposed method of briketyrozani for the distribution of zinc pre-distillation plants is that the dump area is mixed with the current and is preliminarily screened, in order to separate the brick fragments, pieces of clay, which are constantly in the district in small quantities.

Дл  этой цели примен етс  грохот с отверсти ми в 25 мм. Отсев крупной фракции составл ет около 15-20% и зависит от тщательности разделени  раймовки и других материалов во врем  текущего ремонта печи.A screen with 25 mm holes is used for this purpose. The screening of the coarse fraction is about 15-20% and depends on the thoroughness of the separation of the raim and other materials during the current repair of the furnace.

Просе нна  раймовка подвергаетс  измельчению на вальцевой мельнице -и просеиваетс  через сито 3 миллиметра . Крупна  часть возвращаетс  на варки, а мелочь увлажн етс  до 8-10, перемешиваетс  в обычной лопастной мешалке и поступает на брикетирование.The sifting gauge is crushed on a roller mill — and sieved through a 3 mm sieve. The bulk is returned to the cooking, and the fines are moistened to 8-10, mixed in a conventional paddle stirrer and fed to briquetting.

Дл  брикетировани  раймовки могут быть использованы пресса, примен емые дл  прессовки кирпича по сухому способу, т. е. пресса типа ,,Байдо, „Шпенглера и др.For briquetting raits, presses used for pressing bricks by the dry method, i.e., Baido, Spengler and other presses can be used.

Размер брикетов должен определ тьс  требовани ми ватер-жакетной плавки. Наиболее желательным  вл етс  размер брикетов 70 X 70 мм, В отнощении формы брикета требований никаких нет, но очевидно, что округленна  форма -  йцевидна  - будет давать меньше мелочи, чем кубическа  или цилиндрическа  форма, имеюща  острые грани; однако, получить округленную форму на прессах указанного выше типа (изготовл емых в СССР) не представл етс  возможным. После пресса брикеты осторожно складываютс  в специальные вагонетки или на медленно движущийс  транспортер вдоль прессов, с тем, чтобы брикеты могли оставатьс  на ленте или в вагонетке без перегрузки около 3 часов. За это врем  брикеты разогреваютс  за счет окислени  железа и схватываютс  настолько, что могут разгружатьс  в бункер или складыватьс  в открытые щтабел . Весь процесс схватывани  брикетов продолжаетс  около 12 часов.The size of the briquettes should be determined by the requirements of the waterjack fusion. The most desirable is the size of briquettes 70 x 70 mm. There are no requirements with respect to the shape of the briquette, but it is obvious that a rounded shape - ovoid - will give less fines than a cubic or cylindrical shape that has sharp edges; However, it is not possible to obtain a rounded shape on presses of the type indicated above (manufactured in the USSR). After the press, the briquettes are carefully folded into special trolleys or on a slow moving conveyor along the presses so that the briquettes can remain on the belt or in the trolley without overloading for about 3 hours. During this time, the briquettes are heated by the oxidation of iron and set so much that they can be unloaded into a bunker or put into open shtabel. The whole process of setting the briquettes lasts about 12 hours.

Желательно, чтобы первые три часа после прессовани  брикеты находились при температуре 40-50°,It is desirable that the first three hours after pressing the briquettes were at a temperature of 40-50 °,

что. -ускор ет процесс схватывани  брикетов.what. -accelerate the process of setting briquettes.

По указанию изобретател , наилучший результат дает смесь отвальной и текущей раймовок, в которой содержание отвальной раймовки не превосходит 30%. При большем содержании отвайьной раймовки прочность брикетов понижаетс .According to the instructions of the inventor, the best result is given by a mixture of the dump and the current ramovok, in which the content of the raft ravine is less than 30%. With a higher content of wavy ravine, the strength of the briquettes decreases.

Предмет наобрете.ни .Subject to purchase.

Способ брикетировани  раймовки, отличающийс  тем, что отвальную раймовку смешивают в надлежащей пропорции с текущей, увлажн ют и прессуют в брикет, который подвергают сушке.The method of briquetting the racks, characterized in that the waste racks are mixed in proper proportion with the current one, moistened and pressed into a briquette, which is subjected to drying.

SU18649A 1938-08-31 1938-08-31 Method of briquetting raimki SU55719A1 (en)