SU523944A1 - Environment for quenching metals - Google Patents

Environment for quenching metals

Info

Publication number
SU523944A1
SU523944A1 SU2063754A SU2063754A SU523944A1 SU 523944 A1 SU523944 A1 SU 523944A1 SU 2063754 A SU2063754 A SU 2063754A SU 2063754 A SU2063754 A SU 2063754A SU 523944 A1 SU523944 A1 SU 523944A1
Authority
SU
USSR - Soviet Union
Prior art keywords
quenching
environment
medium
metals
quenching metals
Prior art date
Application number
SU2063754A
Other languages
Russian (ru)
Inventor
Анатолий Васильевич Толстоусов
Иван Георгиевич Дружинин
Цунжар Мумузовна Касымова
Original Assignee
Предприятие П/Я В-8843
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я В-8843 filed Critical Предприятие П/Я В-8843
Priority to SU2063754A priority Critical patent/SU523944A1/en
Application granted granted Critical
Publication of SU523944A1 publication Critical patent/SU523944A1/en

Description

(34) СРЕДА ДЛЯ ЗАКАЛКИ МЕТАЛЛОВ(34) ENVIRONMENT FOR HANGING METALS

Изобретение отнсх;итс  к закалочным ере дам, примен емым при термической обработке .  The invention is related to the quenching processes used during heat treatment.

Известные закалоч1изш среды на водной основе с добавками различных солей и ще- почей, обеспечивающие получение высокой твердости, НС предотвращают трещинообрв зование i, 2,The known water-based quenching medium with the addition of various salts and glands, ensuring high hardness, NS prevents the cracking of i, 2,

Известна закалочна  среда, представл ю- ; ща  собой водный раствор поливинилового cnup-i та уЗ, Однако она не предотвращает тре- шинообразовани  при объемной закалке и при содержании в растворе более 1% поливинилового спирта издели  имеют пониже кую твердость.  A quenching medium is known, which is a yu; However, it does not prevent cracking during bulk quenching and when the content in the solution is more than 1% polyvinyl alcohol, the products have a lower hardness.

С целью предотвращени  трещинообразо- , вави  предлагаема  закалочна  среда дополнительно додержит сульфитно-спиртовой щелок при слещюшем соотношении компонентов (в об, %)In order to prevent tarnish-like, Vavi, the proposed quenching medium additionally contains sulphite-alcohol lye at the following ratio of components (in vol.%)

j Сулы|знтно-спиртовой шелок 5-60 Вода,Остальноеj Suly | silk alcohol silk 5-60 Water, the rest

Предложенна  закш Очна  среда повыша;ет скорость охлаждени  в интервале тек ператур иаммеиьшей устойчивости переохлаАiiieinjoro аустенита и замедл ет ее в интврвале температур мартенситного превращений.The proposed liquidation medium increases the cooling rate in the range of temperatures and the worse resistance of the austenite to the freezing point and slows it down in the temperature range of the martensitic transformations.

При закалке пластин приводных роликовых цепей шага 25,4 мм из стали 50 и роликов этой же цепи из стали 65 Г в опвн .сываемой среде с содержанием 18% сулг |фитно-спартового щелока онн имели твердост 56-58 и 60-61 HRC соответственно при (Отсутствии трещин. После закалк детали iимели чистую светлую поверхность, не ну дающуюс  в дополнительной очистке.When quenching the plates of drive roller chains of a pitch of 25.4 mm from steel 50 and rollers of the same chain from steel 65 G in an open medium with a content of 18% sulg | fit-spart liquor, onn had a hardness of 56-58 and 60-61 HRC, respectively at (No cracks. After hardening, the parts have a clean, bright surface that does not need additional cleaning.

1 В процессе работы закалочна  среда стйб 1г1ьна и не мен ет своих свойств в интервале температур 28-10О С.1 In the process, the quenching medium is styb 1g1na and does not change its properties in the temperature range 28-10 ° C.

ФормулFormulas

изобретени the invention

Среда дл  закалки металлов, содержатс  воду, , о т л и ч а io ща  с  . тем, что, р целью предотвращени  трешипообразовани , она дополнительно содержит сульфитио-спирТ08ОЙ ишлок при следующем соотношенииI, Л, В. Петраш, Закалочные среды,A medium for the quenching of metals, contains water. By the fact that, in order to prevent cracking, it additionally contains sulphito-alcohol Alkyl-8 in the following ratios I, L, V. Petrash, quenching media,

Iкомпонентов, об. %: Машгиа, 1959, 57.I components, about. %: Mashgia, 1959, 57.

Сульфитно-спиртовой (щелок 5-602. Авт. св. СССР № 104597,, М. кл.Sulfite-alcohol (lye 5-602. Auth. St. USSR № 104597, M. class.

Вода Остальное Q 21D l/60j 1955 г (аналог).Water Else Q 21D l / 60j 1955 g (equivalent).

Источника инфсфмааиИ| щ  н гыв во 3. РЖ Металлурги  1973 г. № 6jSource of information | shch n gyv 3. RZh Metallurgi 1973 № 6j

-мание Ери экспертизе: :реф. Б246 (прототип).-Mania Eri examination:: ref. B246 (prototype).

523944523944

SU2063754A 1974-09-30 1974-09-30 Environment for quenching metals SU523944A1 (en)