SU482403A1 - Стекло - Google Patents
СтеклоInfo
- Publication number
- SU482403A1 SU482403A1 SU1983793A SU1983793A SU482403A1 SU 482403 A1 SU482403 A1 SU 482403A1 SU 1983793 A SU1983793 A SU 1983793A SU 1983793 A SU1983793 A SU 1983793A SU 482403 A1 SU482403 A1 SU 482403A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- glass
- sealing
- semiconductor devices
- aloz1
- 20cdo1
- Prior art date
Description
1
Изобретение касаетс стекла, используемого в электронной технике.
Известны стекла, включающие 6263, ZnO, SiOa, АЬОз, СаО, MgO и CdO.
Известные стекла мало пригодны дл герметизации полупроводниковых приборов.
Данное изобретение позвол ет осуществл ть качественную герметизацию электронных приборов.
Достигаетс это тем, что стекло содержит указанные компоненты в следующих количествах , вес. %:
ВгОз 25-50СаО1-15
ZnO30-45MgO 0,1 - 10
SiOg1-20CdO1 - 10
АЬОз1 - 15
При применении данного стекла качественна герметизаци достигаетс за счет низкого коэффициента линейного термического расширени , пониженной температуры спаивани , повышенной химической устойчивости, малой склонности к кристаллизации.
Кроме того, стекло обладает хорошими выработочными свойствами.
Мала склонность к кристаллизации позвол ет вырабатывать данное стекло в виде капилл ров. Оно обеспечивает герметизацию полупроводниковых приборов при температурах 700-800°С.
Реальность получени стекла подтверждаетс конкретными примерами.
Дл бескорпусной герметизации кремниевых полупроводниковых приборов с молибденовыми вводами может быть рекомендован следующий конкретный состав стекла, обладающий следующими свойствами.
Пример
ВгОз41,3АЬОз6,6
ZnO32,2СаО7,4
SiOa4,0CdO8,4
Коэффициент линейного термического расширени , град-152-10Температура деформации, °С595
Температура оплавлени , °С720
Химическа устойчивость
(гидролитический класс)1
Предмет изобретени
Стекло, включающее В2Оз, ZnO, SiOz, , СаО, MgO и CdO, отличающеес тем, что, с целью герметизации полупроводниковых приборов, оно содержит указанные компоненты в следующих количествах, вес. %: ВгОз 25-50СаО1-15
ZnO30-45MgO 0,1-10
SiOa1-20CdO1-10
АЬОз1 - 15