SU47812A1 - Method of attaching a rubber sole to a shoe and a press for gluing a rubber sole to leather shoes - Google Patents

Method of attaching a rubber sole to a shoe and a press for gluing a rubber sole to leather shoes

Info

Publication number
SU47812A1
SU47812A1 SU154679A SU154679A SU47812A1 SU 47812 A1 SU47812 A1 SU 47812A1 SU 154679 A SU154679 A SU 154679A SU 154679 A SU154679 A SU 154679A SU 47812 A1 SU47812 A1 SU 47812A1
Authority
SU
USSR - Soviet Union
Prior art keywords
sole
rubber
glue
shoe
press
Prior art date
Application number
SU154679A
Other languages
Russian (ru)
Inventor
Д.Ю. Берман
В.В. Кругов
Е.А. Нисневич
А.И. Позняк
к А.И. Позн
Б.С. Рабинович
Original Assignee
Д.Ю. Берман
В.В. Кругов
Е.А. Нисневич
А.И. Позняк
к А.И. Позн
Б.С. Рабинович
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Д.Ю. Берман, В.В. Кругов, Е.А. Нисневич, А.И. Позняк, к А.И. Позн, Б.С. Рабинович filed Critical Д.Ю. Берман
Priority to SU154679A priority Critical patent/SU47812A1/en
Application granted granted Critical
Publication of SU47812A1 publication Critical patent/SU47812A1/en

Description

Предлагаемый способ, имеющий целью значительно сократить врем  приклейки и прессовки, повысив тем производительность , приобретает особое значение в виду того, что, согласно вырабо .танному дл  обувной промышленности производственному плану, предположен но выпустить до от всего выпуска обуви с резиновыми подошвами. Хот  способ прикреп.1ени  резиновой подошвы к кожаному верху помощью приклейки (в отличие от механических способов пришивки и привинчивани ) сам по себе не представл ет , но предлагаемые в нескольких вариантах приемы приклейки не наруша  проч ности приклейки и не вред  кожаному верху, обеспечивают ускорение процесса, что вполне подтверждаетс  специальными опытами, произведенными на Московской фабрике „Парижска  Коммуна , котора  с ма  м-ца .19Ь5 г. выпускает по предлагаемому способу около 1500 пар обуви ежедневно.The proposed method, which aims to significantly shorten the gluing and pressing times, thereby increasing productivity, is of particular importance in view of the fact that, according to the production plan for the shoe industry, it is expected to be released before the entire production of rubber-soled shoes. Although the method of attaching a rubber sole to a leather upper by gluing (as opposed to mechanical methods of sewing and screwing) does not in itself, but the gluing methods offered in several versions do not damage the durability of the gluing and do not harm the leather upper, accelerate the process. which is fully confirmed by the special experiments carried out at the Moscow factory of the Paris Commune, which since May 1965 produced, according to the proposed method, about 1,500 pairs of shoes every day.

Сущность способа заключаетс  в применении гор чей вулканизации дл  склеивани  с кожаным верхом резиновой или гуттаперчевой пленки, причем особенно благопри тные результаты получаютс  при применении кле  из советской гуттаперчи, которой, однако , нехватает дл  удовлетворени  всей потребности, так что необходимо изыскать другие кле щие материалы. Характерной особенностью предложени , существенно отличающей его от уже известных,  вл етс  применение таких приемов составлени  и промазывани  клеем, при которых высока  температура вулканизации, вредна  дл  кожи, ограничиваетс  пределами подошвы и приклеивающей пленки, не каса сь кожи, дл  чего предназначены прессы, специально сконструированные дл  o3Ha4eHiioA цели, которые изображены в трех вариантах на прилагаемом чертеже (фиг. 1, 2 и 3).The essence of the method is the use of hot vulcanization for bonding a rubber or gutta-percha film to the leather upper, and particularly favorable results are obtained when using glue from Soviet gutta-percha, which, however, is not enough to satisfy all needs, so it is necessary to find other adhesive materials. A characteristic feature of the proposal, which significantly distinguishes it from the already known ones, is the use of such methods of making and coating with glue, in which a high temperature of vulcanization, harmful to the skin, is limited to the limits of the sole and adhesive film, not touching the skin, for which presses are designed, specially designed for o3Ha4eHiioA, the targets are shown in three versions in the attached drawing (Fig. 1, 2 and 3).

За вленный способ предлагаетс  в п ти вариантах:The claimed method is offered in five variants:

1-й вариант (гор ча  вулканизаци ) состоит в том, что на подошву намазывают последовательно три сло  резинового кле , из которых первые два содержат в своем составе серу, ускорители и активаторы вулканизации, а третий таковых не содержит, после чего подошву, нагретую в термостате до 135-140°, накладывают на ботинок, зат жна  кромка которого предварительно промазываетс  несколькими сло ми кле , содержащего также серу, ускорители и активаторы вулканизации, и прессуют.The first variant (hot vulcanization) consists in the fact that three layers of rubber glue are successively spread on the sole, the first two of which contain sulfur, accelerators and vulcanization activators, and the third does not contain those, after which the sole heated in thermostat up to 135-140 °, is applied to the shoe, the tightening edge of which is pre-coated with several layers of glue, which also contains sulfur, accelerators and vulcanization activators, and pressed.

2-ой вариант (полугор ча  вулканизаци ) состоит в том, что к резиновому клею прибавл ют ультраускорители и прогревают не всю подошву, а только кле щую пленку, что позвол ет сократить длительность процесса вулканизации до 0,5-1 минуты.The second variant (semi-vulcanization) consists in adding ultra-accelerators to the rubber glue and heating not the entire sole, but only the adhesive film, which reduces the duration of the vulcanization process to 0.5-1 minutes.

3-й вариант (полувулканизаци ) состоит в том, что клей до нанесени  его на подошву и кожу частично вулканизуетс , причем процесс вулканизации заканчиваетс  при прессовании.The third option (semi-vulcanization) is that the adhesive is partially vulcanized before it is applied to the sole and the skin, and the vulcanization process ends when it is pressed.

4-й вариант, примен емый ко второму варианту, состоит в том, что на кожу вместо резинового кле  наноситс  гуттаперчевый, который разм гчаетс  при соприкосновении с гор чей вулканизованной резиновой подошвой .The 4th variant, applied to the second variant, consists in applying gutta-percha instead of rubber glue, which softens upon contact with a hot vulcanized rubber sole.

5-й вариант состоит в том, что дл  нанесени  на кожу и резину приК1ен етс  смесь гуттаперчи и резинового кле  в количестве до 50% от веса гуттаперчевого кле . Метод работы соответствует методу склеивани  гуттаперчевым клеем, причем повышаетс  термоустойчивость кле .The 5th option is that a mixture of gutta-percha and rubber glue in an amount of up to 50% by weight of gutta-percha glue is applied to the skin and gum. The method of operation corresponds to the method of gluing with gutta-percha glue, and the heat resistance of the glue increases.

Прессы дл  гор чей вулканизации, предлагаемые в трех вариантах, по общей своей конструкции ничем существенно не отличаютс  от общеизвестных , так как состо т из прессовой коробки, откидного хомута, зат жного рычага с ручкой и упоров, прижимающих колодку к прессовой коробке. Характерной Отличител ной особенностью  вл етс  устройство прессовых короток.The presses for hot vulcanization, offered in three versions, are not significantly different from the generally known ones, as they consist of a press box, a folding strap, a tightening lever with a handle and stops that press the pad to the press box. A distinctive feature is the press device is short.

В прессе по 1-му варианту (фиг. 1) прессова  железна  коробка, св занна  с отки 1НЫМ хомутом 5 и зат жным рычагом с ручкой 1, покрываетс  гибкой мембраной 2, состо щей из прорезиненной ткани и кожи, поверх которой кладетс  изолирующий асбестовый слой 3, а поверх последнего-электронагреватель 6, состо щий из переплетени  асбестового шнура с нихромом. При пропускании через него электрического тока получаетс  нагревание резиновой подошвы и сло  кле , нанесенного на зат жную кромку ботинка, дл  создани  же необходимого давлени , прижимающего подошву к зат жной кромке во всех точках их поверхности, служат вода или воздух, нагнетаемые через трубку 4 в коробку, покрытую гибкой мембраной 2. Когда подошва приклеилась , а пленка завулканизовалась, через трубу 4 выпускают воздух или воду, давление падает, откидной рычаг с ручкой 1 откидываетс , хомут 5 такжо, а ботинок с приклеенной подошвой вынимаетс  вместе с колодкой из пресса.In the press according to the 1st version (Fig. 1), the press iron box connected to the roll with the 1N clamp 5 and the tightening lever with the handle 1 is covered with a flexible membrane 2 consisting of rubberized fabric and leather on top of which an insulating asbestos layer is laid 3, and on top of the latter, an electric heater 6, consisting of interweaving an asbestos cord with nichrome. By passing an electric current through it, the rubber sole and glue applied to the pulling edge of the shoe are heated, and to create the necessary pressure, which presses the sole to the pulling edge, water or air pumped through the tube 4 into the box at all points on their surface. covered with flexible membrane 2. When the sole is glued and the film is cured, air or water is released through pipe 4, the pressure drops, the folding lever with handle 1 leans out, clamp 5 is also attached, and the shoe with glued sole aets with the shoe of the press.

В прессе по 2-му варианту (фиг. 2) характерной отличительной особен ностью служит то, что нагревание и создание необходимого давлени  производитс  паром, впускаемым в коробку через трубу 4, в св зи с чем мембрана из ткани замен етс  тонким листом красной меди, а надобность в электронагревателе отпадает.In the press according to the 2nd version (Fig. 2), a characteristic feature is that the heating and the creation of the necessary pressure are produced by steam introduced into the box through pipe 4, and therefore the fabric membrane is replaced with a thin sheet of red copper, and the need for an electric heater is eliminated.

В прессе по 3-му варианту (фиг. 3) отличительной особенностью устройства коробки  вл етс  то, что вместо гибкой мембраны из ткани или меди применена бронзова  рама 6, изготовленна  по профилю колодки и низа ботинка, причем она служит также и нагревателем при помощи впускаемого в прессовую коробку пара.In the press according to the 3rd variant (Fig. 3), a distinctive feature of the box device is that instead of a flexible fabric or copper membrane, a bronze frame 6, made along the profile of the pad and the bottom of the boot, is used, and it also serves as a heater using the inlet in the steam box press.

Наиболее пригодным за вители считают применение способа по 2-му ваj рианту, так как он может производитьс  при помощи любого пресса, не требует обогрева, сокращает врем  прессовани  до одной и, максимум, двух минут и дает значительную экономию в стоимости оборудовани  и в размерах производственной площади, вследствие чего и проведен в жизнь, какThe applicants consider the use of the method according to the 2nd version as the most suitable, since it can be produced using any press, does not require heating, shortens the pressing time to one and maximum two minutes, and provides significant savings in equipment cost and production costs. area, as a result of which,

упоминалось, на фабрике „Парижска  Коммуна.mentioned in the factory of the Paris Commune.

Предмет изобретени .The subject matter of the invention.

Claims (8)

1.Способ прикреплени  резиновой подошвы к обуви, отличающийс  тем, что на резиновую подошву намазывают два сло  резинового кле , содержащего серу, ускорители и активаторы вулканизации , и покрывают третьим слоем резинового кле , не содержащего в своем составе серы, ускорителей и активаторов , после чего подошву подогревают до 135-140° и в гор чем состо нии накладывают на ботинок, зат жную кромку коего промазывают предварительно несколькими сло ми резинового кле , содержащего серу, ускорители и активаторы вулканизации, и спрессовывают по-обычному.1. A method of attaching a rubber sole to a shoe, characterized in that two layers of rubber glue containing sulfur, accelerators and vulcanization activators are spread on the rubber sole and covered with a third layer of rubber glue that does not contain sulfur, accelerators and activators, after which the sole is heated to 135-140 ° and, in a hot condition, is placed on the shoe, the tightening edge of which is pre-coated with several layers of rubber glue containing sulfur, accelerators and vulcanization activators, and pressed together. ychnomu. 2.Видоизменение способа согласно п. 1, отличающеес  тем, что к резиновому клею прибавл ют ультраускорители и прогревают не всю подошву, а только кле щую пленку в течение 30-60 секунд.2. A variation of the method according to claim 1, characterized in that ultra-accelerators are added to the rubber glue and heat not the entire sole, but only the adhesive film for 30-60 seconds. 3.Видоизменение способа по п. 1, отличающеес  тем, что подошву подогревают в процессе прессовани .3. A variation of the method according to claim 1, characterized in that the sole is heated during the pressing process. 4.Прием выполнени  способа по п. 1, отличающийс  тем, что на кожу вместо резинового кле  нанос т гуттаперчевый клей.4. A method according to claim 1, characterized in that gutta-percha glue is applied to the skin instead of rubber glue. 5.Прием выполнени  способа по п. 1, отличающийс  тем, что дл  приклеивани  подошвы примен ют смесь каучукового и гуттаперчевого кле .5. A method of carrying out the method according to claim 1, characterized in that a mixture of rubber and gutta-percha glue is used to glue the sole. 6.Пресс дл  приклеивани  резиновой подошвы к обуви, отличающийс  тем, что он снабжен мембраной из волокнистого материала, поверх которой расположен а сбестовый слой 3 и электронагреватель 6 (фиг. I).6. A press for gluing the rubber sole to the shoe, characterized in that it is provided with a membrane made of fibrous material, above which is the rebate layer 3 and the electric heater 6 (Fig. I). 7.Видоизменение охарактеризованного в п. б пресса, отличающеес  тем, что мембрана 2 выполнена из листовой красной меди и представл ет собою призму паровой коробки (фиг. 2Л7. Alteration of a press characterized in paragraph b, characterized in that the membrane 2 is made of red copper sheet and represents the prism of a steam box (Fig. 2L 8.Видоизменение охарактеризованного в п. 7 пресса, отличающеес  тем, что он состоит из обогреваемой паром коробки с бронзовой рамой, изготовленной по профилю ботинка (фиг. 3).8. Alteration of the press described in paragraph 7, characterized in that it consists of a steam heated box with a bronze frame made along the profile of the shoe (Fig. 3). .:.: ..
SU154679A 1935-09-29 1935-09-29 Method of attaching a rubber sole to a shoe and a press for gluing a rubber sole to leather shoes SU47812A1 (en)