SU468888A1 - Способ очистки щелочно-алюминатных растворов - Google Patents

Способ очистки щелочно-алюминатных растворов

Info

Publication number
SU468888A1
SU468888A1 SU1824738A SU1824738A SU468888A1 SU 468888 A1 SU468888 A1 SU 468888A1 SU 1824738 A SU1824738 A SU 1824738A SU 1824738 A SU1824738 A SU 1824738A SU 468888 A1 SU468888 A1 SU 468888A1
Authority
SU
USSR - Soviet Union
Prior art keywords
solution
iron
sodium sulfite
aluminate solutions
alkaline aluminate
Prior art date
Application number
SU1824738A
Other languages
English (en)
Inventor
Анатолий Иванович Бахтеев
Александр Иванович Савченко
Лидия Михайловна Скрябнева
Ольга Даниловна Герасимова
Original Assignee
Предприятие П/Я В-8407
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я В-8407 filed Critical Предприятие П/Я В-8407
Priority to SU1824738A priority Critical patent/SU468888A1/ru
Application granted granted Critical
Publication of SU468888A1 publication Critical patent/SU468888A1/ru

Description

1
Изобретение относитс  к производству глинозема , в частности к стадии очистки щелочных и алюминатно-щелочных растворов от примесей железа.
Известен способ очистки щелочно-алюминатных растворов от примесей железа путем введени  в раствор окиси кальци  с последующей фильтрацией через слой адсорбента.
Предлагаемый способ отличаетс  от известного тем, что с целью интенсификации процесса , т. е. повышени  степени очистки в исходный раствор добавл ют сульфит натри  в количестве 0,5-10 гл.
Пример 1. В раствор с концентрацией 300 г/л NaaO, 150 г/л АЬОз и 5 г/л ЗЛ св занной в сульфид натри , содержащий соединение железа 0,48 г/л в виде Ре20з, ввод т окись кальци  (5 г/л) и сульфит натри  (2 г/л). Железо из раствора переходит в осадок , который отдел ют известными способами фильтрации. С добавкой окиси кальци  и сульфита натри  концентрацию железа в растворе снижают в два раза, что составл ет 0,24 г/л РеаОз. (без добавки сульфита натри  содержание Ре20з 0,48 г/л).
Пример 2. В раствор с концентрацией 150 г/л NaaO, 75 г/л АЬОз и 2,5 г/л S-, св занной в сульфид натри , содержащий соединени  железа 0,24 г/л в виде Ре20з, ввод т окись кальци  (2,5 г/л) и сульфит натри  (I г/л). Концентрацию железа в растворе снижают до 0,003 г/л Ре2Оз. Без добавки сульфита натри  содержание железа в растворе составл ет 0,24 г/л Ре2Оз.
Пример 3. Сернистый боксит с известью 5% выщелачивают в автоклавах алюминатнощелочным раствором, полученную суспензию разбавл ют растворами от промывки щлама до концентрации 130-150 г/л Na2O и АЬОз и при перемещивании добавл ют сульфит натри  в количестве 1-2 г/л. Раствор от шлама отдел ют декантацией и производ т кон7рольную фильтрацию через слой целлюлознобумажной массы. Содержание Ре2Оз в полученном растворе составл ет 0,003 г/л. Без добавки сульфита натри  содержание железа в растворе составл ет 0,24 г/л Ре2Оз.
Предмет изобретени 
Способ очистки щелочно-алюминатных растворов от примесей железа путем введени  окиси кальци  в раствор с последующей фильтрацией через слой адсорбента, отличающийс  тем, что, с целью интенсификации процесса, в исходный раствор добавл ют сульфит натри  в количестве 0,5-10 г/л.
SU1824738A 1972-09-01 1972-09-01 Способ очистки щелочно-алюминатных растворов SU468888A1 (ru)