SU460175A2 - Способ изготовлени алмазно-абразивного инструмента - Google Patents

Способ изготовлени алмазно-абразивного инструмента

Info

Publication number
SU460175A2
SU460175A2 SU1870012A SU1870012A SU460175A2 SU 460175 A2 SU460175 A2 SU 460175A2 SU 1870012 A SU1870012 A SU 1870012A SU 1870012 A SU1870012 A SU 1870012A SU 460175 A2 SU460175 A2 SU 460175A2
Authority
SU
USSR - Soviet Union
Prior art keywords
diamond abrasive
abrasive tools
making diamond
pressing
tool
Prior art date
Application number
SU1870012A
Other languages
English (en)
Inventor
Валентин Федорович Шаталов
Original Assignee
Предприятие П/Я Р-6707
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я Р-6707 filed Critical Предприятие П/Я Р-6707
Priority to SU1870012A priority Critical patent/SU460175A2/ru
Application granted granted Critical
Publication of SU460175A2 publication Critical patent/SU460175A2/ru

Description

1
Изобретение относитс  к области производства ал1мазно-абразивных инструментов.
По основному авт. св. № 336147 известен способ изготовлени  алмазно-абразивного инструмента на основе древесины, предусматривающий по.мещение заготовки в среду с абразивной суспензией, где осуществл ют внедрение абразива на необходимую глубину с последующим контурным прессованием.
Педостаток известного способа заключаетс  в том, что величину зернистости инструмента определ ет Проходпое сечение пор древесины .
С целью расширени  технологических возможностей инструмента по предлагаемому способу заготовку инструмента предварительно подвергают объемному прессованию. Кроме того, прессование осуществл ют воздухом при ПО-120°С и давлении 200-250 кг/см.
По предлагаемому способу из свежесрубленной натуральной березы вырезают заготовки заданного типоразмера (кольцо, круг и т. п.), высущивают их до влажности 8-10%. После этого заготовки помещают в пресскамеру, в которой повышают давление среды, например
воздуха, до 200-250 кг/см. Затем камеру вместе с заготовкой нагревают до 110-120°С. При этом происходит объемное прессование заготовки, в результате которого увеличиваетс  проходное сечение пор, вследствие уплотнени  древесины за счет межклеточных пространств . После охлаждени  пресска.меры и среды до компатной температуры и снижени  давлени  до атмосферного заготовку извлекают из камеры и внедр ют абразивную суспензию с последующим контурпым прессованием известным способом.
Предмет изобретенп 

Claims (2)

1.Способ изготовлени  алмазно-абразивного инструмента по авт. св. N° 336147, отличающийс  тем, что, с целью расщирени  технологических возможностей инструмента, заготовку инструмента предварительно подвергают объемному прессованию.
2.Способ по п. 1, отличающийс  тем, что прессование осуществл ют воздухом при ПО-120°С и давлении 200-250 кг/см.
SU1870012A 1973-01-11 1973-01-11 Способ изготовлени алмазно-абразивного инструмента SU460175A2 (ru)