SU384884A1 - - Google Patents

Info

Publication number
SU384884A1
SU384884A1 SU1654813A SU1654813A SU384884A1 SU 384884 A1 SU384884 A1 SU 384884A1 SU 1654813 A SU1654813 A SU 1654813A SU 1654813 A SU1654813 A SU 1654813A SU 384884 A1 SU384884 A1 SU 384884A1
Authority
SU
USSR - Soviet Union
Prior art keywords
ingot
nickel
steel
briquettes
mold
Prior art date
Application number
SU1654813A
Other languages
English (en)
Russian (ru)
Inventor
В. И. Явойский Н. А. Пирогов Е. И. Тюрин К. И. Антипов А. Т. Федан Я. П. Думчев Э. В. Гартунг Ю. В. ковский
Original Assignee
, А. Д. Костюк Московский институт стали , сплавов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by , А. Д. Костюк Московский институт стали , сплавов filed Critical , А. Д. Костюк Московский институт стали , сплавов
Priority to SU1654813A priority Critical patent/SU384884A1/ru
Application granted granted Critical
Publication of SU384884A1 publication Critical patent/SU384884A1/ru

Links

Landscapes

  • Continuous Casting (AREA)
  • Treatment Of Steel In Its Molten State (AREA)
SU1654813A 1971-05-05 1971-05-05 SU384884A1 (fr)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU1654813A SU384884A1 (fr) 1971-05-05 1971-05-05

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU1654813A SU384884A1 (fr) 1971-05-05 1971-05-05

Publications (1)

Publication Number Publication Date
SU384884A1 true SU384884A1 (fr) 1973-05-29

Family

ID=20474687

Family Applications (1)

Application Number Title Priority Date Filing Date
SU1654813A SU384884A1 (fr) 1971-05-05 1971-05-05

Country Status (1)

Country Link
SU (1) SU384884A1 (fr)

Similar Documents

Publication Publication Date Title
US3819365A (en) Process for the treatment of molten metals
ES397575A1 (es) Un procedimiento para la colada totalmente continua de me- tales en estado liquido de fusion.
SU384884A1 (fr)
US3414043A (en) Method for the continuous transferring of liquid metals or alloys into solid state with desired cross section without using a mould
US2805145A (en) Exothermic metallurgical composition and method of introducing same into ferrous alloy
US2142031A (en) Process of aluminothermic smelting
US2870005A (en) Process for heating the head of an ingot of molten ferrous material
US2060074A (en) Copper refining apparatus
JPH04100671A (ja) 溶鋼の保温方法
US3030203A (en) Process of producing steel
SU386019A1 (ru) Способ извлечения металлов
SU722658A1 (ru) Способ разливки стали
SU478886A1 (ru) Сплав дл легировани
SU340309A1 (ru) Способ электроннолучевого переплава сталей и сплавов
US3063831A (en) Method of making titaniumcontaining alloys
SU488869A1 (ru) Способ получени ферроалюмини
US1515794A (en) And samuel peacock
SU392106A1 (ru) Способ получения слитков стали
SU773091A1 (ru) Присадочный материал дл обработки жидкой стали
SU551115A1 (ru) Шлакообразующа смесь дл разливки стали
CA1045335A (fr) Methode de coulee centrifuge d'ebauches metalliques
SU406900A1 (ru) Способ выплавки сталей и сплавов
SU544507A1 (ru) Экзотермическа шлакообразующа смесь дл разливки металла
SU415312A1 (fr)
US2179167A (en) Method of making steel