SU370282A1 - - Google Patents

Info

Publication number
SU370282A1
SU370282A1 SU1493699A SU1493699A SU370282A1 SU 370282 A1 SU370282 A1 SU 370282A1 SU 1493699 A SU1493699 A SU 1493699A SU 1493699 A SU1493699 A SU 1493699A SU 370282 A1 SU370282 A1 SU 370282A1
Authority
SU
USSR - Soviet Union
Prior art keywords
cleaning
chloride
urea
composition
sodium chloride
Prior art date
Application number
SU1493699A
Other languages
English (en)
Inventor
Р. А. Опарина С. С. Стаховски Л. Г. Зиненко
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1493699A priority Critical patent/SU370282A1/ru
Application granted granted Critical
Publication of SU370282A1 publication Critical patent/SU370282A1/ru

Description

СПОСОБ ОЧИСТКИ МЕТАЛЛИЧЕСКОЙ ПОВЕРХНОСТИ
1
Изо;бретаЕи.е относитс  к очистке металлической поверхности в солевых расплавах и может быть использовало, в частности в технологии производства изделий электронной техниии.
Известен способ очистки металлической ио;верх1НОсти в расплаве, содержащел хлористый цинк, хлористый натрий п хлористый а:М1МО|Ний.
Предложенный способ отличаетс  от известного введением в состав расплава мочеви .ны при определе-нном содержании компонентов и проведением процесса при 200- 250°С, что позвол ет улучшить качество очистки.
Данный способ имеет следующими химический состав, вес. %:
Хлористый цинк64,0-94,0
Хлористый натрий0,5-4,0
Хлористый аммоний5,0-30,0
Мочевина0,5-2,0
при 200-250°С.
Изобретение может быть проиллюстрировано следующим примером.
Очистке подвергалась проволока из нике2
левых сплавов НП-2 и 47НЦ, окисленна  в среде кислорода при в течение 12 час. Эта проволока очищалась в расплаве следующего состава, вес. %: Хлористый ципк72
Хлористый латрий3
ХлористыГ- ;шмоний24
iMo4eiin ia1
при 1 течение двух ми}|. После очистки поверхность получалась блест ща  серого цвета.
Предмет изобретени 
Способ очистки металлической поверхности в расплаве, содержащем хлористый цинк, хлористый натрий и хлористый аммоний, отличающийс  тем, что, с целью повышени  качества очистки, в состав раснлаза ввод т мочевину при следуюп,ем соотношении компонентов , вес. %:
Хлорпстый цинк64,0-94.0
Хлористый натрий0,5-4,0
Хлористый аммоний5,0-30,0
Мочевина0,5-2,0
и очистку провод т при 200-250 0.
SU1493699A 1970-11-26 1970-11-26 SU370282A1 (ru)