SU346001A1 - - Google Patents

Info

Publication number
SU346001A1
SU346001A1 SU1462562A SU1462562A SU346001A1 SU 346001 A1 SU346001 A1 SU 346001A1 SU 1462562 A SU1462562 A SU 1462562A SU 1462562 A SU1462562 A SU 1462562A SU 346001 A1 SU346001 A1 SU 346001A1
Authority
SU
USSR - Soviet Union
Prior art keywords
metal
strength
reducing
plastic deformation
metals
Prior art date
Application number
SU1462562A
Other languages
English (en)
Inventor
В.И. Спицин
О.А. Троицкий
П.Я. Глазунов
Original Assignee
В. И. Спицин, О. А. Троицкий , П. Я. Глазунов Институт физической химии СССР
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by В. И. Спицин, О. А. Троицкий , П. Я. Глазунов Институт физической химии СССР filed Critical В. И. Спицин, О. А. Троицкий , П. Я. Глазунов Институт физической химии СССР
Priority to SU1462562A priority Critical patent/SU346001A1/ru
Application granted granted Critical
Publication of SU346001A1 publication Critical patent/SU346001A1/ru

Description

Изобретение относитс  к металловедению и технологии обработки металлов давлением.
Известен способ снижени  прочности металлов в процессе пластической деформации, при котором через образцы пропускают импульсы тока величиной а/мм и продолжитель1-4
10
ностью
сек.
По этому способу дальнейша  интенсификаци  холодной пластической деформации должна быть св зана с увеличением плотности тока в импульсах, что сопровождаетс  нежелательным нагревом образцов.
Дл  обеспечени  дальнейшей интенсификации процесса снижени  прочности металла без его нагрева металлы одновременно с пропусканием через него импульсов тока облучают ускоренными электронами.
В зависимости от толшины обрабатываемого металла энерги  облучени  выбираетс  от 1 мэв до 3,5 мэв. Интенсивность потока частиц составл ет эл/см сек. Используема  интенсивность облучени  подобрана экспериментально и примерно соответствует максимуму интенсивности облучени  в радиационных по сах вокруг Земли.
Предмет изобретени 
Способ снижени  прочности металлов, преимушвственно при их пластической деформации, при котором через металл пропускают импульсы тока, отличаюш,ийс  тем, что, с целью интенсификации процесса, металл одновременно с пропусканием через него тока облучают ускоренными электронами.
SU1462562A 1970-08-28 1970-08-28 SU346001A1 (ru)