SU338501A1 - Chemical Resistant Eyes - Google Patents
Chemical Resistant EyesInfo
- Publication number
- SU338501A1 SU338501A1 SU1235458A SU1235458A SU338501A1 SU 338501 A1 SU338501 A1 SU 338501A1 SU 1235458 A SU1235458 A SU 1235458A SU 1235458 A SU1235458 A SU 1235458A SU 338501 A1 SU338501 A1 SU 338501A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- eyes
- chemical resistant
- glaze
- components
- temperature
- Prior art date
Description
Изобретен-ие может быть использовано дл глазуровани керамических изделий.The invention can be used for the glazing of ceramic products.
Известна глазурь, включаюп а SlOz, AlgOs, РбзОз, СаО, MgO, КгО, NagO, ВгОз и ZrOz.Known glaze, including SlOz, AlgOs, RbzOz, CaO, MgO, CrO, NagO, VgOz and ZrOz.
Предложен-на глазурь обеспечивает снижение температуры плавлени и повышение термической стойкости за счет того, что содержит указанные компоненты в следуюищх количествах (вес. %):The proposed glaze provides a decrease in the melting temperature and an increase in thermal stability due to the fact that it contains the indicated components in the following quantities (wt.%):
53,5-64,5 10,2-14,5 0,4-0,6 0,5-0,6 0,3-0,4 1,5-2 5,6-7,4 9,0-11,0 8,0-10,053.5-64.5 10.2-14.5 0.4-0.6 0.5-0.6 0.3-0.4 1.5-2 5.6-7.4 9.0 -11.0 8.0-10.0
Дл приготовлени глазурной For making glaze
массы НС- 25 пользуютс (в вес. %):Mass NS-25 use (in wt.%):
Отвешенные компоненты тш,ательно перемешивают , перемалывают и фриттуют при температуре 1280-1300°С. Далее после гранул ции фильтрованна масса подвергаетс мокрому помолу до тонипы соответствуюш,ей прохождению через сито 10000 отв/см, и полученна эмульси .наноситс на керамические издели известным снособом, пульверизацией или поливом. Обжиг ведут при температуре 950-1100°С.The weighed out components are mixed, ground, ground and frit at a temperature of 1280-1300 ° C. Then, after granulation, the filtered mass is subjected to wet grinding to the appropriate type, passing through a sieve of 10,000 holes / cm, and the resulting emulsion is applied to ceramic products with a known technique, spraying or pouring. Firing is carried out at a temperature of 950-1100 ° C.
Полученный после обжига глазурный покров имеет ровный поверхностный блеск.The glaze cover obtained after roasting has an even surface gloss.
Не наблюдаетс потускнени блеска и потери веса изделий после испытаннй их наNo dimming and weight loss of the products after testing them on
химическую стойкость по отношению к 20% сол ной кислоте и 357о раствору едкого натра в соответствии с ГОСТом 473-64, а также - к концентрированной серной кислоте в соответствии с ГОСТом 5473-53.chemical resistance to 20% hydrochloric acid and 357o sodium hydroxide solution in accordance with GOST 473-64, as well as to concentrated sulfuric acid in accordance with GOST 5473-53.
При испытании на термическую стойкость образцы выдерживают при 250°С более 10 теплосмен.When tested for thermal resistance, the samples are kept at 250 ° C for more than 10 heat cycles.
Предмет изобретени Subject invention
мической стойкости, она содержит указанные компоненты в следующих количествах (вresistance, it contains these components in the following amounts (in
вес. %):weight. %):
53,5-64,553.5-64.5
SiOzSioz
10,2-14,510.2-14.5
АЬОзAoz
0,4-0,60.4-0.6
РезОзRESOZ
0,.б0, .b
0,3-0,40.3-0.4
1,5-21.5-2
5,6-7,45,6-7,4
9,0-11,09.0-11.0
8,,08,, 0