FIELD: coal brequetting process. SUBSTANCE: bituminous cement is heated to 160 to 250 C, heated bituminous binder is foamed by introduction of 1 to 5 mass percent of water, foamed binder is mixed with crushed coal and then the mix is briquetted; heavy petroleum residues are used as binders. EFFECT: facilitated procedure. 3 cl, 1 tbl