SU1669539A1 - Method for regenerating anionites contaminated with silicon - Google Patents

Method for regenerating anionites contaminated with silicon Download PDF

Info

Publication number
SU1669539A1
SU1669539A1 SU894705822A SU4705822A SU1669539A1 SU 1669539 A1 SU1669539 A1 SU 1669539A1 SU 894705822 A SU894705822 A SU 894705822A SU 4705822 A SU4705822 A SU 4705822A SU 1669539 A1 SU1669539 A1 SU 1669539A1
Authority
SU
USSR - Soviet Union
Prior art keywords
solution
silicon
hours
treated
anion
Prior art date
Application number
SU894705822A
Other languages
Russian (ru)
Inventor
Эдуард Константинович Спирин
Original Assignee
Читинский институт природных ресурсов СО АН СССР
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Читинский институт природных ресурсов СО АН СССР filed Critical Читинский институт природных ресурсов СО АН СССР
Priority to SU894705822A priority Critical patent/SU1669539A1/en
Application granted granted Critical
Publication of SU1669539A1 publication Critical patent/SU1669539A1/en

Abstract

Изобретение относитс  к гидрометаллургии и позвол ет повысить механическую прочность анионитов, отрегенерированных от примесей кремни . Отравленный кремнием анионит ВП - 1 AN обрабатывают 20%-ным раствором азотнокислого натри  в течение 3 ч, затем в этот раствор добавл ют щелочи до PH 12,8 и обрабатывают еще в течение 6 ч, после чего анионит дополнительно обрабатывают 20%-ным раствором нитрата кальци  в присутствии 2 - 3 г/л перекиси водорода в течение 2 ч при объемном соотношении смолы и раствора 1 : (2 - 3). 1 табл.The invention relates to hydrometallurgy and makes it possible to increase the mechanical strength of anion exchangers regenerated from silicon impurities. The VP-1 AN anion exchanger poisoned with silicon is treated with a 20% sodium nitrate solution for 3 hours, then alkali is added to this solution up to PH 12.8 and treated for an additional 6 hours, after which the anion exchange resin is further treated with a 20% solution calcium nitrate in the presence of 2–3 g / l of hydrogen peroxide for 2 hours at a volume ratio of resin and solution of 1: (2–3). 1 tab.

Description

Изобретение относитс  к гидрометаллургии , преимущественно к процессам сор- бционного извлечени  цветных, редких и рассе нных элементов из пульп и растворов , полученных в ходе выщелачивани  алюмосиликатных и других руд, может быть использовано дл  восстановлени  физико- химических свойств анионитов в многоцикличном сорбционном процессе.The invention relates to hydrometallurgy, mainly to the process of sorption extraction of color, rare and scattered elements from pulps and solutions obtained during leaching of aluminosilicate and other ores, can be used to restore the physicochemical properties of anion exchangers in a multi-cycle sorption process.

Цель изобретени  - повышение механической прочности отрегенерированных анионитов .The purpose of the invention is to increase the mechanical strength of the regenerated anion exchangers.

Пример. Анионит ВП-1Ап, содержащий 40 % двуокиси кремни ,в колонном аппарате обрабатываетс  20%-ным раствором азотнокислого натри  в течение 3 ч в динамическом режиме, затем в этом раствор добавл ют 20%-ным раствор щелочи до достижени  рН среды 12,8. Полученным раствором обрабатывают анионит в проти- воточном режиме в три стадии в течение 6 ч, отдел ют от десорбирующего раствора и обрабатывают 20%-ным раствором Са(МОз)2 в присутствии 2-3 г/л Н202 в течение 2 ч при непрерывном перемешивании и при соотношении смола - раствор 1:(2-3).Example. Anion exchanger VP-1Ap containing 40% silicon dioxide in the column apparatus is treated with 20% sodium nitrate solution for 3 hours in a dynamic mode, then the solution is added with a 20% solution of alkali until the pH of the medium is 12.8. The resulting solution is treated with anion exchanger in a counter-flow mode in three stages for 6 hours, separated from the stripping solution and treated with a 20% solution of Ca (MO3) 2 in the presence of 2-3 g / l H2202 for 2 hours with continuous stirring and when the ratio of resin - solution 1: (2-3).

Данные по предлагаемому и известному способам приведены в таблице.Data on the proposed and known methods are given in the table.

Технико-экономическа  эффективность способа заключаетс  в сокращении в 3-5 раз потерь сорбента в эксплуатацииTechnical and economic efficiency of the method consists in reducing the sorbent losses in operation by 3-5 times.

Claims (1)

Формула изобретени Invention Formula Способ регенерации анионитов, отравленных кремнием, включающий обработку раствором минеральных солей, щелочью и затем дополнительную обработку раствором азотнокислых солей двухвалентных металлов с концентрацией 150-300 г/л при объемном соотношении анионита к раствору 1:(2-3), отличающийс  тем, что, с целью повышени  механической прочности отрегенерированного анионита, обработку раствором азотнокислой соли двухвалентного металла ведут в присутствии перекиси водорода.A method of regenerating anion exchangers poisoned with silicon, which includes treatment with a solution of mineral salts, alkali, and then additional treatment with a solution of nitrate salts of divalent metals with a concentration of 150-300 g / l with a volume ratio of anion exchange resin to a 1: (2-3) solution, characterized in that in order to increase the mechanical strength of the regenerated anion exchanger, the treatment with a solution of the divalent metal nitrate is carried out in the presence of hydrogen peroxide. 1C1C ON О Ю СЛON O U SL CJCJ юYu
SU894705822A 1989-06-14 1989-06-14 Method for regenerating anionites contaminated with silicon SU1669539A1 (en)