SU1578014A1 - Method of butt welding of plastic tubes - Google Patents

Method of butt welding of plastic tubes Download PDF

Info

Publication number
SU1578014A1
SU1578014A1 SU874340612A SU4340612A SU1578014A1 SU 1578014 A1 SU1578014 A1 SU 1578014A1 SU 874340612 A SU874340612 A SU 874340612A SU 4340612 A SU4340612 A SU 4340612A SU 1578014 A1 SU1578014 A1 SU 1578014A1
Authority
SU
USSR - Soviet Union
Prior art keywords
joint
pipe
butt welding
heated
welding
Prior art date
Application number
SU874340612A
Other languages
Russian (ru)
Inventor
Владимир Филиппович Тимощук
Original Assignee
Конструкторско-Технологическое Бюро С Опытным Производством "Белгазтехника"
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Конструкторско-Технологическое Бюро С Опытным Производством "Белгазтехника" filed Critical Конструкторско-Технологическое Бюро С Опытным Производством "Белгазтехника"
Priority to SU874340612A priority Critical patent/SU1578014A1/en
Application granted granted Critical
Publication of SU1578014A1 publication Critical patent/SU1578014A1/en

Abstract

Изобретение относитс  к сварке пластмасс и может найти применение при строительстве и эксплуатации полиэтиленовых газопроводов. Цель - повышение качества сварного соединени  при ремонте трубопроводов. В способе стыковой сварки пластмассовых труб перед нагревом соедин емых торцов осуществл ют нагрев по меньшей мере одного участка трубы, расположенного на рассто нии от стыка. Сжатие торцов труб производ т путем раст жени  нагретого участка трубы в направлении к стыку. 2 ил.The invention relates to the welding of plastics and can be used in the construction and operation of polyethylene gas pipelines. The goal is to improve the quality of the welded joint in the repair of pipelines. In the method of butt welding of plastic pipes, at least one section of the pipe located at a distance from the joint is heated before heating the joined ends. Compression of the pipe ends is performed by stretching the heated pipe section towards the joint. 2 Il.

Description

Изобретение относитс  к сварке пластмасс и может найти применение при строительстве и эксплуатации полиэтиленовых газопроводов.The invention relates to the welding of plastics and can be used in the construction and operation of polyethylene gas pipelines.

Целью изобретени   вл етс  повышение качества сварного соединени  при ремонте трубопроводов.The aim of the invention is to improve the quality of the welded joint in the repair of pipelines.

На биг. 1 изображена установка дл  -реализации способа, общий вид, на биг. 2 - закладной нагревательный элемент.On big. 1 shows an installation for the implementation of the method, a general view, on Big. 2 - embedded heating element.

Способ стыковой сварки пластмассовых труб заключаетс  в следующем.The method of butt welding of plastic pipes is as follows.

Свариваемые трубы 1 и 2 фиксируют в зажимах 3 и 4. Между торцами создают зазор, необходимый дл  размещени  торцевател  (не показан) или нагревательного элемента. Заданную величину зазора между торцами получают путем предварительной приварки к одной из труб вставки различной длины в зависимости от повреждени  на трубопроводе. Концы труб 1 и 2 при этом заземлены землей. После торцевани  труб в зазор между торцами устанавливают нагревательный элемент 5 (закладной или дисковый). На участках труб, расположенных на рассто нии от стыка, размещают нагревательные хомуты 6. Вначале осуществл ют равномерный нагрев по меньшей мере одного участка трубы, расположенного на рассто нии о г стыка, нагревательными хомутами 6. Затем включают нагревательный элемент 5 и механизм 7 сжати . Осуществл ют нагрев и торцов труб. В случае использовани  закладного нагревательного элемента он остаетс  в теле 1рубы. В случае использовани  дискового нагревательного элемента после нагрева торцов его удал ют из зазора и торцы трубThe welded pipes 1 and 2 are fixed in the clips 3 and 4. Between the ends they create a gap, which is necessary for the placement of an end sealer (not shown) or a heating element. The specified gap between the ends is obtained by pre-welding to one of the insertion pipes of different lengths depending on the damage to the pipeline. The ends of pipes 1 and 2 are grounded at the same time. After facing the pipes, the heating element 5 is installed in the gap between the ends (mortgage or disk). Heating sections 6 are placed on the pipe sections located at a distance from the joint. At first, at least one section of the pipe located at the joint distance is heated uniformly with heating collars 6. Then the heating element 5 and the compression mechanism 7 are turned on. The ends of the pipes are also heated. If the embedded heating element is used, it remains in the body of the pipe. In the case of using a disk heating element after heating the ends, it is removed from the gap and the ends of the pipes

СДSD

JJ

ЭОEO

Ј.Ј.

Составитель Н, т пнсегва Редактор М. Бандура Texperf Т.Олкйн -к Корректор Л.ПатайCompiled by N, t pnsegva Editor M. Bandura Texperf T. Olkyn -k Proofreader L. Patay

Заказ 1883 Order 1883

Тираж 530Circulation 530

ВНИИПИ Государственного комитета по кзобреткни м н открыти м при ГКНТ СССР 113035, Москва, Ж-35, Раушска  наб„3 д. 4/5VNIIPI of the State Committee for Critics of Discovery at the State Committee on Science and Technology of the USSR 113035, Moscow, Zh-35, Raushsk nab. 3 d. 4/5

ПодписноеSubscription

Claims (1)

Формула изобретения Способ стыковой сварки пластмассовых труб, включающий торцевание, нагрев соединяемых торцов труб, сжатие их и охлаждение сварного шва, отличающийся тем, что, с целью повышения качества сварного соединения при ремонте трубопроводов, перед нагревом соединяемых торцов осуществляют нагрев по меньшей мере одного участка трубы, расположенного на расстоянии от стыка, а сжатие торцой труб осуществляют путем растяжения нагретого участка трубы в направлении к стыку,.SUMMARY OF THE INVENTION A method for butt welding of plastic pipes, including trimming, heating the pipe ends to be joined, compressing them and cooling the weld, characterized in that, in order to improve the quality of the welded joint when repairing pipelines, at least one pipe section is heated before heating the connected ends located at a distance from the joint, and the compression of the end pipe is carried out by stretching the heated pipe section in the direction of the joint.
SU874340612A 1987-12-08 1987-12-08 Method of butt welding of plastic tubes SU1578014A1 (en)