SU1442631A1 - Diamond crown bit - Google Patents
Diamond crown bit Download PDFInfo
- Publication number
- SU1442631A1 SU1442631A1 SU864154068A SU4154068A SU1442631A1 SU 1442631 A1 SU1442631 A1 SU 1442631A1 SU 864154068 A SU864154068 A SU 864154068A SU 4154068 A SU4154068 A SU 4154068A SU 1442631 A1 SU1442631 A1 SU 1442631A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- crown
- diamonds
- matrix
- diamond
- rock
- Prior art date
Abstract
Изобретение относитс к буровой технике . Цель - повышение эксплуатационной стойкости коронки путем использовани шлама Дл самозатачивани коронки в процессе бурени . Коронка содержит корпус 1 с алмазосодержащей матрицей (/VI) 3 и радиальные промывочные отверсти 5. На внутренней поверхности М 3 со стороны торцов выполнены выемки 4. Отверсти выполнены в стенке М 3 и сообщены с выемками 4. М 3 армирована гранулированными алмазами, оболочка последних содержит алмазы мелкой фракции. Алмазы, выкращива сь, создают дополнительный абразивный шлам. Последний снижает прочность горной породы, поддержива необходимую величину абразивного потока на забое скважины. Т.о., процесс износа способствует разрушению горной породы. 1 з.п. ф-лы, 2 ил.The invention relates to a drilling technique. The goal is to increase the operational durability of the crown by using sludge to self-sharpen the crown during drilling. The crown contains a housing 1 with a diamond-containing matrix (/ VI) 3 and radial washing holes 5. Recesses 4 are made on the inner surface of M 3 from the ends 4. Holes are made in the wall of M 3 and communicated with grooves 4. M 3 is reinforced with granulated diamonds, the shell of the latter contains diamonds of small fraction. Diamonds, vykraschiva, create additional abrasive slurry. The latter reduces the strength of the rock, maintaining the necessary amount of abrasive flow at the well bottom. Thus, the process of wear contributes to the destruction of the rock. 1 hp f-ly, 2 ill.
Description
(Л(L
4 4 N54 4 N5
Ot СОOt sb
иг. 1ig. one
Изобретение относитс к буровой технике , а именно к алмазному породоразрушаю- щему инструменту.The invention relates to a drilling technique, namely, a diamond rock cutting tool.
Цель изобретени - повышение эксплуатационной стойкости коронки путем использовани шлама дл самозатачивани коронки в процессе бурени .The purpose of the invention is to increase the operational durability of the crown by using sludge to self-sharpen the crown during the drilling process.
На фиг. 1 изображена алмазна бурова коронка; на фиг. 2 - торец матрицы коронки , вид сверху.FIG. 1 shows a diamond of a crown; in fig. 2 - the end of the matrix crowns, top view.
Алмазна бурова коронка выключает в себ корпус 1 с торцовыми прорез ми 2, алмазосодержащую матрицу 3 с радиальными выемками 4 с внутренней стороны .матрицы и промывочными отверсти ми 5.The diamond bit crown turns off the body 1 with the end slots 2, the diamond-containing matrix 3 with the radial recesses 4 on the inner side of the matrix and the washing holes 5.
Алмазна бурова коронка работает следующим образом.Diamond of a brown crown works as follows.
При бурении твердых и низкоабразивных горных пород шлам, образующийс за счет разрушени горной породы и износа матрицы , улавливаетс и накапливаетс во внутренних выемках 4 матрицы. Количество накопленного шлама зависит от числа промывочных отверстий 5, а также от рассто ни между центрами промывных отверстий 5 и торцом матрицы коронки. Так как промывочные отверсти 5 имеюгс не во всех выемках, шлам используетс многократно , попада под торец набегающего сектора коронки. Причем измельченна фракци шлама вымываетс 3 первую очередь, а крупна работает повторно.When drilling hard and low-abrasive rocks, the sludge produced by the destruction of the rock and the wear of the matrix is captured and accumulated in the inner grooves 4 of the matrix. The amount of accumulated sludge depends on the number of flushing holes 5, as well as the distance between the centers of the flushing holes 5 and the end of the crown matrix. Since the washing holes 5 of the imeugs are not in all the grooves, the sludge is used repeatedly, falling under the butt of the incoming crown sector. Moreover, the crushed sludge fraction is washed 3 first and the large one is recycled.
00
5five
00
5five
00
Твердосплавна оболочка гранул рабочих алмазов армирована алмазами мелкой фракции, выкрашива сь, они создают дополнительный абразивный шлам, который, создава на поверхности забо микродефекты, снижает прочность горной породы поддержива необходимую величину механической скорости бурени , следовательно, поддержива необходимую величину абразивного потока на забое скважины.The carbide shell of working diamond granules reinforced with fines of diamonds, crumbled, they create additional abrasive slurry, which, creating microscopic defects on the bottom surface, reduces the strength of the rock, maintaining the necessary amount of mechanical drilling speed, and therefore maintaining the necessary amount of abrasive flow to the bottom hole.
Таким образом, процесс износа матрицы способствует разрушению горной породы, а последний, в свою очередь, способствует процессу износа матрицы, повыша этим эксплуатационную стойкость коронки.Thus, the process of wear of the matrix contributes to the destruction of the rock, and the latter, in turn, contributes to the process of wear of the matrix, thereby increasing the operational durability of the crown.
Claims (2)