SU138379A1 - Способ получени негорючих пенопластов - Google Patents

Способ получени негорючих пенопластов

Info

Publication number
SU138379A1
SU138379A1 SU649312A SU649312A SU138379A1 SU 138379 A1 SU138379 A1 SU 138379A1 SU 649312 A SU649312 A SU 649312A SU 649312 A SU649312 A SU 649312A SU 138379 A1 SU138379 A1 SU 138379A1
Authority
SU
USSR - Soviet Union
Prior art keywords
obtaining non
epoxy resin
combustible
foams
combustible foams
Prior art date
Application number
SU649312A
Other languages
English (en)
Inventor
В.Д. Валгин
И.П. Лосев
Original Assignee
В.Д. Валгин
И.П. Лосев
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by В.Д. Валгин, И.П. Лосев filed Critical В.Д. Валгин
Priority to SU649312A priority Critical patent/SU138379A1/ru
Application granted granted Critical
Publication of SU138379A1 publication Critical patent/SU138379A1/ru

Description

Способ получени  негорючих пенопластов на основе эпоксидных Смол и легкоплавких ангидридов путем вспенивани  известен.
Предложенный метод получени  негорючих пенопластов повышенной теплостойкости на основе низкомолекул рной эпоксидной смолы с хлорэндиковым ангидридом-диизоцианатом  вл етс  новым и в литературе не описан. Кроме того, этот способ характеризуетс  тем, что:
1.Вспенивание эпоксидной смолы с ангидридом осуществл етс  диизоцианатом в результате последовательно проход щих реакций;
а) ангирид + ОН - группы эпоксидной смолы СООН-группы; б)---СООН группы +O C N группы СОг+пространственные св зи.
2.Диизоцианат используетс  не только как вспениватель, но и как растворитель хлорэндикового ангидрида, позвол   осуществл ть гомогенное совмещение последнего с эпоксидной смолой и снижа  в зкость смеси.
Полученный по новому методу пенопласт из эпоксидной смолы хлорэндикового ангидрида и 2,4-толуилендиизоцианата обладает следующими ценными свойствами: удовлетворительной механической прочностью , высокой теплостойкостью, (рабоча  температура выще 1ЬО°), негорючестью. Разработанный пенопласт  вл етс  заливочным.
Технологи  получени  пенопластов следующа .
В жидкую эпоксидную смолу п|1И 60-70° вводитс  одновременно ангидрид, диизоциант и эмульгатор.Смешение компонентов при 60-70° производитс  в течение 10 - 20 мин, после чего полученна  жидка  композици , немного подвспененна , выливаетс  в
SU649312A 1960-01-03 1960-01-03 Способ получени негорючих пенопластов SU138379A1 (ru)