FIELD: metallurgy. SUBSTANCE: method for production of foil from alloys based on titanium nickelide provides for production of alloy by hardening from liquid state with temperature of 110-1300 C and annealing at 500-550 C for 5-7 min. EFFECT: provision of production of foil with thickness up to 20-50 mcm by increased plasticity. 2 cl, 1 tbl