SU1244120A1 - Способ упрочнени стекла - Google Patents

Способ упрочнени стекла Download PDF

Info

Publication number
SU1244120A1
SU1244120A1 SU833547869A SU3547869A SU1244120A1 SU 1244120 A1 SU1244120 A1 SU 1244120A1 SU 833547869 A SU833547869 A SU 833547869A SU 3547869 A SU3547869 A SU 3547869A SU 1244120 A1 SU1244120 A1 SU 1244120A1
Authority
SU
USSR - Soviet Union
Prior art keywords
glass
heat treatment
hardening glass
temperature
hours
Prior art date
Application number
SU833547869A
Other languages
English (en)
Inventor
Ахмед Магомедович Бутаев
Галина Ивановна Баранцева
Original Assignee
Предприятие П/Я А-7840
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я А-7840 filed Critical Предприятие П/Я А-7840
Priority to SU833547869A priority Critical patent/SU1244120A1/ru
Application granted granted Critical
Publication of SU1244120A1 publication Critical patent/SU1244120A1/ru

Description

12
Изобретение относитс  к упрочнению стекла методом низкотемпературного ионного обмена и может быть ч
использовано в стекольной промьпплен- ности.
Целью изобретени   вл етс  повьппе- .ние безопасной прочности стекла.
Сущность изобретени  заключаетс  в следующем.
Трехмиллиметровое листовое стекла упрочн ют в расплаве нитрата кали  при в течение 24 ч, охлаждают до комнатной температуры, остатки
соли отмывают проточной водой и ПОД
202
вергают термообработке в воздушном термостате при 300-400 С в течение 0,5-24 ч. Затем стекло дополнительно обрабатывают в расплаве соли (нитрата кали ) в интервале температур.на 30-150 С выше температуры термообработки в течение 2-6 ч. Упрочненное таким образом стекло испытывают на механическую прочность методом центрального симметричного изгиба .
Полученные экспериментальные данные приведены в таблице.

Claims (1)

  1. СПОСОБ УПРОЧНЕНИЯ СТЕКЛА путем ионного обмена в расплаве соли с последующей промывкой и термообработкой при 300-400 С в течение 0,524 ч, отличающийся тем, что, с целью повышения безопасной прочности, стекло после термообработки дополнительно обрабатывают в- расплаве соли при температуре на 50150 С выше температуры термообработки в течение 2-6 ч.
SU833547869A 1983-01-31 1983-01-31 Способ упрочнени стекла SU1244120A1 (ru)