SU1186428A1 - Method of indirect arc welding of highly heat-conducting metal with consumable electrode - Google Patents
Method of indirect arc welding of highly heat-conducting metal with consumable electrode Download PDFInfo
- Publication number
- SU1186428A1 SU1186428A1 SU843739280A SU3739280A SU1186428A1 SU 1186428 A1 SU1186428 A1 SU 1186428A1 SU 843739280 A SU843739280 A SU 843739280A SU 3739280 A SU3739280 A SU 3739280A SU 1186428 A1 SU1186428 A1 SU 1186428A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- welding
- electrode
- lining
- arc
- combustion
- Prior art date
Abstract
СПОСОБ ОДНОСТОРОННЕЙ ДУГОВОЙ СВАРКИ ВЫСОКОТЕПЛОПРОВОДНрГО МЕТАЛЛА ПЛАВЯЩИМСЯ ЭЛЕКТРОДОМ в среде защитного газа, при котором производ т предварительный подогрев свариваемых кромок, а процесс ведут на формирующей подкладке с возбуждением дуги на выводной планке, отличающийс тем, что, с целью повыщени качества сварного соединени и производительности процесса путем улучщени формировани обратной стороны шва и сокращени длительности подогрева, в качестве формирующей подкладки используют брикеты термитной смеси, предварительный подогрев осуществл ют путем поджига подкладки сварочной дугой, возбуждаемой между электродом и выводной планкой, а в момент достижени заданной температуры подогрева начальными участками свариваемы.х кромок начинают перемещение электрода и поджим образовавшегос при сгорании порошкообразного шлакового материала, причем сварку производ т со скоростью, равной ско- S рости сгорани термитной смеси. (ОMETHOD UNILATERAL ARC WELDING VYSOKOTEPLOPROVODNrGO METAL consumable electrode gas shielded at which produce preheating welded edges, and the process is carried out in forming lining from arc excitation on the output bar, characterized in that, with a view to the Enhance quality weld and productivity by process to improve the formation of the back side of the seam and reduce the duration of heating; briquettes of thermite mixture are used as a forming lining; Heating is effected by igniting the lining with a welding arc excited between the electrode and the exit plate, and at the moment when the preheating temperature is reached, the initial sections of the edges to be welded start moving the electrode and pressing the powdered slag material formed during combustion, and the welding is performed at a speed equal to rate of combustion of the thermite mixture. (ABOUT
Description
JZJz
/У/////Л/ U ///// L
;/-:: ; / - ::
0000
О) 4 ЮO) 4 U
0000
//
Claims (1)